Corrosion behavior of Al–Si–Mg alloy made by selective laser melting method

Fomina M.A., Dynin N.V., Shurtakov S.V., Morozova S.E.
Fomina M.A., Dynin N.V., Shurtakov S.V., Morozova S.E. Corrosion behavior of Al–Si–Mg alloy made by selective laser melting method // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-91-100. URL: https://www.viam-works.ru/en/journal/2018/4/11
Keywords
corrosion behavior, selective laser melting, aluminum alloys, additive technologies, Al–Si–Mg, intergranular corrosion.
Abstract

Selective laser melting (SLM) is a promising technology for complicated configuration details manufacture. Al-Si alloys are the most investigated alloys in selective laser melting manufacture at the time. A mechanical, corrosion and operational performance of SLM and as-cast details are deeply vary because cast structure stands in stark difference to SLM structure. In this article a corrosion behavior of synthesized and heat treated Al–Si–Mg alloy is shown. Also the results of general and intergranular corrosion are shown. The corrosion behavior of AlSi10Mg aluminum alloy with additives of Cu, Zr, Al–Si–Mg system Ce directly depends on structure of a material which in turn depends on manufacturing techniques and modes of thermal processing. In a cast condition the material shows the lowered corrosion resistance owing to formation of large dentritny structure in the course of crystallization. Development of corrosion processes in an alloy made by a SLS method, depends on quantity, the

Reference list
  1. Kablov E.N. Additivnye tehnologii – dominanta nacionalnoj tehnologicheskoj iniciativy [The additive technologies – dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Buchbinder D. High Power Selective Laser Melting of Aluminum Parts // Physics Procedia. 2011. Vol. 12. P. 271–278. DOI: 10.1016/j.phpro.2011.03.035.
  4. Sercombe T.B., Li X. Selective laser melting of aluminium and aluminium metal matrix composites: review // Materials Technology. 2016. Vol. 31:2. P. 77–85. DOI: 10.1179/1753555715Y.0000000078.
  5. Dynin N.V., Ivanova A.O., Hasikov D.V., Oglodkov M.S. Selektivnoe lazernoe splavlenie alyuminievyh splavov (obzor) [Selective laser melting of aluminium alloy (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №8. St. 02. Available at: http://www.viam-works.ru (accessed: March 19, 2018). DOI: 10.18577/2307-6046-2017-0-8-2-2.
  6. Aboulkhai N.T., Maskery I., Tuck C. The microstructure and mechanical properties of se-lectively laser melted AlSi10Mg: The effect of a conventional T6-like heat treatment // Materials Science & Engineering: A. 2016. Vol. 667. P. 139–146. DOI: 10.1016/j.msea.2016.04.092.
  7. Read N., Wang W., Essa K. Selective laser melting of AlSi10Mg alloy: Process optimisation and mechanical properties development // Materials and Design. 2015. Vol. 65. P. 417–424. DOI: 10.1016/j.matdes.2014.09.044.
  8. Aboulkhai N.T., Tuck C., Ashcroft I. et al. On the precipitation hardening of selective laser melted AlSi10Mg //The Minerals, Metals & Materials Society and ASM International 2015. Metallurgical and materials transactions A. Vol. 46a, August 2015–3337. DOI:10.1007/s11661-015-2980-7.
  9. Pei W., Zhengying W., Zhen C. The AlSi10Mg samples produced by selective laser melting: single track, densification, microstructure and mechanical behavior // Applied surface sci-ence. 2007. DOI: 10.1016/j.apsusc.2017.02.215.
  10. Prashanth K.G., Scudino S., Klauss H.J. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: Effect of heat treatment // Materials Science & Engineering: A. 2014. Vol. 590. P. 153–160.
  11. Kimura T. Effect of silicon content on densification, mechanical and thermal properties of Al-xSi binary alloys fabricated using selective laser melting // Materials Science & Engineer-ing: A. November 17, 2016. DOI: 10.1016/j.msea.2016.11.059.
  12. Tang M., Pistorius P.C. Anisotropic Mechanical Behavior of AlSi10Mg Parts Produced by Selective Laser Melting // The Minerals, Metals & Materials Society. January, 2017. DOI: 10.1007/s11837-016-2230-5.
  13. Ryabov D.K., Antipov V.V., Korolev V.A., Medvedev P.N. Vliyanie tehnologicheskih faktorov na strukturu i svojstva silumina, poluchennogo s ispolzovaniem tehnologii sel-ektivnogo lazernogo sinteza [Effect of technological factors on structure and properties of Al–Si alloy obtained by selective laser melting] // Aviacionnye materialy i tehnologii. 2016. №S1 (43). S. 44–51. DOI: 10.18577/2071-9140-2016-0-S1-44-51.
  14. Ryabov D.K., Morozova L.V., Korolev V.A., Ivanova A.O. Izmenenie mehanicheskih svojstv splava AK9ch., poluchennogo po tehnologii selektivnogo lazernogo splavleniya [Alternation of mechanical features of alloy AK9ch manufactured by selective laser melting] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9 (45). St. 02. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2016-0-9-2-2.
  15. Ryabov D.K., Zajcev D.V., Dynin N.V., Ivanova A.O. Izmenenie struktury splava AK9ch., poluchennogo selektivnym lazernym spekaniem, v processe termicheskoj obrabotki [Alternation of structure of selective laser melted aluminum alloy AK9ch during heat treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9. St. 03. Available at: http://www.viam-works.ru (accessed: March 19, 2018). DOI: 10.18557/2307-6046-2016-0-9-3-3.
  16. Ivanova A.O., Zavodov A.V., Dynin N.V., Fomina M.A. Effektivnost vvedeniya malyh dobavok perehodnyh metallov v splavy tipa AlSi10Mg, prednaznachennye dlya polucheniya izdelij po tehnologii selektivnogo lazernogo splavleniya [Efficiency of complex alloying AlSi10Mg type alloy with transition metals for selective laser melting technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №7 (55). St. 01. Available at: http://www.viam-works.ru (accessed: March 19, 2018). DOI: 10.18577/2307-6046-2017-0-7-1-1.
  17. Kablov E.N., Lukina E.A., Sbitneva S.V., Hohlatova L.B., Zajcev D.V. Formirovanie metastabilnyh faz pri raspade tverdogo rastvora v processe iskusstvennogo stareniya Al-splavov [Forming of metastable phases at disintegration of solid solution in the course of artificial aging of Al-alloys] // Tehnologiya legkih splavov. 2016. №3. S. 7–17.
  18. Sinyavskij V.S., Valkov V.D., Budov G.M. Korroziya i zashhita alyuminievyh splavov [Corrosion and protection of aluminum alloys]. M.: Metallurgiya, 1979. 224 s.
  19. Fomina M.A., Kutyrev A.E., Klochkova Yu.Yu., Sbitneva S.V. Issledovanie korrozionnyh harakteristik vysokoprochnogo splava sistemy Al–Cu–Li v zavisimosti ot razlichnyh rezhimov termicheskoj obrabotki [Research of corrosion characteristics of high-strength alloy of Al–Cu–Li system depending on various modes of heat treatment] // Aviacionnye materialy i tehnologii. 2016. №S2 (44). S. 39–48. DOI: 10.18577/2071-9140-2016-0-S2-39-48.
  20. Karimova S.A., Kutyrev A.E., Fomina M.A., Chesnokov D.V. Modelirovanie processa vozdejstviya agressivnyh komponentov promyshlennoj atmosfery na metallicheskie materialy v kamere solevogo tumana [Modeling of process of influence of aggressive components of the industrial atmosphere on metal materials in the salt spray chamber] //Aviacionnye materialy i tehnologii. 2015. №1. 86–94.
  21. Cabrini M., Lorenzi S., Pastore T. et al. Corrosion behavior of aluminum-silicon alloys obtained by Direct Metal Laser Sintering // Proceedings of the European Corrosion Congress (EUROCORR 2017). 2017. P. 150–158.
  22. Revilla R., Liang J., Godet S., De Graeve I. Local Corrosion Behavior of Additive Manu-factored AlSiMg Alloy Assessed by SEM and SKPFM // Journal of Electrochemical Society. 2017. Vol. 164. P. C27–C35.
  23. Cabrini M., Lorenzi S., Pastore T. et al. Effetto di trattamenti termici sul comportamento a corrosione di una lega AlSiMg ottenuta mediante Direct Metal Laser Sintering (DMLS) // Atti delle Giornate Nazionali sulla Corrosione e Protezione. XI ed. Ferrara, Italia, 2015 (СD-R).
  24. Feliu Jr.S., Maffiotte C., Samaniego A. et al. Effect of the chemistry and structure of the native oxide surface film on the corrosion properties of commercial AZ31 and AZ61 alloys // Applied Surface Science. Vol. 4. 2011. Р. 257.
  25. Liu Y., Wang Z., Ke W. Study on influence of native oxide and corrosion products on atmospheric corrosion of pure Al // Corrosion. Science. 2014. Vol. 80. P. 169–178.
  26. Cabrini M., Lorenzi S., Pastore T. et al. Corrosion resistance of direct metal laser sintering AlSiMg alloy // Surface and Interface Analysis. 2016. Vol. 48. P. 818.
  27. Cabrini M., Lorenzi S., Pastore T. et al. Evaluation of corrosion resistance of Al–10Si–Mg alloy obtained by means of Direct Metal Laser Sintering // Journal of Materials Processing Technology. 2016. Vol. 231. P. 326.
  28. Cabrini M., Lorenzi S., Pastore T. et al. Effect of heat-treatment on corrosion resistance of DMLS AlSi10Mg alloy // Electrochimica Acta. 2016. Vol. 206. P. 346.
  29. ECSS-Q-70-37C. European Cooperation for Space Standartization. Determination of the susceptibility of metals to stress-corrosion cracking. Requirements & Standards Division. Noordwijk, 2008. P. 31.