Tribological characteristics of the alkyd coverings filled with abrasive fillers of different size

Alifanov E.V., Chaykun A.М., Gorlov D.S., Venediktova M.A.
Alifanov E.V., Chaykun A.М., Gorlov D.S., Venediktova M.A. Tribological characteristics of the alkyd coverings filled with abrasive fillers of different size // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-84-90. URL: https://www.viam-works.ru/en/journal/2018/4/10
Keywords
polymers, nonskid coating, tribologiya, friction coefficient, polyurethane, fillers.
Abstract

In article results of research of tribological properties of model systems of nonskid coatings based on one-component alkyd binding with abrasive fillers like sand and electrocorundum of different fractions was applied. Submitted data can be used when developing nonskid coatings which are actively applied, both in the aviation industry, and in other spheres of national economy. Intelligent approach to the nature and the size of the chosen filler will allow not only to improve considerably functionality of nonskid coating, but also to increase term of its operation. Values of friction coefficient, as one of the main characteristics of this type of coatings, are given. Observations concerning surface qualities and resistance to abrasion are showed. Definition of friction coefficient were carried out on the tribometer CETR UMT-3MT with use of drive of R33HE350 for reciprocating motion on the mode modeling the beginning of slipping of shoe sole on dry nonskid coating. It is shown that ex

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  4. Kablov E.N. Materialy dlya aviakosmicheskoj tehniki [Materials for aerospace equipment] // Vse materialy. Enciklopedicheskij spravochnik. 2007. №5. S. 7–27.
  5. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih soz-daniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  6. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  7. Mudrov O.A., Savchenko I.M., Shitov V.S. Spravochnik po elastomernym pokrytiyam i germetikam v sudostroenii [The directory on elastomeric coverings and hermetics in ship-building]. L.: Sudostroenie, 1982. 184 s.
  8. Drinberg A.S., Kalinskaya T.V., Udenko I.A. Tehnologiya sudovyh pokrytij [Technology of ship coverings]. M.: LKM-press, 2016. 672 s.
  9. Rozenfeld I.L., Rubinshtejn F.I., Zhigalova K.A. Zashhita metallov ot korrozii lakokraso-chnymi pokrytiyami [Protection of metals against corrosion by paint coatings]. M.: Himiya, 1987. 224 s.
  10. Denker I.I. Tehnologiya okraski samoletov i vertoletov: ucheb. posobie [Technology of coloring of airplanes and helicopters: manual]. M.: Mashinostroenie, 1980. 190 s.
  11. Semenova L.V., Malova N.E., Kuznetsova V.A., Pozhoga A.A. Lakokrasochnye materialy i pokrytiya [Paint and varnish materials and coatings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
  12. Nefyodov N.I., Semyonova L.V. Nanesenie lakokrasochnyh pokrytij metodom «syroj po syromu» [The application of paint and varnish coatings by method «crude on crude»] // Aviacionnye materialy i tehnologii. 2013. №4. S. 39–42.
  13. Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Lakokrasochnye pokrytiya dlya zashhity metallicheskih i polimernyh kompozicionnyh materialov ot stareniya, korrozii i biopovrezhdeniya [Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration] // Aviacionnye materialy i tehnologii. 2017. №S. S. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
  14. Semenova L.V., Novikova T.A., Nefedov N.I. Klimaticheskaya stojkost i starenie lakokrasochnogo pokrytiya [Climatic stability and ageing paint coating] // Aviacionnye ma-terialy i tehnologii. 2014. №S3. S. 31–34. DOI: 10.18577/2071-9140-2017-0-S-393-404.
  15. Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Sistemy lakokrasochnyh pokrytij dlya vertoletnoj tehniki [Systems of paint coatings for helicopter equipment] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
  16. Livshic M.L., Pshiyalkovskij B.I. Lakokrasochnye materialy: spravochnoe posobie [Paint and varnish materials: handbook]. M.: Himiya, 1982. 360 s.
  17. Patton T.K. Tehnologiya alkidnyh smol. Sostavlenie receptur i raschety [Technology of the alkyd pitches. Creation of compoundings and calculations]. M.: Himiya, 1970. 128 s.
  18. Antislip coating materials: pat. KR20150024368 (A); publ. 06.03.15.
  19. Antiskid elastic coating and mfg. technology thereof: pat. CN1483518 (A); publ. 24.03.04.
  20. Williamson N., O’Donoghue M., Datta V.J. Overview of Anti-Slip Coatings for Structural Steel // Journal of Protective Coatings & Linings. 2003. June. P. 41–49. Available at: http://www.paintsquare.com/jpcl/ (accessed: March 20, 2018).
  21. Alifanov E.V., Chajkun A.M., Gorlov D.S., Venediktova M.A. Osobennosti mehanizma treniya elastomernyh materialov razlichnyh tipov. Teoreticheskie i prakticheskie aspekty (obzor) [Features of the mechanism of friction of elastomeric materials of different types. Theoretical and practical aspects (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №1 (61). St. 08. Available at: http://www.viam-works.ru (accessed: March 20, 2018). DOI: 10.18577/2307-6046-2018-0-1-8-8.