Ways of increasing corrosion resistance of superalloys (review)

Bazyleva O.A., Arginbaeva E.G., Lutskaya S.A.
Bazyleva O.A., Arginbaeva E.G., Lutskaya S.A. Ways of increasing corrosion resistance of superalloys (review) // Proceedings of VIAM. 2018. No. 4. DOI: 10.18577/2307-6046-2018-0-4-3-8. URL: https://www.viam-works.ru/en/journal/2018/4/1
Keywords
nickel alloys, intermetallic, alloying, corrosion resistance, heat resistance, rare earth elements.
Abstract

Ni-based superalloys are widely used in the aviation, energy and nuclear industries. They are used in conditions of high temperatures, stresses and corrosive medium, which is why the issue of oxidation resistance is actual. The article describes the results of recent studies aimed at increasing the corrosion resistance of high-temperature Ni-based alloys. Traditionally, the issue of increasing corrosion resistance is solved by a variation in the chemical composition. Elements such as aluminum and chromium contribute to the formation of a complex oxide film on the metal surface. This has a beneficial effect on the operational characteristics of the alloy. When analyzing the literature data, the results of studies carried out by the authors on intermetallic alloys were confirmed: doping of alloys with refractory elements such as Mo and Re has a negative effect on the corrosion resistance. Most actively carried out research work in the direction of additional alloying of materials with

Reference list
  1. Kablov E.N. Litejnye zharoprochnye splavy. Effekt S.T. Kishkina [Foundry hot strength alloys. Kishkin's effect]. M.: Nauka, 2006. 272 s.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlya perspektivnyh aviacionnyh GTD [Cast heat resisting nickel alloys for perspective aviation GTE] // Tehnologiya legkih splavov. 2007. №2. S. 6–16.
  3. Ospennikova O.G. Itogi realizacii strategicheskih napravlenij po sozdaniyu novogo pokoleniya zharoprochnyh litejnyh i deformiruemyh splavov i stalej za 2012–2016 gg. [Implementation results of the strategic directions on creation of new generation of heat-resisting cast and wrought alloys and steels for 2012–2016] // Aviacionnye materialy i tehnologii. 2017. №S. S. 17–23. DOI: 10.18577/2071-9140-2017-0-S-17-23.
  4. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Tendencii razvitiya intermetallidnyh splavov na osnove nikelya [Development trends of nickel-based intermetallic alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  5. Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Alloys based on nickel aluminides // Metal Science and Heat Treatment. 1999. Vol. 41. No. 1–2. P. 36–38.
  6. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  7. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  8. Padture N.P., Gell M., Jordan E.H. Thermal barrier coatings for gas-turbine engine appli-cations // Science. 2002. Vol. 296. P. 280–284.
  9. Yun D.W., Seo S.M., Jeong H.W. et al. The cyclic oxidation behavior of Ni-based superalloy GTD-111 with sulphur impurities at 1100°C // Corrosion Science. 2015. Vol. 90. P. 392–401.
  10. Payet M., Marchetti L., Tabarant M., Chevalier J.-P. Corrosion mechanism of a Ni-based alloy in supercritical water: Impact of surface plastic deformation // Corrosion Science. 2015. Vol. 100.
  11. P. 47–56.
  12. Cheng H., Leng B., Chen K. et al. EPMA and TEM characterization of intergranular tellurium corrosion of Ni–16Mo–7Cr–4Fe superalloy // Corrosion Science. 2015. Vol. 97. P. 1–6.
  13. Xu Y., Yan J., Sun F. et al. Effect of further alloying elements on corrosion resistance of Ni–Cr alloys in molten glass // Corrosion Science. 2016. Vol. 112. P. 647–656.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. He J., Zhang Z., Peng H. et al. The role of Dy and Hf doping on oxidation behavior of two-phase (γ+β) Ni–Al alloys // Corrosion Science. 2015. Vol. 98. P. 699–707.
  16. Li D., Guo H., Wang D. et al. Cyclic oxidation of β-NiAl with various reactive element dopants at 1200°C // Corrosion Science. 2013. Vol. 66. P. 125–135.
  17. Guo H., Li D., Zheng L. et al. Effect of co-doping of two reactive elements on alumina scale growth of β-NiAl at 1200°C // Corrosion Science. 2014. Vol. 88. P. 197–208.
  18. Kablov D.E., Sidorov V.V., Budinovskij S.A., Min P.G. Vliyanie primesi sery na zharostojkost monokristallov zharoprochnogo splava ZhS36-VI s zashhitnym pokrytiem [The influence of sulfur impurity on heat resistance of single crystals of ZhS36-VI alloy with protective coating] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 20–23. DOI: 10.18577/2071-9140-2016-0-1-20-23.
  19. Brenneman J., Wei J., Sun Z. et al. Oxidation behavior of GTD111 Ni-based super alloy at 900°C in air // Corrosion Science. 2015. Vol. 100. P. 267–274.
  20. Yan K., Guo H., Gong S. High-temperature oxidation behavior of β-NiAl with various reactive element dopants in dry and humid atmospheres // Corrosion Science. 2014. Vol. 83. P. 335–342.
  21. Fuhrmann L., Konrad C.H., Völkl R., Glatzel U. Transition from internal to external oxidation in binary Ni–Zr and ternary Ni–Zr–Y alloys // Corrosion Science. 2015. Vol. 94. P. 218–223.
  22. He J., Luan Y., Guo H. et al.The role of Cr and Si in affecting high-temperature oxidation behavior of minor Dy doped NiAl alloys // Corrosion Science. 2013. Vol. 77. P. 322–333.
  23. Liu R.D., Jiang S.M., Yu H.J. et al. Preparation and hot corrosion behaviour of Pt modified AlSiY coating on a Ni-based superalloy // Corrosion Science. 2016. Vol. 104. P. 162–172.
  24. Han B., Ma Y., Peng H. et al. Effect of Mo, Ta, and Re on high-temperature oxidation behavior of minor Hf doped NiAl alloy // Corrosion Science. 2016. Vol. 102. P. 222–232.
  25. Pint B.A., More K.L., Wright I.G. Effect of quaternary additions on the oxidation behavior of Hf-doped NiAl // Oxidation of Metals. 2003. Vol. 59. P. 257–283.
  26. Cruchley S., Taylor M.P., Ding R. et al. Comparison of Chromia Growth Kinetics in a Ni-based Superalloy, with and without Shot-peening // Corrosion Science. 2015. Vol. 100. P. 242–252.
  27. Tolpygo V.K., Clarke D.R. Microstructural study of the theta-alpha transformation in alumina scales formed on nickel-aluminides // High Temperature Material Processes. 2000. Vol. 100. P. 59–70.
  28. Yang L., Zheng L., Guo H. The residual stress of oxide scales grown on Ni–Al alloys doped with minor Dy and Y // Corrosion Science. 2016. Vol. 112. P. 542–551.
  29. Huang Y., Peng X. The promoted formation of an α-Al2O3 scale on a nickel aluminide with surface Cr2O3 particles // Corrosion Science. 2016. Vol. 112. P. 226–232.