Investigation of the modification shungite of carbon plastic on the basis of epoxy matrix

Bolshakov V.A., Antyufeeva N.V.
Bolshakov V.A., Antyufeeva N.V. Investigation of the modification shungite of carbon plastic on the basis of epoxy matrix // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-103-110. URL: https://www.viam-works.ru/en/journal/2018/3/12
Keywords
thermoanalysis, polymeric composite materials, schungites, thermal conductivity, electrical conductivity, kinetics of curing, thermogravimetry.
Abstract

Structural polymeric composite materials on the set of characteristics are at a level, and sometimes exceed the characteristics of other structural materials. Recently, modification of polymer composites by carbon nanoparticles is of particular interest, but due to their high cost and limited volume, a number of difficulties in their application may arise. Shungites are a natural rock containing fulleroid nanostructures. In addition, they have a significantly lower cost compared to synthesized carbon nanoparticles and their use in large volumes is not difficult. The purpose of this work is to study the effect of modification of polymeric composites with shungite.

Reference list
  1. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coalplastics and fibreglasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://www.viam-works.ru (accessed: February 07, 2018).
  2. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Aleksashin V.M., Gunyaev G.M., Ilchenko S.I. i dr. Vliyanie proizvodnyh fullerena S60 na svojstva polimernoj matricy uglerodnogo kompozita [Influence of derivatives of C60 fullerene on properties of polymeric matrix of carbon composite] // Nanotehnika. 2004. №4. S. 89.
  4. Harris P. Uglerodnye nanotruby i rodstvennye struktury. Novye materialy XXI veka [Carbon nanopipes and related structures. New materials of the XXI century.]. M.: Tehnosfera, 2003. S. 10–28.
  5. Gunyaev G.M., Komarova O.A., Ilchenko S.I. i dr. Fulleroidnye nanomaterialy – aktivnye strukturnye modifikatory polimerov i polimernyh kompozitov [Fulleroidnye nanomaterials – active structural modifiers of polymers and polymeric composites] // Plasticheskie massy. 2003. №10. S. 18–21.
  6. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional carbon plastics carbon nanoparticles] // Rossijskij himicheskij zhurnal. 2010. T. 54. №1. S. 3–11.
  7. Gojnya F.H., Wichmanna M.G.H., Fiedlera B. et. al. Influence of nano-modification on the mechanical and electrical properties of conventional fibre-reinforced composites // Compo-sites: Part A. 2005. Vol. 36. P. 1525–1535.
  8. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  9. Aldoshin S.M., Badamshina E.R., Kablov E.N. Polimernye nanokompozity – novoe pokolenie polimernyh materialov s povyshennymi ekspluatacionnymi harakteristikami [Polymeric nanocomposites – new generation of polymeric materials with the increased utilization properties] // I Mezhdunar. forum po nanotehnologiyam «Rosnanoteh 08»: sb. tez. dokl. nauch.-tehnologich. sekcij. M., 2008. S. 385–387.
  10. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  11. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Buznik V.M., Kablov E.N. Tehnologii polucheniya i adaptacii materialov dlya primeneniya v Arktike [Technologies of receiving and adaptation of materials for application in the Arctic] // V Mezhdunar. konferenciya-shkola po himicheskoj tehnologii: sb. tez. dokl. satellitnoj konf. HH Mendeleevskogo sezda po obshhej i prikladnoj himii. M., 2016. S. 9–10.
  13. Antyufeeva N.V., Aleksashin V.M., Zhelezina G.F., Stolyankov Yu.V. Metodicheskie podhody termoanaliticheskih issledovanij dlya ocenki svojstv prepregov i ugleplastikov [Me-thodical approaches of thermoanalytical researches for assessment of properties of prepregs and coal plastics] // Prilozhenie k zhurnalu «Vse materialy. Enciklopedicheskij spravochnik». 2012. №4. S. 18–27.
  14. Kondrashov S.V., Gunyaeva A.G., Shashkeev K.A., Barinov D.Ya., Soldatov M.A., Shevchenko V.G., Muzafarov A.M. Elektroprovodyashhie gibridnye polimernye kompozicionnye materialy na osnove nekovalentno funkcionalizirovannyh uglerodnyh nanotrubok [Electrically-conductive hybrid polymer composite materials on the basis of noncovalent functional carbon nanotubes] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №2. St. 10. Available at: http://www.viam-works.ru (accessed: February 07, 2018). DOI: 10.18577/2307-6046-2016-0-2-10-10.
  15. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.