Effect of samples parameters on mechanical properties of heat-resistant titanium and nickel alloys

Golinets S.A, Gorbovets M.A., Karanov V.A.
Golinets S.A, Gorbovets M.A., Karanov V.A. Effect of samples parameters on mechanical properties of heat-resistant titanium and nickel alloys // Proceedings of VIAM. 2018. No. 3. DOI: 10.18577/2307-6046-2018-0-3-86-94. URL: https://www.viam-works.ru/en/journal/2018/3/10
Keywords
titanium alloys, nickel alloys, samples parameters, tension test, stress-rupture, mechanical properties.
Abstract

As is well known, for tension test and stress-rupture test of titanium alloys applying to compressor blades and discs, in most cases are used the standard samples with 5 mm diameter and 25 mm gauge length. In a construction of gas turbine engines are applied the compressor blades of the small sizes made of fine dimensional stampings that causes the necessity of monitoring procedure of material of these compressor blades on small samples with a diameter of 3 mm and gage length of 15 mm. This work is devoted to effect of samples parameters on short-term strength and stress-rupture characteristics of heat-resistant titanium alloys VT3-1, VT9, VT18 and nickel alloys VGL12U, GS6U.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  3. Inozemcev A.A., Bashkatov I.G., Koryakovcev A.S. Titanovye splavy v izdeliyah razrabotki OAO «Aviadvigatel» [Titanium alloys in products of development of JSC «Aviadvigatel»] // Sovremennye titanovye splavy i problemy ih razvitiya: sb. M.: VIAM, 2010. S. 43–46.
  4. Kresanov Yu.S., Kachan A.Ya., Chigirinskij V.V., Ben A.N. Vliyanie parametrov goryachego vydavlivaniya zagotovok rabochih lopatok kompressora na kachestvo ih izgotovleniya [Influence of parameters of hot extrusion of preparations of working compressor blades on quality of their manufacturing] // Vestnik dvigatelestroeniya. 2009. №2. S. 108–115.
  5. Boguslaev V.A., Muravchenko F.M., Zhemanyuk P.D. i dr. Tehnologicheskoe obespechenie ekspluatacionnyh harakteristik detalej GTD [Technological support of utilization properties of details of GTE]. Zaporozhe: Motor Sich, 2003. Ch. 1: Lopatki kompressora i ventilyatora. 420 s.
  6. Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Vliyanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlya lopatok KVD [Influence of modes of thermal processing on structure and property of heat resisting titanium alloy for KVD blades] // Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.
  7. Kablov E.N., Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Razrabotka opytno-promyshlennoj tehnologii izgotovleniya polufabrikatov iz psevdo-α-titanovogo splava VT41 [Development of trial manufacturing techniques of semi-finished products from псевдо-α-титанового alloy ВТ41] // Titan. 2016. №2 (52). S. 33–42.
  8. Gejkin V.A. Razrabotka tehnologij dlya novyh materialov v dvigatelestroenii [Development of technologies for new materials in engine building] // Dvigatel. 2017. №3. S. 10–11.
  9. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye splavy novogo pokoleniya [Foundry hot strength alloys of new generation] // 75 let. Aviacionnye materialy. M.: VIAM, 2007. S. 27–44.
  10. Sidorov V.V., Kablov D.E., Rigin V.E. Metallurgiya litejnyh zharoprochnyh splavov: tehnologiya i oborudovanie / pod obshh. red. E.N. Kablova [Metallurgy of foundry hot strength alloys: technology and equipment / gen. ed. by E.N. Kablov]. M.: VIAM, 2016. S. 10–11.
  11. Solonina O.P., Glazunov S.G. Zharoprochnye titanovye splavy [Heat resisting titanium alloys]. M.: Metallurgiya, 1976. 448 s.
  12. Popov A.A., Popova M.A. Izotermicheskie diagrammy vydeleniya silicidnyh i alyuminidnyh faz v zharoprochnyh titanovyh splavah [Isothermal charts of allocation of silicide and aluminide phases in heat resisting titanium alloys] // Metallovedenie i termicheskaya obrabotka metallov. 2016. №11 (737). S. 23–28.
  13. Osobennosti ekspluatacii litejnyh zharoprochnyh nikelevyh splavov i predyavlyaemye k nim trebovaniya // Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya / pod obshh. red. E.N. Kablova. 2-e izd. [Features of operation of cast heat resisting nickel alloys and demands made to them / gen. ed. by E.N. Kablov. 2nd ed.]. M.: Nauka, 2006. S. 19–34.
  14. Duhl D.N. Directionally solidified superalloys // Superalloys II. N.Y.: Wiley-Interscience, 1987. P. 189–214.
  15. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  16. Goryunov A.V., Rigin V.E. Sovremennaya tehnologiya polucheniya litejnyh zharoprochnyh nikelevyh splavov [The modern technology of cast nickel base superalloys production] // Aviacionnye materialy i tehnologii. 2014. №2. S. 3–7.
  17. Solovyev A.E., Golynets S.A., Khvatsky K.K., Aslanyan I.R. Provedenie staticheskih ispytanij pri rastyazhenii na mashinah firmy Zwick/Roell [Performing of static tensile tests on Zwick/Roell machines] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 12. Available at: http://viam-works.ru (accessed: February 27, 2018). DOI: 10.18577/2307-6046-2015-0-8-12-12.
  18. Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Prochnostnye ispytaniya i issledovaniya aviacionnyh materialov [Strength tests and researches of aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.