Interaction of model compositions with plastic equipment made using 3D printing technology

Vlasova K.A., Klyukvina T.D., Leonov A.A., Larionov S.A.
Vlasova K.A., Klyukvina T.D., Leonov A.A., Larionov S.A. Interaction of model compositions with plastic equipment made using 3D printing technology // Proceedings of VIAM. 2018. No. 2. DOI: 10.18577/2307-6046-2018-0-2-7-7. URL: https://www.viam-works.ru/en/journal/2018/2/7
Keywords
model composition, ABS plastic, shrinkable shell, investment casting, wax, separation coating.
Abstract

This article discusses the interaction of the model composition and plastic equipment. An experiment was conducted with the participation of three model compositions, different in composition and properties, using the example of a thin-walled shaped casting of «Kronstejn» component, manufactured by investment casting. Differences in the tendency of model compositions to form shrinkage shells were revealed. A comparative analysis of the experimental results was carried out. Based on the results of the experiment, the optimal model composition for the production of «Kronstein» casting model was selected.

Reference list
  1. Ivanov V.N., Kazennov S.A., Kurchman B.S. i dr. Lite po vyplavlyaemym modelyam. 3-e izd., pererab. i dop. [Investment casting. 3rd prod., reslave. and additional. 3rd ed., rev. and add.]. M.: Mashinostroenie, 1984. 408 s.
  2. Truhov A.P., Sorokin A.Yu., Ershov M.Yu. i dr. Tehnologiya litejnogo proizvodstva: Lite v peschanye formy: ucheb. [Technology of foundry production: Sand casting: textbook]. M.: Akademiya, 2005. 528 s.
  3. Ivanov V.N. Slovar-spravochnik po litejnomu proizvodstvu [The dictionary reference on foundry production]. M.: Mashinostroenie, 1990. 384 s.
  4. Metally i splavy: spravochnik / pod red. Yu.P. Solnceva [Metals and alloys: directory / ed. by Yu.P. Solncev]. SPb.: Professional, Mir i semya, 2003. 1066 s.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dinamika razvitiya magnievyh i litejnyh alyuminievyh splavov [Dynamics of the development of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
  7. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  8. Kablov E.N. Additivnye tehnologii – dominanta nacionalnoj tehnologicheskoj iniciativy [The additive technologies – dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
  9. Petrova G.N., Sapego Yu.A., Larionov S.A., Platonov M.M., Laptev A.B. Pozharobezopasnye termoplastichnye materialy dlya 3D-tehnologii [Fireproof thermoplastic materials for 3D-technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №9 (57). St. 07. Available at: http://www.viam-works.ru (accessed: January 29, 2018). DOI: 10.18577/2307-6046-2017-0-9-7-7.
  10. Petrova G.N., Larionov S.A., Sapego Yu.A., Platonov M.M. Reologicheskie svojstva termoplastichnoj kompozicii na osnove polikarbonata: zavisimost ot temperatury pererabotki; vliyanie na mehanicheskie harakteristiki i razmernuyu stabilnost obektov, sozdannyh po FDM-tehnologii [Rheological properties of the thermoplastic composition with a reduced fire hazard polycarbonate-based: depending on the temperature processing; effect on mechanical properties and stability dimension objects created software FDM-technology] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4. St. 09. Available at: http://viam-works.ru (accessed: January 29, 2018). DOI: 10.18577/2307-6046-2017-0-4-9-9.
  11. Lakedemonskij A.V., Kvasha F.S., Mendeleev Ya.I. i dr. Litejnye defekty i sposoby ih ustraneniya [Foundry defects and ways of their elimination]. M.: Mashinostroenie, 1972. 152 s.
  12. Ozerov V.A., Garanin V.F. Lite povyshennoj tochnosti po razovym modelyam: ucheb. posobie [Enhanced accuracy molding on one-time models: manual]. M.: Vysshaya shkola, 1988. 87 s.
  13. Petrova G.N., Larionov S.A., Platonov M.M., Perfilova D.N. Termoplastichnye materialy novogo pokoleniya dlya aviacii [Thermoplastic materials of new generation for aviation] // Aviacionnye materialy i tehnologii 2017. №S. S. 420–436. DOI: 10.18577/2071-9140-2017-0-S-420-436.
  14. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  15. Ospennikova O.G. Issledovanie vliyaniya napolnitelej na svojstva i stabilnost modelnyh kompozicij, vybor optimalnyh sostavov [Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures] // Aviacionnye materialy i tehnologii. 2014. №3. S. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.
  16. Ospennikova O.G. Issledovanie i razrabotka parametrov tehnologicheskogo processa izgotovleniya modelej iz modelnyh kompozicij na osnove sinteticheskih voskov [Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes] // Aviacionnye materialy i tehnologii. 2014. №3. S. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.