Thin-walled structural component soldering by amorphous tape solder VPr51

Stolyankov Yu.V., Lukin V.I., Afanasiev-Khodykin A.N.
Stolyankov Yu.V., Lukin V.I., Afanasiev-Khodykin A.N. Thin-walled structural component soldering by amorphous tape solder VPr51 // Proceedings of VIAM. 2018. No. 2. DOI: 10.18577/2307-6046-2018-0-2-3-3. URL: https://www.viam-works.ru/en/journal/2018/2/3
Keywords
amorphous tape solder material, thin-walled structural component, brazing.
Abstract

In the article some peculiar structure features and properties of the amorphous tape solder on the basis of the nickel alloy (VPr51) are provided. The solder engineered for the thin-walled structural component brazing made from stainless steels and nickel-based alloys. Some data related to the solder alloy composition, its brazing conditions (i. e. temperature and delay time), technological properties (flowing and wetting), erosive activity to the stainless steels and strength characteristics of soldered joints are brought here in the article as well.

Reference list
  1. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Stolyankov Yu.V., Lukin V.I., Rylnikov V.S. Amorfnye metallicheskie pripoi [Amorphous metal solders] // Tez. dokl. mezhotr. nauch.-praktich. konf. «Problemy sozdaniya novyh materialov dlya aviakosmicheskoj otrasli v XXI veke». M.: VIAM, 2002. S. 48–49.
  4. Lukin V.I., Stolyankov Yu.V., Rylnikov V.S., Shherbakov A.I. Pajka amorfnymi pripoyami [Soldering amorphous solders] // Aviacionnye materialy i tehnologii. 2002. №4. S. 96–102.
  5. Lukin V.I., Rylnikov V.S., Stolyankov Yu.V., Shherbakov A.I. Bystrozakalennye zharoprochnye pripoi na osnove titana i nikelya [The fast-tempered heat resisting solders on the basis of titanium and nickel] // Tez. dokl. Mezhdunar. nauch.-tehnich. konf. «Aktualnye voprosy aviacionnogo materialovedeniya» M.: VIAM, 2007. S. 25–26.
  6. Fizikohimiya amorfnyh (stekloobraznyh) metallicheskih materialov / pod red. Yu.K. Kovneristogo [Physics chemistry amorphous (glass figurative) metal materials / ed. by Yu.K. Konevristiy]. M.: Metallurgiya, 1987. 328 s.
  7. Amorfnye metallicheskie materialy [Amorphous metal materials]. M.: Nauka, 1984. 158 s.
  8. Sudzuki K., Fudzimori H., Hasimoto K. Amorfnye metally [Amorphous metals]. M.: Metallurgiya, 1987. 328 s.
  9. Kovneristyj Yu.K., Osipov E.K., Trofimova E.A. Fiziko-himicheskie osnovy sozdaniya amorfnyh metallicheskih splavov [Physical and chemical bases of creation of amorphous metal alloys]. M.: Nauka, 1983. 145 s.
  10. Amorfnye metallicheskie splavy. Per. s angl. / pod red. F.E. Lyuborskogo [Amorphous metal alloys. Trans. for Engl. / ed. by F.E. Lyuborskiy]. M.: Metallurgiya, 1987. 584 s.
  11. Polk D.E., Gissen B.K. Metallicheskie stekla. Per. s angl. [Metal glasses. Trans from Engl.]. M.: Metallurgiya, 1984. S. 12–39.
  12. Stolyankov Yu.V., Aleksashin V.M., Antyufeeva N.V. K voprosu ob ocenke sklonnosti metallicheskih sistem k stekloobrazovaniyu (obzor) [On the question of glass-forming ability tendency evaluation (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №7. St. 08. Available at: http://www.viam-works.ru (accessed: December 20, 2017). DOI: 10.18577/2307-6046-2015-0-7-8-8.
  13. Stolyankov Yu.V., Aleksashin V.M., Antyufeeva N.V., Shheglova T.M. Ocenka stekloobrazuyushhej sposobnosti metallicheskoj sistemy na osnove nikelya tipa «metall–metalloid» [Glass-forming ability evaluation of the nickel-based «metall–metalloid» system] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 66–71. DOI: 10.185.77/2071-9140-2016-0-1-66-71.
  14. Afanasev-Hodykin A.N., Lukin V.I., Rylnikov V.S. Vysokotehnologichnye polufabrikaty zharoprochnyh pripoev (lenty i pasty na organicheskom svyazuyushhem) [High-tech semi-finished high-temperature solders (tape and paste on an organic binder] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 02. Available at: http://www.viam-works.ru (accessed: December 20, 2017).
  15. Kablov E.N., Lukin V.I., Ospennikova O.G. Svarka i pajka v aviakosmicheskoj promyshlennosti [Welding and the soldering in the aerospace industry] // Tr. Vseros. nauch.-praktich. konf. «Svarka i bezopasnost». Yakutsk: IFTPS SO RAN, 2012. S. 21–30.
  16. Rylnikov V.S., Lukin V.I. Pripoi, primenyaemye dlya pajki materialov aviacionnogo naznacheniya [Solders used for soldering materials aviation applications] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 02. Available at: http://viam-works.ru (accessed: December 20, 2017).
  17. Stolyankov Yu.V., Antyufeeva N.V., Raskutin A.E., Karimova S.A. Issledovanie vozmozhnosti sozdaniya sloistyh metallopolimernyh kompozicionnyh materialov s ispolzovaniem tonkolistovyh amorfnyh splavov [Research of possibility of creation of layered metalpolymeric composite materials with usage thin sheet amorphous alloys] // Kompozity i nanostruktury. 2014. T. 6. №1. S. 25–31.
  18. Stolyankov Yu.V., Gulyaev I.N., Aleksashin V.M., Antyufeeva N.V. Amorfnye metallicheskie materialy v sostave pezoelektricheskih sloistyh elementov-aktyuatorov [Amorphous metal materials in piezoelectric laminated actuators components] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 03. Available at: http://viam-works.ru (accessed: December 20, 2017). DOI: 10.18577/2307-6046-2015-0-4-3-3.