Application of atomic emission spectrometry with inductively coupled plasma for the analysis of electrolytes during electrolytic extraction of the phases of nickel alloys

Dvoretskov R.M., Baranovskaya V.B., Mazalov I.S., Karachevtsev F.N.
Dvoretskov R.M., Baranovskaya V.B., Mazalov I.S., Karachevtsev F.N. Application of atomic emission spectrometry with inductively coupled plasma for the analysis of electrolytes during electrolytic extraction of the phases of nickel alloys // Proceedings of VIAM. 2018. No. 12. DOI: 10.18577/2307-6046-2018-0-12-107-120. URL: https://www.viam-works.ru/en/journal/2018/12/12
Keywords
atomic emission spectrometry, inductively coupled plasma, electrolyte analysis, phase extraction, electrolytic dissolution, anodic residue, phase analysis, heat resistant nickel alloys.
Abstract

To improve the accuracy of quantitative evaluation of the phase composition of high-alloyed alloys, electrolytic phase extraction is used, which includes anodic dissolution of the alloy sample in a specially selected electrolyte for passivation of the corresponding components, study of the phase and chemical composition of the passivated anodic residue and using the results of these studies for calculating the mass fraction of phases in the sample alloy and distribution of elements between phases. A scheme has been proposed for studying the quantitative phase composition of nickel alloys using electrolytic extraction of phases in which the chemical composition of the anodic residue is determined by the difference in the concentrations of elements in the alloy and in the electrolyte after the extraction. To determine the elements dissolved in the electrolyte, the method of atomic emission spectrometry with inductively coupled plasma was used. The model solutions were used to investigate the interfering effects of the components of five electrolytes in the inductively coupled plasma atomic emission analysis of electrolytes after electrolytic extraction of the phases of nickel alloys. In order to minimize the influence of electrolyte components on the analytical signal of the elements being detected, it is recommended to electrolytically dissolve samples of nickel alloys to a mass of not less than 0.25 g per 250 ml of electrolyte, so that the electrolyte can be diluted. Methods for compensating disturbing influences are chosen - using solutions of standard samples of nickel alloys and internal standardization. An internal standard line Indium 230.606 nm is selected. The suitability of the presented research scheme for evaluation of the quantitative phase composition of samples of ZhS6K and VZh159 alloys using electrolytic extraction and inductively coupled plasma atomic emission analysis of the electrolytes was carried out. A compari

Reference list
  1. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resursosberegayushchiye tekhnologii vyplavki perspektivnykh liteynykh i deformiruyemykh superzharoprochnykh splavov s uchetom pererabotki vsekh vidov otkhodov [Resource-saving technologies for smelting promising casting and wrought superhigh-strength alloys with regard to processing all types of waste] // Elektrometallurgiya. 2016. №9. S. 30–41.
  2. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Monokristallicheskij zharo-prochnyj nikelevyj splav novogo pokoleniya s nizkoj plotnostyu [Single-crystal nickel-based superalloy of a new generation with low-density] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  3. Shein E.A. Tendentsii v oblasti legirovaniya i mikrolegirovaniya zharoprochnykh monokris-tallicheskikh splavov na osnove nikelya (obzor) [Tendencies in the field of alloying and microalloying of heat resisting single-crystal alloys on the basis of nickel (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №3. St. 02. Available at: http://viam-works.ru (accessed: November 10, 2018). DOI: 10.18557/2307-6046-2016-0-3-2-2.
  4. Kuznetsov V.P., Lesnikov V.P., Popov N.A., Vasilyev A.S., Popova Ye.N. Fazovyye prev-rashcheniya v monokristallicheskom zharoprochnom nikelevom splave, legirovannom tan-talom, reniyem i ruteniyem [Phase transformations in a single-crystal superalloy nickel alloy doped with tantalum, rhenium and ruthenium] // Metallovedeniye i termicheskaya obrabotka metallov. 2018. №2 (752). S. 41–46.
  5. Solntsev Yu.P., Pryakhin E.I. Materialovedeniye [Materials Science]. SPb.: Khimizdat, 2007. S. 144–159.
  6. Kablov E.N., Golubovskiy Ye.R. Zharoprochnost nikelevykh splavov [Heat resistance of nickel alloys]. M.: Mashinostroyeniye, 1998. 464 s.
  7. Chabina E.B., Lomberg B.S., Filonova E.V., Ovsepyan S.V., Bakradze M.M. [Change of structural and phase condition of heat resisting deformable nickel alloy at alloying tantalum and rhenium] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 03. Available at: http://www.viam-works.ru (accessed: November 10, 2018). DOI: 10.18577/2307-6046-2015-0-9-3-3
  8. Petrushin N.V., Elyutin E.S., Nazarkin R.M., Pakhomkin S.I. i dr. Segregatsiya legiruyush-chikh elementov v napravlenno zakristallizovannykh zharoprochnykh nikelevykh splavakh, soderzhashchikh reniy i ruteniy [Segregation of alloying elements in directionally crystallized nickel-containing superalloys containing rhenium and ruthenium] // Voprosy ma-terialovedeniya. 2015. №1 (81). S. 27–37.
  9. Kurikhina T.V. Kinetika obrazovaniya klasterov fazy Ni3Al pri raspade tverdogo rastvora [The kinetics of the formation of clusters of the Ni3Al phase during decomposition of the solid solution] // Rossiyskiye nanotekhnologii. 2015. T. 10. №1–2. S. 72–75.
  10. Sims CH., Khagel V. Zharoprochnyye splavy [High-temperature alloys]. M.: Metallurgiya, 1976. 568 s.
  11. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Ten-dencii razvitiya intermetallidnyh splavov na osnove nikelya [Development trends of nickel-based intermetallic alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  12. Morozova G.I. Fenomen γ-fazy v zharoprochnykh nikelevykh splavakh [The γ-phase phenomenon in heat-resistant nickel alloys] // Doklady akademii nauk SSSR. 1992. T. 325. №6. C. 1193–1198.
  13. Kolobov Yu.R., Kablov E.N., Kozlov E.V., Koneva N.A. i dr. Struktura i svoystva interme-tallidnykh materialov s nanofaznym uprochneniyem [Structure and properties of intermetallic materials with nanophase hardening]. M.: Izd. dom MISiS, 2008. S. 41–45.
  14. Petrushin N.V., Visik E.M., Gorbovets M.A., Nazarkin R.M. Strukturno-fazovyye kharakter-istiki i mekhanicheskiye svoystva monokristallov zharoprochnykh nikelevykh reniysoderzhashchikh splavov s intermetallidno-karbidnym uprochneniyem [Structural-phase characteristics and mechanical properties of single crystals of heat-resistant nickel-rhenium-containing alloys with intermetallic-carbide hardening] // Metally. 2016. №4. S. 57–70.
  15. Zaitsev D.V., Treninkov I.A., Alekseev A.A. Ultradispersnye plastinchatye vydeleniya v zharoprochnyh nikelevyh splavah [Ultrafine lamellar precipitation in Ni-based superalloys] // Aviacionnye materialy i tehnologii. 2015. №1. S. 49–55.
  16. Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov M.R. Neobratimyye iz-meneniya tonkoy struktury monokristallov zharoprochnykh nikelevykh splavov v protsesse dlitelnoy ekspluatatsii turbinnykh lopatok [The irreversible structural modification of single crystals fine structure of Ni-based superalloys at enduring operation of turbine blades] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2015. №12. St. 03. Available at: http://www.viam-works.ru (accessed: November 10, 2018). DOI: 10.18577/2307-6046-2015-0-12-3-3.
  17. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. Metallurgicheskie osnovy obespecheniya vysokogo kachestva monokristallicheskih zharoprochnyh nikelevykh splavov [The metal-lurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel al-loys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  18. Morozova G.I. Kompensatsiya disbalansa legirovaniya zharoprochnykh nikelevykh splavov [Compensation of imbalance in alloying of heat-resistant nickel alloys] // MiTOM. 2012. №12. C. 52–56.
  19. Umanskiy Ya.S., Skakov Yu.A. i dr. Kristallografiya, rentgenografiya i elektronnaya mikros-kopiya [Crystallography, radiography and electron microscopy]. M.: Metallurgiya, 1982. 632 s.
  20. Nazarkin R.M. Rentgenodifrakcionnye metodiki precizionnogo opredeleniya parametrov kristallicheskih reshetok nikelevyh zharoprochnyh splavov (kratkij obzor) [X-ray diffraction techniques for precise determination of lattice constants in Ni-based superalloys: a brief review] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 41–48.
  21. Malakhov V.V. Problemy diagnostiki funktsionalnykh materialov (obzor) [Problems of diagnostics of functional materials (review)] // Zavodskaya laboratoriya Diagnostika materi-alov. 2011. T. 77. №2. S. 3–10.
  22. Chabina Ye.B., Zaytsev D.V., Alekseyev A.A., Sbitneva S.V. Issledovaniye struktury i raz-rabotka komplekta standartnykh obraztsov sostava i struktury zharoprochnykh nikelevykh i intermetallidnykh splavov [Study of the structure and development of a set of standard sam-ples of the composition and structure of high-temperature nickel and intermetallic alloys] // Standartnyye obraztsy. 2016. №1. S. 21–30.
  23. Rid S.Dzh.B. Elektronno-zondovyy mikroanaliz i rastrovaya elektronnaya mikroskopiya v geologii [Electron probe microanalysis and scanning electron microscopy in geology]. M.: Tekhnosfera, 2008. S. 17.
  24. Moroz A.N., Terekhov V.N., Kanyuka V.I. Metodicheskiye aspekty mikrorentgenospek-tralnogo analiza faz i vklyucheniy razmerom meneye 1 mkm v stalyakh i splavakh [Methodi-cal aspects of micro X-ray analysis of phases and inclusions smaller than 1 micron in steels and alloys] // Metallovedeniye i termicheskaya obrabotka metallov. 2008. №7 (637). S. 30–33.
  25. Morozova G.I. Znachenie metoda fiziko-himicheskogo fazovogo analiza v razvitii avi-acionnogo metallovedeniya i sozdanii zharoprochnyh nikelevyh splavov [The importance of physicochemical phase analysis technique in the development of aviation metallic material science and creation of Ni-based superalloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1 (37). St. 07. Available at: http://www.viam-works.ru (accessed: November 10, 2018). DOI: 10.18577/2307-6046-2016-0-1-50-55.
  26. Titov V.I., Tarasenko L.V., Utkina A.N., Shalkevich A.B. Fazovyy analiz novoy kompozitsii vysokoprochnoy konstruktsionnoy stali [Phase analysis of the new composition of high-strength structural steel] // Zavodskaya laboratoriya. Diagnostika materialov. 2015. T. 81. №2. S. 35–39.
  27. Golubtsova R.B. Fazovyy analiz nikelevykh splavov [Phase analysis of nickel alloys]. M.: Nauka, 1969. 234 s.
  28. ASTM E963–95. Standard Practice for Electrolytic Extraction of Phases from Ni and Ni–Fe Base Superalloys Using a Hydrochloric-Methanol Electrolyte. 2017. Available at: https://www.astm.org/Standards/E963.htm (accessed: November 12, 2018). DOI: 10.1520/E0963-95R17.
  29. Karpov Yu.A. Analiticheskiy kontrol metallurgicheskogo proizvodstva [Analytical control of metallurgical production]. M.: Metallurgiya, 1995. S. 97–107.
  30. Letov A.F., Karachevtsev F.N., Zagvozdkina T.N. Razrabotka kompleksa metodik izmereniy khimicheskogo sostava splavov na nikelevoy osnove [Development the set of methods measurements of the chemical composition of nickel-based alloys] // Trudy VIAM: el-ektron. nauch.-tekhnich. zhurn. 2018. №8 (68). S. 89–97. Available at: http://www.viam-works.ru (accessed: November 10, 2018). DOI: 10.18577/2307-6046-2018-0-8-89-97.
  31. Pupyshev A.A., Danilova D.A. Ispolzovaniye atomno-emissionnoy spektrometrii s in-duktivno-svyazannoy plazmoy dlya materialov i produktov chernoy metallurgii [Using atomic emission spectrometry with inductively coupled plasma for materials and products of ferrous metallurgy] // Analitika i kontrol. 2007. T. 11. №2–3. S. 131–181.
  32. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  33. Dvoretskov R.M., Karachevtsev F.N., Zagvozdkina T.N., Mekhanik E.A. Opredeleniye legiruyushchikh elementov nikelevykh splavov aviatsionnogo naznacheniya metodom AES-ISP v sochetanii s mikrovolnovoy probopodgotovkoy [Determination of alloying elements of nickel alloys for aviation purposes by AES-ICP method in combination with microwave sample preparation] // Zavodskaya laboratoriya. Diagnostika materialov. 2013. T. 79. №9. S. 6–9.
  34. Lashko N.F., Zaslavskaya L.V., Kozlova M.N. i dr. Fiziko-khimicheskiy fazovyy analiz staley i splavov [Physico-chemical phase analysis of steels and alloys]. M.: Metallurgiya, 1970. 476 s.
  35. Lee H.-Y., Demura M., Xub Y. et al. Selective dissolution of the g phase in a binary Ni(γ)/Ni3Al(γ) two-phase alloy // Corrosion Science. 2010. Vol. 52. P. 3820–3825.
  36. Bellot C., Lamesle P. Quantitative measurement of gamma prime precipitates in two indus-trial nickel-based superalloys using extraction and high resolution SEM imaging // Journal of Alloys and Compounds. 2013. Vol. 570. P. 100–103.
  37. Roy G. Baggerly Electrolytic phase extraction: A useful technique to evaluate precipitates in nitinol // Powder Diffraction. 2012. Vol. 27. No. 2. P. 136–139.
  38. Chylinska R., Garbiak M., Piekarski B. Electrolytic Phase Extraction in Stabilised Austenitic Cast Steel // Materials Science. 2005. Vol. 11. No. 4. P. 348–351.
  39. Li R.B., Yao M., Liu W.C., He X.C. Isolation and determination for δ, γ, γʺ phases in Inconel 718 alloy // Scripta Materialia. 2002. Vol. 46. P. 635–638.
  40. Lidin R.A. Konstanty neorganicheskikh veshchestv: spravochnik [Inorganic Constants: A Handbook]. M.: Drofa, 2006. C. 350–352.
  41. Lukina E.A., Bazaleyeva K.O., Petrushin N.V., Tsvetkova E.V. Osobennosti formirovaniya struktury zharoprochnogo nikelevogo splava ZhS6K-VI pri selektivnom lazernom plavlenii [Features of the formation of the structure of the heat-resistant nickel alloy ZhS6K-VI with selective laser melting] // Tsvetnyye metally. 2016. №3 (879). S. 57–62.
  42. Prager S.M., Solodova T.V., Tatarenko O.Yu. Issledovaniye mekhanicheskikh svoystv i struktury obraztsov, poluchennykh metodom selektivnogo lazernogo splavleniya (SLS) iz splava VZH159 [Research of mechanical properties and microstructure of samples obtained by SLS from metal powder composition of VZh159 alloy] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №11 (59). St. 01. Available at: http://www.viam-works.ru (accessed: November 10, 2018). DOI: 10.18577/2307-6046-2017-0-11-1-1.