Definition of quantitative factors, significantly influencing on technological characteristics of model compositions

Aslanyan I.R., Rassokhina L.I., Ospennikova O.G.
Aslanyan I.R., Rassokhina L.I., Ospennikova O.G. Definition of quantitative factors, significantly influencing on technological characteristics of model compositions // Proceedings of VIAM. 2018. No. 12. DOI: 10.18577/2307-6046-2018-0-12-3-13. URL: https://www.viam-works.ru/en/journal/2018/12/1
Keywords
factorial experiment, planning matrix, regression equation, model compositions, dropping temperature, heat stability.
Abstract

The modern model compositions for investment casting represent the complex the mixes, possessing diverse properties that is caused by availability of the big numbers of initial components in their structure. In this regard identification of the general patterns of change of technical characteristics on model compositions in dependences on quantitative structure even basic components, and, therefore, and development of modern model compositions, the models of casting intended for manufacturing of responsible details, represents quite complex challenge quantitative and qualitative choice of initial components.

In this work this task decided by means of mathematical methods of planning of experiment that has allowed to establish the influence of basic components (mutual solvent, the polymer, strengthening component and filler) on some technological properties of model compositions.

Use of the full factor experiment when developing model compositions with the set technological by properties has allowed to determine the extent of influence of quantitative factors (the main components which are a part of model compositions) on dropping temperature and heat stability of model structures. As a result of the carried out experiments it is established that on dropping temperature the main influence renders strengthening component and polymer, and on heat stability temperature the main influence renders polymer and mutual solvent. With increase quantities of strengthening component and polymer in model compositions of its dropping temperature will decrease. Temperature of heat stability of the model compositions will decrease with increase in amount of polymer and mutual solvent in its structure. Thus maintenance of filler, as separate factor, does not make considerable impact on dropping temperature and heat stability of model compositions, but infl

Reference list
  1. Kablov E.N. Shestoy tekhnologicheskiy uklad [The sixth technological structure] // Nauka i zhizn. 2010. №4. S. 2–7.
  2. Perov N.S. Konstruirovanie polimernykh materialov na molekulyarnykh printsipakh. I. Sozdanie polimernykh materialov s dopolnitelnymi mekhanizmami dissipatsii mekhanicheskoy energii pri nizkikh temperaturakh [Design of polymer materials on the molecular principles. I. The development of polymer materials with additional mechanisms of dissipation of mechanical energy at low temperatures] // Aviacionnye materialy i tehnologii. 2017. №3 (48). S. 50–55. DOI: 10.18577/2071-9140-2017-0-3-50-55.
  3. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  4. Kondrashov S.V., Shashkeyev K.A., Popkov O.V. Sposob vychisleniya effektivnykh parametrov periodicheskoy sredy [A method for calculating effective electromagnetic parameters of a periodic medium] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №6 (54). St. 09. Available at: http://www.viam-works.ru (accessed: November 29, 2018). DOI: 10.18577/2307-6046-2017-0-6-9-9.
  5. Kablov E.N. Aviatsionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and prospects] // Vestnik Rossiyskoy akademii nauk. 2002. T. 72. №1. S. 3–12.
  6. Filin V.Yu., Artemev D.M., Ilin A.V., Larionov A.V. O problemakh perekhoda k kolichestvennym otsenkam energoyemkosti razrusheniya pri ispytaniyakh padayushchim gruzom obraztsov naturnoy tolshchiny [Difficulties of the transition to quantitative estimation of fracture energy intensity at drop-weight tear tests of specimens in full thickness] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 87–94. DOI: 10.18577/2071-9140-2017-0-4-87-94.
  7. Timoshkov P.N., Khrulkov A.V., Yazvenko L.N. Kompozitsionnye materialy v avtomobilnoy promyshlennosti (obzor) [Composite materials in automotive industry (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №6 (54). St. 07. Available at: http://www.viam-works.ru (accessed: November 29, 2018). DOI: 10.18577/2307-6046-2017-0-6-7-7.
  8. Lityye lopatki gazoturbinnykh dvigateley: splavy, tekhnologiya, pokrytiya / pod obshch. red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technology, coating / gen. ed. By E.N. Kablov]. 2-ye izd. M.: Nauka, 2006. 632 s.
  9. Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [Materials and technologies of VIAM for «Aviadvigatel»] // Permskiye aviatsionnyye dvigateli. 2014. №31. S. 43–47.
  10. Kablov E.N. Razrabotki VIAM dlya gazoturbinnykh dvigateley i ustanovok [Development of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
  11. Ospennikova O.G., Aslanyan I.R. Napravleniya razvitiya tekhnologii izgotovleniya modelnykh kompozitsiy dlya lopatok i drugikh detaley GTD [Directions of development of the technology of manufacturing model compositions for blades and other parts of the GTE] // Liteynoye proizvodstvo. 2018. №3. S. 20–24.
  12. Aslanyan I.R., Ospennikova O.G. Sovremennyye tendentsii razvitiya tekhnologii izgotovleniya modelnykh kompozitsiy dlya litya zharoprochnykh splavov [Modern trends in the development of technology for manufacturing model compositions for casting high-temperature alloys] // Sb. dokl. Vseros. nauch.-tekhnich. konf. «Fundamentalnyye i prikladnyye issledovaniya v oblasti sozdaniya liteynykh zharoprochnykh nikelevykh i intermetallidnykh splavov i vysokoeffektivnykh tekhnologiy izgotovleniya detaley GTD». M.: VIAM, 2017. S. 49–58.
  13. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Slavutskiy L.A. Osnovy registratsii dannykh i planirovaniya eksperimenta: ucheb. posobiye [Basics of data recording and experiment planning: students guide]. Cheboksary: Izd-vo ChGU, 2006. 200 s.
  15. Aslanyan I.R., Shuster L.Sh., Semenov V.I. Opredeleniye faktorov, sushchestvenno vliyayushchikh na fretting-iznashivaniye elektroliticheskikh NiP pokrytiy [Identifying factors that significantly affect the fretting wear of electrolytic NiP coatings] // Vestnik UGATU. 2012. T. 16. №1 (46). S. 57–61.