Study of changes in the heat-resistant alloy coating structure after heat resistance tests
UDC
669.018.44
DOI
10.18577/2307-6046-2018-0-11-64-73
Article PDF (Russian)
(1001.06 KB)
How to cite
Movenko D.A., Medvedev P.N., Smirnov A.A. Study of changes in the heat-resistant alloy coating structure after heat resistance tests // Proceedings of VIAM. 2018. No. 11. DOI: 10.18577/2307-6046-2018-0-11-64-73. URL: https://www.viam-works.ru/en/journal/2018/11/8
Keywords
heat shield, rhenium-containing nickel alloy, diffusion interaction, isothermal heat resistance, ceramic coating layer, heat resistant coating layer
Abstract
The material of the heat-resistant alloy with a heat-resistant coating (Ni–Cr–Al–Ta–Re–Y–Hf)+(Al–Ni–Y)+(Zr–Gd–Y–O) was investigated. It is shown that as a result of vacuum annealing at 1050°C/3 h, interaction zones between components of the coating and the substrate alloy form in the structure of the material due to their mutual diffusion. After heat-resistant tests of 1200°C/100 h, the coating loses its layered structure, the morphology of the structural components changes, the composition of the main elements of the coating is aligned with its depth, which indicates the complete flow of diffusion processes.
Reference list
- Kablov E.N., Muboyadzhyan S.A. Teplozashchitnyye pokrytiya s keramicheskim sloyem ponizhennoy teploprovodnosti na osnove oksida tsirkoniya dlya lopatok turbiny vysokogo davleniya perspektivnykh GTD [Heat-protective coatings with a ceramic layer of low thermal conductivity based on zirconium oxide for blades of a high-pressure turbine of promising gas turbine engines] // Sb. dokl. konf. «Sovremennyye dostizheniya v oblasti sozdaniya perspektivnykh nemetallicheskikh kompozitsionnykh materialov i pokrytiy dlya aviatsionnoy i kosmicheskoy tekhniki». M.: VIAM, 2015. S. 3.
- Kablov E.N., Solntsev S.S., Rozenenkova V.A., Mironova N.A. Sovremennyye polifunktsionalnyye vysokotemperaturnyye pokrytiya dlya nikelevykh splavov, uplotnitelnykh metallicheskikh voloknistykh materialov i berilliyevykh splavov [Modern polyfunctional high-temperature coatings for nickel alloys, sealing metallic fiber materials and beryllium alloys] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2013. №1. St. 05. Available at: http://www. materialsnews.ru (accessed: October 29, 2018).
- Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Smirnov A.A. Poluchenie keramicheskih teplozashhitnyh pokrytij dlya rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Receiving ceramic heat-protective coatings for working blades of turbines of aviation GTD magnetronny method] // Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8.
- Chubarov D.A., Matveev P.V. Novye keramicheskie materialy dlya teplozashhitnyh pokrytij rabochih lopatok GTD [New ceramic materials for thermal barrier coating using in GTE turbine blades] // Aviacionnye materialy i tehnologii. 2013. №4. S. 43–46.
- Budinovskij S.A., Chubarov D.A., Matveev P.V. . Sovremennye sposoby naneseniya teplozashhitnyh pokrytij na lopatki gazoturbinnyh dvigatelej (obzor) [Modern methods for deposition of thermal barrier coatings on GTE turbine blades] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 38–44.
- Chubarov D.A., Budinovskij S.A. Vybor keramicheskogo materiala dlya teplozashhitnyh pokrytij lopatok aviacionnyh turbin na rabochie temperatury do 1400°C [Choosing ceramic materials for thermal barrier coating of GTE turbine blades on working temperatures up to 1400°С] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2015. №4. St. 07. Available at: http://viam-works.ru (accessed: September 15, 2018). DOI: 10.18577/2307-6046-2015-0-4-7-7.
- Chubarov D.A., Budinovskij S.A., Smirnov A.A. Magnetronnyj sposob naneseniya keramicheskih sloev teplozashhitnyh pokrytij [Magnetron sputtering method for applying ceramic layers for thermal barrier coatings] // Aviacionnye materialy i tehnologii. 2016. №4. S. 23–30. DOI: 10.18577/2107-9140-2016-0-4-23-30.
- Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
- Kablov E.N., Muboyadzhyan S.A. Erozionnostoykiye pokrytiya dlya lopatok kompressora gazoturbinnykh dvigateley [Erosion-resistant coatings for compressor blades for gas turbine engines] // Elektrometallurgiya. 2016. №10. S. 23–38.
- Matveev P.V., Budinovskij S.A., Chubarov D.A. Tehnologiya polucheniya ionno-plazmennyh zharostojkih podsloev s povyshennym soderzhaniem alyuminiya dlya perspektivnyh TZP [Technology for production of ion-plasma heat-resistant bonding sub-layers with increased aluminum content for advanced TBCs] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 56–60. DOI: 10.18577/2071-9140-2014-0-s5-56-60.
- Smirnov A.A., Budinovskij S.A., Matveev P.V., Chubarov D.A. Razrabotka teplozashhitnyh pokrytij dlya lopatok TVD iz nikelevyh monokristallicheskih splavov VZhM4, VZhM5U [The development of thermal barrier coatings for turbine blades of single-crystal nickel alloys VZHM4, VZHM5U] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1. St. 03. Available at: http://www.viam-works.ru (accessed: September 15, 2018). DOI: 10.18577/2307-6046-2016-0-1-17-24.
- Walston W.S., Schaefer J.C., Murphy W.H. A new type of microstructural instability in superalloys – SRZ // Superalloys. The Minerals, Metals & Materials Society, 1996. P. 9–18.
- Budinovskiy S.A., Muboyadzhyan S.A., Gayamov A.M., Kos'min A.A. Zharostoykiye ionno-plazmennyye pokrytiya dlya lopatok turbin iz nikelevykh splavov, legirovannykh reniyem [Heat-resistant ion-plasma coatings for turbine blades of nickel alloys alloyed with rheniu] // MiTOM. 2008. №6. C. 31–36.
- Gayamov A.M., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Vybor zharostojkogo pokrytija dlya zharoprochnogo nikelevogo renij-rutenijsoderzhashhego splava marki VZhM4 [Selection of heat-resistant coating with metalloceramic barrier layer for protection of Re-Ru nickel-based superalloy] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №1. St. 01. Available at: http://viam-works.ru (accessed: September 18, 2018).
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Cutler R.W. The 1200°C Isothermal Sections of the Ni–Al–Cr and the Ni–Al–Mo Ternary Phase Diagrams: thesis for the Master Science Degree in Graduate Program in Materials Science and Engineering. Ohio. 2011. 58 p.
- Grushko B., Kowalski W., Pavlyuchkov D. etc. A contribution to the Al–Ni–Cr phase diagram // Journal of Alloys and Compounds. 2008. №460. P. 299–304.