The use of the rheological tests in the development of polymeric materials for various purposes
UDC
678.8:620.1
DOI
10.18577/2307-6046-2018-0-11-35-44
Article PDF (Russian)
(677.92 KB)
How to cite
Guseva M.A. The use of the rheological tests in the development of polymeric materials for various purposes // Proceedings of VIAM. 2018. No. 11. DOI: 10.18577/2307-6046-2018-0-11-35-44. URL: https://www.viam-works.ru/en/journal/2018/11/5
Keywords
rheological tests, viscosity, thermomechanical curve, polymeric binding, model composition, development of polymer material.
Abstract
Rheological tests allow to determine the behavior of the material under the unfluence of external loads, to evaluate its technological and operational characteristics and parameters. Рresents examples of the application of the rheological method for predicting the behavior of various polymer systems at the initial stage of development. Reviewed the results of tests of samples of a film silicone binder, the initial components for the paint coating based on polytetrafluorethylene, as well as model composition for investment casting.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsional'noy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
- Zelenskiy E.S., Kuperman A.M., Gorbatkina Yu.A. i dr. Armirovannyye plastiki – sovremennyye konstruktsionnyye materialy [Reinforced plastics - modern construction materials] // Rossiyskiy khimicheskiy zhurnal. 2001. T. XLV. №2. S. 56–74.
- Mamunya Ye., Lurzhenko M. Advances in progressive thermoplastic polymers, perspectives and application // Technopress. 2012. 425 р.
- Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Issledovaniye epoksidno-polisul'fonovykh polimernykh sistem kak osnovy vysokoprochnykh kleyev aviatsionnogo naznacheniya [The study of epoxy-polysulfone polymer systems as the basis of high-strength adhesives for aviation purposes] // Klei. Germetiki. Tekhnologii. 2017. №3. S.7–12.
- Zarubina A.Yu., Kozhevnikov V.S., Trofimov A.N. i dr. Reologicheskiye svoystva teplostoykikh svyazuyushchikh na osnove polifunktsionalnogo epoksidnogo oligomera [Rheological properties of heat-resistant binders based on polyfunctional epoxy oligomer] // Vestnik MITKHT. 2013. T. 8. №3. S. 63–66.
- Muranov A.N., Malysheva G.V., Nelyub V.A. i dr. Issledovaniye svoystv polimernykh kompozitsionnykh materialov na osnove geterogennoy matritsy [Investigation of the Properties of Polymer Composite Materials Based on a Heterogeneous Matrix] // Vse materialy. Entsiklopedicheskiy spravochnik. 2012. №4. S. 2–6.
- Volkov A.S., Kryuchkov I.A., Kerber M.L. i dr. Reokineticheskiye svoystva svyazuyushchego na osnove bifunktsionalnogo epoksidnogo oligomera v smesi s tetra- i poliglitsidilovymi modifikatorami [Reokinetic properties of a binder based on a bifunctional epoxy oligomer mixed with tetra- and polyglycidyl modifiers] // Uspekhi v khimii i khimicheskoy tekhnologii. 2007. T. XXI. №5 (73). S. 51–55.
- Guseva M.A. Cianovye efiry – perspektivnye termoreaktivnye svyazujushhie (obzor) [Cyanic esters are prospective thermosetting binders (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 45–50.
- Merkulova Yu.I., Muhametov R.R., Dolgova E.V., Ahmadieva K.R. Policianuratnoe svyazuyushhee dlya polucheniya kompozitov propitkoj pod davleniem [Polycyanurates binding for composites production by impregnation under pressure] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №11 (47). St. 05. Available at: http://www.viam-works.ru (accessed: November 5, 2018). DOI: 10.18577/2307-6046-2016-0-11-5-5.
- Kopitsyna M.N., Bessonov I.V., Kotomin S.V. Treshchinostoykost epoksidnykh svyazuyushchikh, modifitsirovannykh termoplastichnym polisulfonom i furfurolatsetonovoy smoloy [Crack resistance of epoxy binders modified with thermoplastic polysulfone and furfurol-acetone resin] // Inzhenernyy zhurnal: nauka i innovatsii. 2016. №12. S. 1–9.
- Guseva M.A. Besednov K.L., Khaskov M.A., Tkachuk A.I. Issledovaniye vliyaniya prirody epoksidnykh oligomerov na protsess sovmeshcheniya s termoplastichnymi modifikatorami [Study of the effect of the nature of epoxy oligomers on the process of combining with thermoplastic modifiers] // Mekhanika kompozitsionnykh materialov i konstruktsiy. 2017. T. 23. №4. S. 567–578.
- Surikov P.V., Trofimov A.N., Kokhan E.I. i dr. Vliyaniye molekulyarnykh kharakteristik epoksidnykh oligomerov i ikh smesey na reologicheskiye svoystva [The influence of the molecular characteristics of epoxy oligomers and their mixtures on the rheological properties] // Plasticheskiye massy. 2009. №9. S. 3–7.
- Babin A.N., Guseva M.A., Grebeneva T.A., Tkachuk A.I. Issledovanie reologicheskikh i strukturnykh kharakteristik epoksidnykh sviazuiushchikh, modifitsirovannykh poliizotsianatom [Study of the rheological and structural characteristics of the epoxy resins, modified by polyisocyanate] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №1. St. 11. Available at: http://www.viam-works.ru (accessed: November 5, 2018). DOI: 10.18577/2307-6046-2016-0-1-90-98.
- Melnikov D.A., Khaskov M.A., Guseva M.A., Antyufeeva N.V. K voprosu o razrabotke rezhimov pressovaniya sloistykh PKM na osnove prepregov [To the question of the development of pressing mode for laminated PCMs based on prepregs] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №2. St. 09. URL: http://www.viam-works.ru (data obrashcheniya: 05.11.2018). DOI: 10.18577/2307-6046-2018-0-2-9-9.
- Babin A.N., Guseva M.A. Reologicheskiy metod issledovaniya rastvorimosti komponentov v polimernykh kompozitsiyakh [Rheological method for studying the solubility of components in polymer compositions] // Vse materialy. Kommentarii k standartam, TU, sertifikatam. 2016. №4. S. 17–20.
- Alentyev A.Yu., Yablokova M.Yu. Svyazuyushchiye dlya polimernykh kompozitsionnykh materialov: ucheb. posobiye [Binders for polymer composite materials: students guide]. M.: Izd-vo MGU, 2010. 69 s.
- Mikhaylin A.Yu. Teplo-, termo- i ognestoykost' polimernykh materialov [Heat, heat and fire resistance of polymeric materials]. SPb.: Nauchnyye osnovy i tekhnologii, 2011. 416 s.
- Kraev I.D., Popkov O.V., Shuldeshov E.M. i dr. Perspektivy ispolzovaniya kremniyorganicheskikh polimerov pri sozdanii sovremennykh materialov i pokrytiy razlichnykh naznacheniy [Prospects for the use of organosilicon elastomers in the development of modern polymer materials and coatings for various purposes] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №12. St. 05. Available at: http://www.viam-works.ru (accessed: November 07, 2018). DOI: 10.18577/2307-6046-2017-0-12-5-5.
- Davydova I.F., Kavun N.S. Plenochnye kremnijorganicheskie svyazuyushhie dlya stekloplastikov [Film silicon organosilicon resins for glassfibers] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 15–18. DOI: 10.18577/2071-9140-2014-0-s2-15-18.
- Severs E.T. Reologiya polimerov [Polymer rheology]. M.: Khimiya, 1966. 198 c.
- Tager A.A. Fiziko-khimiya polimerov [Physical chemistry of polymers]. M.: Khimiya, 1968. 545 c.
- Kiryukhin D.P., Kichigina G.A., Buznik V.M. Telomery tetraftoretilena: radiatsionno-khimicheskiy sintez, svoystva i perspektiva ispolzovaniya [Telomeres of tetrafluoroethylene: radiation-chemical synthesis, properties and prospects of use] // Vysokomolekulyarnyye soyedineniya. Ser.: A. 2013. T. 55. №11. C. 1321–1332.
- Ospennikova O.G. Issledovanie i razrabotka parametrov tehnologicheskogo processa izgotovleniya modelej iz modelnyh kompozicij na osnove sinteticheskih voskov [Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes] // Aviacionnye materialy i tehnologii. 2014. №3. S. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.
- Ospennikova O.G. Issledovanie vliyaniya napolnitelej na svojstva i stabilnost modelnyh kompozicij, vybor optimalnyh sostavov [Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures] // Aviacionnye materialy i tehnologii. 2014. №3. S. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.