Features of influence of atmospheric factors on aviation organic glass

Mekalina I.V., Aizatulina M.K., Sentiourin E.G., Popov A.A.
Mekalina I.V., Aizatulina M.K., Sentiourin E.G., Popov A.A. Features of influence of atmospheric factors on aviation organic glass // Proceedings of VIAM. 2018. No. 11. DOI: 10.18577/2307-6046-2018-0-11-28-34. URL: https://www.viam-works.ru/en/journal/2018/11/4
Keywords
organic glass, polymethylmethacrylate, copolymer, climatic aging, weather resistance, mechanical characteristics, transmittance, operation, glazing.
Abstract

The paper studies the influence of atmospheric factors on the properties of polymethylmethacrylate and copolymer organic glasses after aging in different climatic zones. The assessment of physical and mechanical, optical characteristics, «silver resistance», softening temperature of organic glasses after aging in the conditions of FCC, Arizona (USA), Florida (USA). The basic features of the climatic ageing of organic glasses of the partially cross-linked structure: polimetilmetakrilata SO-120S and copolymer VOS-1 and VOS-2 – in the oriented and unoriented states. A comparative analysis of the data obtained with commercially used рlexiglas SO-120A, AO-120 and E-2.

Reference list
  1. Sentyurin E.G., Kuklina L.S., Trigub T.S., Pashkova T.V. Vliyaniye atmosferostoykosti na ekspluatatsionnuyu nadezhnost orgstekol [Influence of weather resistance on the operational reliability of plexiglass] // Aviatsionnaya promyshlennost. 1984. №5. S. 56–58.
  2. Gudimov M.M., Sentyurin Ye.G., Trigub T.S. Serebrostoykost ostekleniya samoletov iz organicheskogo stekla v protsesse yego proizvodstva i ekspluatatsii [Silver resistance of glazing of airplanes made of organic glass in the process of its production and operation] // Aviatsionnaya promyshlennost. 1995. №9–10. S. 55–60.
  3. Gudimov M.M. Treshchiny serebra na organicheskom stekle [Cracks of silver on organic glass]. M.: TSIPKK AP, 1997. 260 s.
  4. Gudimov M.M., Perov B.V. Organicheskoye steklo [Organic glass]. M.: Khimiya, 1981. 215 s.
  5. Sentyurin E.G., Mekalina I.V., Ajzatulina M.K., Isaenkova Yu.A. Istoriya sozdaniya materialov samoletnogo ostekleniya i polimernyh materialov so spetsialnymi svojstvami (k 75-letiyu laboratorii polimernyh materialov so spetsial'nymi svojstvami) [The history of aircraft materials of glass and polymer materials with special properties (To the 75th anniversary Laboratory of polymer materials with special properties)] // Aviatsionnye materialy i tekhnologii. 2017. №3 (48). S. 81–86. DOI: 10.18577/2071-9140-2017-0-3-81-86.
  6. Pavlyuk B.F. Osnovnye napravleniya v oblasti razrabotki polimernyh funktsionalnyh materialov [The main directions in the field of development of polymeric functional materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  7. Sentyurin E.G., Mekalina I.V., Ayzatulina M.K., Bogatov V.A. Akrilatnyye vysokotemperaturnyye organicheskiye stekla. Opyt primeneniya. Perspektivy [Acrylate high-temperature organic glass. Experience of application. Perspectives] // Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Khimiya i khimicheskaya tekhnologiya. 2015. T. 58. №8. S. 22–24.
  8. Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  9. Lutsenko A.N., Odintsev I.N., Grinevich A.V. i dr. Issledovanie protsessa deformatsii materiala optiko-korrelyatsionnymi metodami [Study of material deformation by optical-correlation methods] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 70–86. DOI: 10.18577/2071-9140-2014-0-s4-70-86.
  10. Yakovlev N.O. Issledovanie i opisanie relaksacionnogo povedeniya polimernyh materialov (obzor) [Study and description of relaxation behavior of polymers (review)] //Aviacionnye materialy i tehnologii. 2014. №S4. S. 50–54. DOI: 10.18577/2071-9140-2014-0-s4-50-54.
  11. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  12. Kablov E.N. Materialy i khimicheskiye tekhnologii dlya aviatsionnoy tekhniki [Materials and chemical technologies for aviation technology] // Vestnik Rossiyskoy akademii nauk. 2012. T. 82. №6. S. 520–530.
  13. Kablov E.N. Rol khimii v sozdanii materialov novogo pokoleniya dlya slozhnykh tekhnicheskikh sistem [The role of chemistry in the creation of a new generation of materials for complex technical systems] // Tez. dokl. KHKH Mendeleyevskogo s"yezda po obshchey i prikladnoy khimii. Yekaterinburg: UrO RAN, 2016. S. 25–26.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Akolzin S.V., Frolkov A.I. Vosstanovleniye rabotosposobnosti teplostoykogo aviatsionnogo ostekleniya pri remonte i v ekspluatatsii [Restoration of heat-resistant aviation glazing during repair and operation] // Aviatsionnaya promyshlennost. 2014. №1. S. 41–44.