Research on the creation of a new high-temperature heat-resistant matrix based on intermetallic compounds NiAl–Ni3Al

Bondarenko Yu.A., Bazyleva O.A., Raevskih A.N., Narskiy A.R.
Bondarenko Yu.A., Bazyleva O.A., Raevskih A.N., Narskiy A.R. Research on the creation of a new high-temperature heat-resistant matrix based on intermetallic compounds NiAl–Ni3Al // Proceedings of VIAM. 2018. No. 11. DOI: 10.18577/2307-6046-2018-0-11-3-11. URL: https://www.viam-works.ru/en/journal/2018/11/1
Keywords
high-gradient directional crystallization, intermetallic heat-resistant alloy, structure, phase composition, short-term strength, plasticity, heat resistance.
Abstract

In this work the possibility of creating a new high-temperature heat-resistant matrix based on intermetallic compounds NiAl and Ni3Al. It is found that the alloys based on the new matrix have good heat resistance and low density. Under the conditions of high-gradient directional crystallization in the samples it was possible to form a directed dendritic structure, oriented along the axis of the samples, consisting of intermetallic NiAl and Ni3Al. In assessing the strength of them managed to get a fairly high strength and ductility.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Lityye lopatki gazoturbinnykh dvigateley: splavy, tekhnologii, pokrytiya / pod obshch. red. E.N. Kablov. 2-ye izd. [Cast blades of gas turbine engines: alloys, technologies, coatings / gen. ed. E.N. Kablov. 2nd ed.]. M.: Nauka, 2006. 632 s.
  3. Kablov E.N. Bez novykh materialov – net budushchego [Without new materials - there is no future] // Metallurg. 2013. №12. S. 4–8.
  4. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Liteynyye zharoprochnyye nikelevyye splavy dlya perspektivnykh aviatsionnykh GTD [Casting heat-resistant nickel alloys for promising aircraft GTE] // Tekhnologiya legkikh splavov. 2007. №2. S. 6–16.
  5. Kablov E.N., Ospennikova O.G., Petrushin N.V. Novyj monokristallicheskij intermetallidnyj (na osnove γʹ-fazy) zharoprochnyj splav dlya lopatok GTD [New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 34–40. DOI: 10.18577/2071-9140-2015-0-1-34-40.
  6. Ospennikova O.G. Tendencii sozdaniya zharoprochnyh nikelevyh splavov nizkoj plotnosti s polikristallicheskoj i monokristallicheskoj strukturoj (obzor) [Tendencies of development of heat-resistant nickel alloys of low density with polycrystalline and single-crystal structures (review)] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 3–19. DOI: 10.18577/2071-9140-2016-0-1-3-19.
  7. Walston S., Cetel A., MacKay R. et. al. Dreshfield R. Joint development of a fourth generation single crystal superalloys // Superalloys-2004. Minerals, Metals & Materials Society, 2004. P. 15–24.
  8. Koizumi Y., Kobayashi T., Yokokawa T. et al. Development of next-generation Ni-base single crystal superalloys // Superalloys-2004. Minerals, Metals & Materials Society, 2004. P. 35–43.
  9. Kablov E.N., Ospennikova O.G., Svetlov I.L. Vysokoeffektivnoe ohlazhdenie lopatok goryachego trakta GTD [Highly efficient cooling of GTE hot section blades] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  10. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] // Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  11. Kablov E.N., Buntushkin V.A., Bazyleva O.A. Malolegirovannyye legkiye zharoprochnyye liteynyye splavy na osnove intermetallida Ni3Al [Low-alloy lightweight heat-resistant casting alloys based on Ni3Al intermetallic compound] // Metally. RAN. 1999. №1. S. 56–65.
  12. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Tendencii razvitiya intermetallidnyh splavov na osnove nikelya [Development trends of nickel-based intermetallic alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  13. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Monokristallicheskie zharoprochnye nikelevye splavy dlya turbinnyh lopatok perspektivnyh GTD [Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  14. Hubert-Protopopescu M., Hubert H. Aluminium-cobalt-nickel // Ternary alloys: a comprehensive compendium of evaluated constitutional data and phase diagrams. Weinheim – N.Y.: VCH Cop., 1991. P. 234–244.
  15. Kornilov I.I. Fiziko-khimicheskiye osnovy zharoprochnosti splavov [Physical and chemical bases of heat resistance of alloys]. M.: Izd-vo AN SSSR, 1961. 516 s.
  16. Kornilov I.I., Mints R.S. Issledovaniye sistemy Ni–Cr–NiAl [Investigation of the Ni–Cr–NiAl System] // Neorganicheskaya khimiya 1958. T. III. Vyp. 5. S. 699–707.
  17. Bondarenko Yu.A., Kablov E.N. Napravlennaya kristallizatsiya zharoprochnykh splavov s povyshennym temperaturnym gradiyentom [Directional crystallization of superalloys with a high temperature gradient] // MiTOM. 2002. №7. S. 20–23.