Analysis of the data of full-scale climatic tests combined with the application of operational factors of nonmetallic materials (review)

Gladkikh A.V., Kurs I.S., Kurs M.G.
Gladkikh A.V., Kurs I.S., Kurs M.G. Analysis of the data of full-scale climatic tests combined with the application of operational factors of nonmetallic materials (review) // Proceedings of VIAM. 2018. No. 10. DOI: 10.18577/2307-6046-2018-0-10-74-82. URL: https://www.viam-works.ru/en/journal/2018/10/9
Keywords
polymer composite materials, operational factors, natural climatic influence, laboratory tests, loads.
Abstract

Aging of polymer composite materials is a multifactorial process, therefore it is necessary to study not only the influence of individual aggressive factors, but also to take into account their synergistic effect on changes in the performance characteristics of the material. The most important impact factors include: moisture saturation, elevated temperatures, thermal cycling, and mechanical loads. The paper discusses the combined effect of mechanical loads and clima-tic factors on changes in the properties of polymer composite materials for aviation purposes.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoye stareniye kompozitsionnykh materialov aviatsionnogo naznacheniya. I. Mekhanizmy stareniya [Climatic aging of composite materials for aviation purposes. I. Mechanisms of aging] // Deformatsiya i razrusheniye materialov. 2010. №11. S. 19–27.
  3. Kablov E.N. Vserossiyskomu institutu aviatsionnykh materialov – 80 let [All-Russian Institute of Aviation Materials – 80 years] // Deformatsiya i razrusheniye materialov. 2012. №6. S. 17–19.
  4. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoye stareniye kompozitsionnykh materialov aviatsionnogo naznacheniya. III. Znachimyye faktory stareniya // Deformatsiya i razrusheniye materialov. 2011. №1. S. 34–40.
  5. Startsev O.V., Vapirov Yu.M., Deyev I.S. i dr. Vliyaniye dlitelnogo atmosfernogo stareniya na svoystva i strukturu ugleplastika // Mekhanika kompozitnykh materialov. 1986. №4. S. 637–642.
  6. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  7. Vapirov Yu.M., Krivonos V.V., Startsev O.V. Interpretatsiya anomalnogo izmeneniya svoystv ugleplastika KMU-1y pri starenii v raznykh klimaticheskikh zonakh [Interpretation of the anomalous change in the properties of CFRP CMU-1y during aging in different climatic zones] // Mekhanika kompozitnykh materialov. 1994. №2. S. 266–273.
  8. Startsev O.V., Krotov A.S., Golub P.D. Effect of Climatic and Radiation Ageing on Properties of Glass Fibre Reinforced Epoxy Laminates // Polymers and Polymer Composites. 1998. Vol. 6. No. 7. P. 481–488.
  9. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoye stareniye kompozitsionnykh materialov aviatsionnogo naznacheniya. II. Relaksatsiya iskhodnoy strukturnoy neravnovesnosti i gradiyent svoystv po tolshchine [Climatic aging of composite materials for aviation purposes. Ii. Relaxation of the initial structural nonequilibrium and gradient of thickness properties] // Deformatsiya i razrusheniye materialov. 2010. №12. S. 40–46.
  10. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  11. Morskaya korroziya: spravochnoye izdaniye. Per. s angl. / pod red. A.I. Stepanova [Marine corrosion: reference book. Trans. from Engl. / ed. By A.I. Stepanov]. M.: Metallurgiya, 1983. 512 s.
  12. Aviatsionnyye materialy: spravochnik v 13 t. 7-ye izd., pererab. i dop. / pod obshch. red. E.N. Kablova [Aviation materials: a reference book in 13 t. 7th ed., rev. and add. / gen. ed. by E.N. Kablov]. T. 13: Klimaticheskaya i mikrobiologicheskaya stoykost nemetallicheskikh materialov. M.: VIAM, 2015. 270 s.
  13. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://viam-works.ru (accessed: June 18, 2018).
  14. Kuleznev V.N., Ushakova O.B. Struktura i mekhanicheskiye svoystva polimerov: konspekt kursa lektsiy [Structure and mechanical properties of polymers: lecture course outline]. M.: MITKhT, 2006. Ch. 3. C. 28–31.
  15. Stepanov R.D., Shlenskiy O.F. Raschet na prochnost konstruktsiy iz plastmass, rabotayushchikh v zhidkikh sredakh [Calculation of the strength of structures made of plastic, working in liquid media]. M.: Mashinostroyeniye, 1981. 270 s.
  16. Ivanova I.V., Semenycheva I.V., Startsev O.V. i dr. Klimaticheskiye ispytaniya tormoznykh shchitkov izdeliya An-72 [Climatic Testing of An-72 Brake Shields] // Voprosy aviatsionnoy nauki i tekhniki // Klimaticheskoye stareniye polimernykh kompozitsionnykh materialov. M.: VIAM, 1990. S. 6–13.
  17. Kirillov V.N., Yefimov V.A., Matveyenkova T.E., Korenkova T.G. Vliyaniye posledovatelnogo vozdeystviya klimaticheskikh i ekspluatatsionnykh faktorov na svoystva stekloplastikov [The influence of the successive effects of climatic and operational factors on the properties of fiberglass] // Aviatsionnaya promyshlennost. 2004. №1. S. 45–48.
  18. Tkachenko V.N., Gunyaev G.M. Klimaticheskaya stoykost ugleplastikov pod nagruzkoy [Climatic resistance of carbon fiber plastic under load] // Aviacionnyye materialy. Korroziya i stareniye materialov v morskikh subtropikakh / pod red. B.V. Perova, V.A. Zasypkina. M.: VIAM, 1983. S. 18–31.
  19. Panferov K.V., Romanenkov I.G., Abashidze G.S. i dr. Atmosferostoykost stekloplastikov, nakhodyashchikhsya pod nagruzkoy [Atmosphere-resistance of glass plastics under load] // Plasticheskiye massy. 1968. №6. S. 32–33.
  20. Bulmanis V.N., Yartsev V.A, Krivonos V.V. Rabotosposobnost konstruktsiy iz polimernykh kompozitov pri vozdeystvii staticheskikh nagruzok i klimaticheskikh faktorov [Efficiency of structures made of polymer composites under the influence of static loads and climatic factors] // Mekhanika kompozitsionnykh materialov. 1987. №5. S. 915–920.
  21. Voprosy aviatsionnoy nauki i tekhniki. Ser.: Aviacionnyye materialy. Vyp.: Klimaticheskoye stareniye PKM / pod red. B.V. Perova, O.V. Startseva [Questions of aviation science and technology. Ser.: Aviation materials. Issue: Climatic aging of the RMB / ed. by B.V. Perov, O.V. Startsev]. M.: ONTI VIAM, 1990. 100 s.
  22. Ispytaniya uprugikh sterzhney metodom prodolnogo izgiba / pod red. V.F. Savina, A.N. Blaznova [Tests of elastic rods by the method of buckling / ed. by V.F. Savin, A.N. Blaznov.]. Barnaul: Izd-vo Alt. gos. un-ta, 2009. 221 s.
  23. Rudolf A.Ya., Savin V.F., Startsev O.V. i dr. Prodolnyy izgib dlya opredeleniya prochnosti plit aviatsionnykh ugleplastikov [Longitudinal bend for determining the strength of aircraft carbon fiber plates] // Tekhnika i tekhnologiya proizvodstva teploizolyatsionnykh materialov iz mineralnogo syrya: doklady IX Vseros. nauch.-praktich. konf. 17–19 iyunya 2009 g. Biysk: Izd-vo BTI AltGTU, 2009. S. 148–153.
  24. Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Tsentry dlya klimaticheskikh ispytaniy aviatsionnykh PKM [Climate Test Centers for Aviation PCM] // Aviatsionnaya promyshlennost. 2009. №4. S. 36–46.