Calculation of tension in a layered material

Oreshko E.I., Erasov V.S., Lashov O.A., Podzhivotov N.Y., Kachan D.V.
Oreshko E.I., Erasov V.S., Lashov O.A., Podzhivotov N.Y., Kachan D.V. Calculation of tension in a layered material // Proceedings of VIAM. 2018. No. 10. DOI: 10.18577/2307-6046-2018-0-10-93-106. URL: https://www.viam-works.ru/en/journal/2018/10/11
Keywords
stability analysis, layered material, finite elements method, tension, critical strength of buckling.
Abstract

Calculations in the final element program ANSYS complex showed that tension which arise in layered samples at loading do not depend on quantity of layers if the total thickness of materials with different values of the module of elasticity does not change. The model is developed for calculation of tension in each layer of a layered plate. The schedule of dependence of settlement factor for calculation of tension in a layered sample from the relation of modules of elasticity of its materials in case of equal thickness of layers with different values of the module of elasticity is constructed. The system of the equations, allowing to define tension in plate layers with different values of the module of elasticity is offered.

Reference list
  1. Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyy klass sloistykh alyumostekloplastikov na osnove alyuminiy-litiyevogo splava 1441 s ponizhennoy plotnostyu [A new class of layered aluminum-glass plastics based on an aluminum-lithium alloy 1441 with a lower density] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2011. №SP2. S. 174–183.
  2. Buznik V.M., Kablov E.N., Koshurina A.A. Materialy dlya slozhnykh tekhnicheskikh ustroystv arkticheskogo primeneniya [Materials for complex technical devices of arctic use] // Nauchno-tekhnicheskiye problemy osvoyeniya Arktiki. M.: Nauka, 2015. S. 275–285.
  3. Bokhoyeva L.A. Osobennosti rascheta na prochnost elementov konstruktsiy iz izotropnykh i kompozitsionnykh materialov s dopustimymi defektami [Features of strength analysis of structural elements of isotropic and composite materials with permissible defects]. Ulan-Ude: Izd-vo VSGTU, 2007. S. 5–6.
  4. Bert Ch.U., Martindeyl D.L. Tochnyy uproshchennyy metod issledovaniya povedeniya tonkikh plastin pri bol'shikh progibakh [The exact simplified method for studying the behavior of thin plates at large deflections] // Aerokosmicheskaya tekhnika. 1988. №11. S. 131–138.
  5. Bokhoyeva L.A. Ustoychivost i rost kruglykh rassloyeniy v sloistykh elementakh konstruktsiy [Stability and growth of round bundles in layered structural elements] // Izvestiya vuzov. Mashinostroyeniye. 1989. №8. S. 12–15.
  6. Bokhoyeva L.A. Vliyaniye defektov tipa otsloyeniy v sloistykh plastinakh na velichinu kriticheskoy nagruzki [The effect of flaws of the type of delaminations in layered plates on the critical load] // Vestnik BGU. 2005. Vyp. 5. S. 243–264.
  7. Damdinov T.A., Aseyev A.V., Belyakov A.V., Bokhoyeva L.A. Opredeleniye kriticheskikh nagruzok s pomoshchyu energeticheskogo kriteriya ustoychivosti [Definition of critical loads with the help of the energy stability criterion] // XII Tupolevskiye chteniya: mezhdunar. molodezh. nauch. konf.: materialy konf. Kazan: Izd-vo Kazan. gos. tekhn. un-ta, 2004. S. 53.
  8. Sborovskiy A.K., Savelyev N.F. Mekhanizmy razrusheniya oriyentirovannykh stekloplastikov pri szhatii [Mechanisms of destruction of oriented glass plastics under compression] // Voprosy sudostroyeniya. Tekhnologiya sudostroyeniya. 1976. Vyp. 12. S. 12–18.
  9. Serensen S.V., Zaytsev G.P. Nesushchaya sposobnost tonkostennykh konstruktsiy iz armirovannykh plastikov s defektami [Bearing capacity of thin-walled structures made of reinforced plastics with defects]. Kiev: Naukova dumka, 1982. 295 s.
  10. Siratori M., Miyesi T., Matsusita Kh. Vychislitelnaya mekhanika razrusheniya [Computational Fracture Mechanics]. M.: Mir, 1986. 336 s.
  11. Chen H.P., Doong J.L. Postbuckling Behavior of a Thick Plate // AIAA Journal. 1983. Vol. 21. No. 8. P. 1157–1161.
  12. Evams A.G., Hutchinson J.W. On the mechanics of delamination and spelling on compressed felms // International Journal of Lolids and structures. 1984. Vol. 20. No. 5. P. 455–466.
  13. Fei Z., Yin W.L. Post Buckling growth of a circular delamination in a laminate under compression and bending // Proceedings of the Twelfth South-eastern Conference on Theoretical and Applied Mechanics. Georgia Institute of Technology (May 10–11, 1984). Auburn. 1984. Vol. 2. P. 130–134.
  14. Grishchenko S.V. Raschet i proyektirovaniye izdeliy konstruktsiy samoleta iz sloistykh kompozitov s uchetom mezhsloyevykh effektov [Calculation and design of products of aircraft structures made of laminated composites, taking into account interlayer effects] // Trudy MAI. 2015. №84. S. 1–19.
  15. Huang H., Kardomateas G. Buckling and initial postbuckling behavior of sandwich beams including transverse shear // AIAA Journal. 2002. Vol. 40. No. 11. P. 2331–2335.
  16. Kim H.J. Postbuckling analysis of composite laminates // Computers and Structures. 1997. Vol. 62. No. 6. P. 975–983.
  17. Grigolyuk E.I., Kogan E.A., Mamay V.I. Problemy deformirovaniya tonkostennykh sloistykh konstruktsiy s rassloyeniyami [Problems of deformation of thin-walled laminated structures with bundles] // Izvestiya Rossiyskoy akademii nauk. Mekhanika tverdogo tela. 1994. №2. S. 6–32.
  18. Ihibaoko J. On the buckling of an Eliptic plate with Champed Edge // Journal of the Physical Society of Japan. 1957. Vol. 12. No. 5. P. 529–532.
  19. Williams J.G. On the calculation of energy release rates for cracked laminates // International Journal of Fracture. 1988. Vol. 36. P. 101–119.
  20. Storakers B., Andersson B. Nonlinear plate theory applied to delamination in composites // Journal of Mechanics and Physics solids. 1988. Vol. 36. No. 6. P. 689–718.
  21. Well N.A. Large Deflections of Elliptical Plates // Journal of applied Mechanics. 1956. Vol. 23. No. 1. P. 21–26.
  22. Kiseleva R.Z., Gureyeva N.A., Kiselev A.P. Raschet mnogosloynoy obolochki s ispolzovaniyem obemnogo konechnogo elementa [Calculation of a multilayer shell using a bulk finite element] Izvestiya VolgGTU. 2010. №4. S. 125–128.
  23. Yin W.-L., Fei Z. Delamination buckling and growth in a champed circular plate // AIAA Journal. 1988. Vol. 26. No. 4. P. 438–445.
  24. Yin W.-L., Wang J.T.S. The Energy-Release Rate in the Growth of a One-Dimensional Delamination // Journal of applied Mechanics. 1984. Vol. 51. P. 939–941.
  25. Sendetski D. Mekhanika kompozitsionnykh materialov [Mechanics of composite materials]. M.: Mir, 1978. T. 2. 564 s.
  26. Bottega W.J. Peeling of a cylindrical layer // International Journal of Fracture. 1988. Vol. 38. No. 1. P. 3–14.
  27. Buchanan G.R., Hung Y.K., Chin H.J. Nonlinear analysis for a champed bar // Transactions of the American society of Mechanical Engineers. 1969. Vol. 36. No. 2. P. 355–357.
  28. Chai H., Babcock C.D. Two-dimensional modeling of Compressive Failure in Delaminated laminates // Journal of Composite materials. 1985. Vol. 19. No. 1. P. 67–91.
  29. Chan W.S., Wang A.S.D. A study on the effects of the 900 ply on matrix cracks in composite laminates // AIAA/ASME/ASCE/AHC structures, structural: Dynamics and Materials Conference 27: Collection of Technical Papers. 1986. Vol. 1. P. 689–694.
  30. Shivacumar K.N., Whitcomb J.D. Buckling of Sublaminate in a Quasi-Isotropic Composite Laminate // Journal of Composite materials. 1985. Vol. 19. No. 1. P. 2–18.
  31. Dimitriyenko Yu.I., Gubareva E.A., Kolzhanova D.Yu. Modelirovaniye sloistykh kompozitov s konechnymi deformatsiyami metodom asimptoticheskoy gomogenizatsii [Simulation of layered composites with finite deformations by the method of asymptotic homogenization] // Inzhenernyy zhurnal: nauka i innovatsii. Available at: http://engjournal.ru/catalog/msm/pmcm/1405.html (accessed: October 25, 2018).
  32. Alfutov N.A., Zinovyev P.A., Popov B.G. Raschet mnogosloynykh plastin i obolochek iz kompozitsionnykh materialov [Calculation of multilayer plates and shells of composite materials]. M.: Mashinostroyeniye, 1984. 263 s.
  33. Antokhonov V.B., Bokhoyeva L.A. Obrazovaniye tekhnologicheskikh napryazheniy v koroblenii v pressovannykh kompozitnykh plastinakh [Formation of technological stresses in warping in pressed composite plates] // Mezhvuzovskiy sbornik. Irkutsk, 2000. S. 56–60.
  34. Bolotin V.V. Defekty tipa rassloyeniy v konstruktsiyakh iz kompozitsionnykh materialov [Defects of the type of bundles in structures made of composite materials] // Mekhanika kompozitsionnykh materialov. 1984. №2. S. 239–256.
  35. Si D. Mekhanika razrusheniya kompozitnykh materialov [Mechanics of destruction of composite material] // Mekhanika kompozitnykh materialov. 1979. №3. S. 434–446.
  36. Timoshenko S.P., Voykovskiy-Kriger S. Plastinki i obolochki [Sheets and shells]. M.: Fizmatgiz, 1963. 635 s.
  37. Troshin V.P. Vliyaniye prodolnogo rassloyeniya v sloistoy tsilindricheskoy obolochke na velichinu kriticheskogo vneshnego davleniya [The effect of longitudinal delamination in a layered cylindrical shell on the critical external pressure] // Mekhanika kompozitnykh materialov. 1982. №5. C. 838–842.
  38. Feodosyev V.I. Izbrannyye zadachi i voprosy po soprotivleniyu materialov [Selected problems and questions on the resistance of materials]. M.: Nauka, 1973. 399 s.
  39. Fudzii T., Dzako M. Mekhanika razrusheniya kompozitsionnykh materialov [Mechanics of Fracture of Composite Materials]. M.: Mir, 1982. 232 s.
  40. Khellan K. Vvedeniye v mekhaniku razrusheniya [Introduction to Fracture Mechanics]. M.: Mir, 1988. 364 s.
  41. Tsigler G. Osnovy teorii ustoychivosti konstruktsii [Basics of the theory of stability of a structure]. M.: Mir, 1971. 192 s.
  42. Bolotin V.V., Zebelyan Z.Kh., Kurzin L.A. Ustoychivost szhatykh elementov s defektami tipa rassloyeniy [Stability of compressed elements with defects such as delaminations] // Problemy prochnosti. 1980. №7. S. 3–8.
  43. Cherepanov G.P. Mekhanika razrusheniya kompozitsionnykh materialov [Fracture mechanics of composite materials]. M.: Nauka, 1983. 264 s.
  44. Cherepanov G.P. Mekhanika razrusheniya mnogosloynykh obolochek. Teoriya treshchin rasslaivaniya [Mechanics of destruction of multilayer shells. Theory of delamination cracks] // Prikladnaya matematika i mekhanika. 1983. T. 47. Vyp. 5. S. 832–845.
  45. Budiaushy B. Theory of buckling and post buckling of elastic structures // Advances in Applied Mechanics. 1974. Vol. 14. P. 1–65.
  46. Chen H.P., Doong J.L. Postbuckling Behavior of a Thick Plate // AIAA Journal. 1983. Vol. 21. No. 8. P. 1157–1161.
  47. Dharen C.K.H. Fracture mechanics of Composite materials // Journal of Materials and Technology. 1978. Vol. 100. No. 3. P. 233–247.
  48. Kulkarni S.V., Frederick D. Buckling of Partially Debonded Layered Cylingrical Shells // AJAA Report. 1973. No. 73. P. 9.
  49. Alfutov N.A. Osnovy rascheta na ustoychivost uprugikh system [Fundamentals of calculation on the stability of elastic systems]. M.: Mashinostroyeniye, 1991. 336 s.
  50. Antipov V.V., Oreshko E.I., Erasov V.S., Serebrennikova N.Y. Hybrid laminates for application in north conditions // Mechanics of Composite Materials. 2016. Vol. 52. Nо. 5. P. 973–990.
  51. Bokhoyeva L.A., Antokhonov V.B., Zangeyev B.I. Teoreticheskaya otsenka maksimalnykh razmerov bezopasnykh defektov tipa otsloyeniy [Theoretical estimation of the maximum sizes of safe defects such as delaminations] // Problemy mekhaniki sovremennykh mashin: materialy Mezhdunar. nauch. konf. Ulan-Ude, 2000. S. 14–15.
  52. Bokhoyeva L.A., Damdinov T.A. Opredeleniye kriticheskikh nagruzok energeticheskim metodom s uchetom deformatsiy sdviga [Determination of critical loads by the energy method taking into account shear deformations] // Vestnik KGTU im. A.N. Tupoleva. 2006. №1. S. 3–8.
  53. Oreshko E.I., Erasov V.S., Podzhivotov N.Yu. Vybor shemy raspolozheniya vysokomodulnyh sloev v mnogoslojnoj gibridnoj plastine dlya ee naibolshego soprotivleniya potere ustojchivosti [Arrangement of high-modular layers in a multilayer hybrid plate for its greatest resistance to stability loss] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 109–117. DOI: 10.18577/2071-9140-2014-0-S4-109-117.
  54. Viktorov E.G. Podrastaniye i izlom otsloyeniy v kompozitakh pri szhatii [Growth and fracture of delaminations in composites during compression] // Mekhanika materialov i konstruktsiy. M.: Izd-vo MEI, 1982. S. 36–40.
  55. Tarnopolskiy Yu.M. Rassloyeniye szhimayushchikh sterzhney iz kompozitov [Lamination of compressive rods of composites] // Razrusheniye kompozitnykh materialov. Riga, 1979. S. 160–166.
  56. Tarnopolskiy Yu.M., Khitrov V.V., Shemshurin M.V., Vasilevskiy V.M. Opasnost rassloyeniya korotkikh metallokompozitnykh sterzhney pri osevom szhatii [Danger of stratification of short metal-composite rods under axial compression] // Mekhanika polimerov. 1978. №1. S. 2–33.
  57. Troshin V.P. K ustoychivosti tsilindricheskikh obolochek s rassloyeniyami [To the stability of cylindrical shells with bundles] // Mekhanika kompozitnykh materialov. 1981. №4. C. 729–731.
  58. Bottega W.J., Maewal A. Delamination buckling and growth in lamination // Journal Applied Mechanics. 1983. Vol. 50. No. 1. P. 184–189.
  59. Chai H., Babcock C.D., Knous W.G. One dimensional modeling of failure in laminated plates by delamination buckling // International Journal of Solids and Structures. 1981. Vol. 14. No. 11. P. 1069–1083.
  60. Chen H.P. Shear deformation theory for compressive delamination buckling and growth // AIAA Journal. 1991. Vol. 29. No. 5. P. 813–819.
  61. Kim S., Cho M. Efficient higher-order shell theory for laminated composites with multiple delaminations // AIAA Journal. 2003. Vol. 41. No. 5. P. 941–950.
  62. Kulkarni S.V., Frederick D. Propagation of delamination in a laiered cylindrical shell // International Journal of Fracture. 1973. Vol. 9. No. 1. P. 113–115.
  63. Mysyk D.A., Shakimov L.A. Eksperimentalno-teoreticheskoye issledovaniye ustoychivosti trekhsloynykh stekloplastikovykh tsilindricheskikh obolochek [Experimental and theoretical study of the stability of three-layer fiberglass cylindrical shells] // Mekhanika konstruktsiy iz kompozitsionnykh materialov. Kiev: Naukova dumka, 1977. S. 110–118.
  64. Oreshko E.I., Erasov V.S., Podzhivotov N.Yu., Lutsenko A.N. Raschet na prochnost gibridnoj paneli kryla na baze listov i profilej iz vysokoprochnogo alyuminijlitievogo splava i sloistogo alyumostekloplastika [Strength calculation of hybrid wing panel on the basis of sheets and profiles from high-strength aluminum lithium alloy and laminated aluminum fiberglass] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 53–61. DOI: 10.18577/2071-9140-2016-0-1-53-61.
  65. Wang S.S., Zahlan N.M. Sicemasu H. Compressive stability of delamination random short-fiber composite // Journal of Composite materials. 1985. Vol. 19. No. 4. P. 317–333.
  66. Way S. Bending of Circular Plates with Large Deflection // Transactions of the American Society of Mechanical Engineers. 1934. Vol. 23. No. 56. P. 627–636.
  67. Whitcomb J.D. Finite element analysis of instability related delamination growth // Journal of Composite Materials. 1981. Vol. 15. P. 403–426.
  68. Yin Wo-L., Sallam S.N., Simitsees C.J. Ultimate axial load capacity of a delaminates bam-plate // AIAA Journal. 1986. Vol. 24. No. 1. P. 123–128.
  69. Kollerov M.Yu., Usikov V.D., Kuftov V.S., Gusev D.E., Oreshko E.I. Mediko-tekhnicheskoye obosnovaniye ispolzovaniya titanovykh splavov v implantiruyemykh konstruktsiyakh dlya stabilizatsii pozvonochnika [Medico-technical rationale for the use of titanium alloys in implantable structures to stabilize the spine] // Titan. 2013. №1 (40). S. 39–45.
  70. Gusev D.E., Kollerov M.Yu., Rudakov S.S., Korolev P.A., Oreshko E.I. Otsenka biomekhanicheskoy sovmestimosti implantiruyemykh opornykh plastin iz splavov na osnove titana i nikelida titana metodom kompyuternogo modelirovaniya [Assessment of the biomechanical compatibility of implantable base plates of alloys based on titanium and titanium nickelide using computer simulation] // Titan. 2011. №3 (33). S. 39–44.
  71. Basov K.A. Graficheskiy interfeys kompleksa ANSYS [Graphic interface of the ANSYS comple]. M.: DMK Press, 2006. 248 s.
  72. Oreshko E.I., Erasov V.S., Lutsenko A.N. Matematicheskoe modelirovanie deformirovaniya konstrukcionnogo ugleplastika pri izgibe [Mathematical modeling of deformation constructional carbon fiber at a bend] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 50–59. DOI: 10.18577/2071-9140-2016-2-50-59.
  73. Borovkov A.I. Vozmozhnosti sistemy konechno-elementnogo modelirovaniya ANSYS/LS–DYNA [Possibilities of the system of finite element modeling ANSYS / LS – DYNA] // Sb. mater. I Mezhdunar. konf. polzovateley programmnogo obespecheniya ANSYS E. M.: EMT–ANSYS-tsentr, 2003. S. 128–136.
  74. Oreshko E.I., Erasov V.S., Lucenko A.N., Terentev V.F., Slizov A.K. Postroenie diagramm deformirovaniya v trehmernom prostranstve σ–ε–t [Creation of the 3D stress-strain diagrams σ–ε–t] // Aviacionnye materialy i tehnologii. 2017. №1 (46). S. 61–68. DOI: 10.18577/2071-9140-2017-0-1-61-68.
  75. Chigarev A.V., Kravchuk A.S., Smalyuk A.F. ANSYS dlya inzhenerov: sprav. posob. [ANSYS for engineers: ref. benefit]. M: Mashinostroyeniye-1, 2004. 512 s.
  76. Kotov A.G. Osnovy modelirovaniya v srede ANSYS: ucheb. posobiye [Basics of modeling in the ANSYS environment: study guide]. Perm: Perm. gos. tekhn. un-t, 2008. 200 s.
  77. Kravchuk A.S., Smalyuk A.F., Kravchuk A.I. Elektronnaya biblioteka mekhaniki i fiziki: lektsii po ANSYS s primerami resheniya zadach v pyati chastyakh [Electronic library of mechanics and physics: lectures on ANSYS with examples of solving problems in five parts]. Minsk: BGU, 2013. CH. 5. S. 105.
  78. Oreshko E.I., Erasov V.S., Krylov V.D. Construction of 3D stress-strain diagram for the analysis of mechanical behavior of the material tested at various loading rates // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 59–66. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  79. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  80. Grishin V.I., Dzyuba A.S., Dudarkov Yu.I. Prochnost i ustoychivost elementov i soyedineniy aviatsionnykh konstruktsiy iz kompozitov [Strength and stability of elements and compounds of aircraft structures made of composites]. M.: Fizmatlit, 2013. S. 81–84.
  81. Oreshko E.I., Erasov V.S., Lutsenko A.N. Osobennosti raschetov ustojchivosti sterzhnej i plastin [Calculation features of cores and plates stability] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 74–79. DOI: 10.18577/2071-9140-2016-0-4-74-79.
  82. Kollerov M.Yu., Gusev D.E., Oreshko E.I. Eksperimentalno-teoreticheskoye obosnovaniye vybora metoda i implantatov dlya ustraneniya voronkoobraznoy deformatsii grudnoy kletki [Experimental and theoretical substantiation of the choice of the method and implants for eliminating funnel chest deformation] // Nauchnyye trudy (Vestnik MATI). 2012. №19 (91). S. 331–336.
  83. Kollerov M.Yu., Yegorova M.V., Oreshko E.I. i dr. Eksperimentalno-teoreticheskoye obosnovaniye algoritma rannego ortodonticheskogo lecheniya detey s odnostoronney rasshchelinoy guby i neba neyemnymi apparatami [Experimental and theoretical substantiation of the algorithm of early orthodontic treatment of children with unilateral cleft lip and palate with non-removable devices] // Stomatologiya detskogo vozrasta i profilaktika. 2011. T. KH. №1 (36). S. 23–27.
  84. Timoshenko S.P. Ustoychivost sterzhney, plastin i obolochek [Stability of rods, plates and shells]. M.: Nauka, 1971. S. 34–41.
  85. Volmir A.S. Ustoychivost deformiruyemykh system [Stability of deformable systems]. M.: Nauka, 1967. S. 20–27.
  86. Oreshko E.I., Erasov V.S., Lutsenko A.N. Kriticheskiye napryazheniya poteri ustoychivosti v gibridnykh sloistykh plastinakh [Critical voltages of buckling in hybrid layered plates] // Materialovedeniye. 2016. №11. S. 17–21.
  87. Ponomarev S.D., Biderman V.L., Likhachev K.K. i dr. Raschety na prochnost v mashinostroyenii [Strength calculations in mechanical engineering]. M.: Gos. nauch.-tekhn. izd-vo mashinostroitelnoy lit., 1959. T. 3. S. 764–768.
  88. Oreshko E.I., Erasov V.S. Chislennyye issledovaniya ustoychivosti plastin s sharnirno zakreplennymi poperechnymi kromkami [Numerical studies of the stability of plates with hinged transverse edges] // Deformatsiya i razrusheniye materialov. 2018. №6. S. 7–11.
  89. Oreshko E.I., Erasov V.S., Kachan D.V., Lashov O.A. Researches of stability of cores and plates at compression with the jammed cross-section edges // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №9 (69). St. 07. Available at: http://www.viam-works.ru (accessed: October 19, 2018). DOI: 10.18577/2307-6046-2018-0-9-61-70.
  90. Belyaev N.M. Soprotivleniye materialov [Strength of materials]. M.: Gos. izd-vo tekhn.-teor. lit., 1953. S. 83–85.