Features of the mechanism of friction of elastomeric materials of different types. Theoretical and practical aspects (review)

Alifanov E.V., Chaykun A.М., Gorlov D.S., Venediktova M.A.
Alifanov E.V., Chaykun A.М., Gorlov D.S., Venediktova M.A. Features of the mechanism of friction of elastomeric materials of different types. Theoretical and practical aspects (review) // Proceedings of VIAM. 2018. No. 1. DOI: 10.18577/2307-6046-2018-0-1-8-8. URL: https://www.viam-works.ru/en/journal/2018/1/8
Keywords
rubber, tribology, friction, coefficient friction, the rubber wear-resistance, hysteresis, automobile tires, nonslip coating.
Abstract

The overview is devoted to the analysis of the mechanism of friction of elastomeric materials. Products from them are in large quantities applied as accessories in products of aviation engineering. Theoretical and practical aspects of friction and wear of polymeric materials including elastomer features of application of lubricant and its influence on character of friction and wear of elastomer Are shown are analyzed. Features of the mechanism of friction of elastomeric materials of different classes are given. Modern development of VIAM Federal State Unitary Enterprise in the field of nonskid polymer coatings for aviation application is shown. Are noted their basic components and defined their technical characteristics.

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Bartenev G.N., Lavrentev V.V. Trenie i iznos polimerov [Friction and wear of polymers]. M.: Himiya, 1984. 224 s.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  5. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  6. Kablov E.N. Materialy dlya aviakosmicheskoj tehniki [Materials for aerospace equipment ] // Vse materialy. Enciklopedicheskij spravochnik. 2007. №5. S. 7–27.
  7. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  8. Shajdakov V.V. Svojstva i ispytanie rezin [Properties and testing of rubbers]. M.: Himiya, 2002. 231 s.
  9. Mur D. Trenie i smazka elastomerov [Friction and lubricant of elastomer]. M.: Himiya, 1977. 262 s.
  10. Erasov V.S., Oreshko E.I., Lutsenko A.N. Povrezhdaemost materialov pri staticheskom rastyazhenii [Damageability of materials in tension testing] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 91–94. DOI: 10.18577/2071-9140-2015-0-4-91-94.
  11. Krylov V.D., Yakovlev N.O., Kurganova Yu.A., Lashov O.A. Mezhsloevaya treshchinostoikost konstruktsionnykh polimernykh kompozitsionnykh materialov [Mezhsloyevy crack firmness of constructional polymeric composite materials] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 79–85. DOI: 10.18577/2071-9140-2016-0-1-79-85.
  12. Murashov V.V. Ocenka stepeni nakopleniya mikropovrezhdenij struktury PKM v detalyah i konstrukciyah nerazrushayushhimi metodami [Assessment of accumulation degree of microdamages of PCM structure in structures determined by nondestructive methods] // Aviacionnye materialy i tehnologii. 2016. №3 (42). S. 73–81. DOI: 10.18577/2071-9140-2016-0-3-73-81.
  13. Koshelev F.F., Kornev A.E., Bukanov A.M. Obshhaya tehnologiya reziny [General technology of rubber]. M.: Himiya, 1978. 527 s.
  14. Slovar-spravochnik po treniyu, iznosu i smazke detalej mashin [The dictionary reference on friction, wear and lubricant of details of machines]. Kiev: Naukova dumka, 1979. 188 s.
  15. Bulgin D., Hubbard G.D., Walters M.H. Road and laboratory studies of friction of elastomers // Rubber technology conference. London, 1962. P. 173–188.
  16. Kummer H.W., Meyer W.E. New theory permits better frictional coupling between tire and rout // Automobile congress. Munich, 1966. Paper №B11.
  17. Denny D.F. The influence of load surface roughness on the friction of rubber-like materials // Proceeding of the Royal Society. 1953. Vol. 66. P. 386.
  18. Moore D.F. An elastohydrodynamic theory of tire skidding // Automobile congress FISITA. Barcelona, 1968. Paper No. 11.
  19. Chaikun A.M., Naumov I.S., Alifanov E.V. Rezinovye uplotnitelnye materialy (obzor) [Rubber sealing materials (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №1 (49). St. 12. Available at: http //www.viam-works.ru (accessed: December 04, 2017). DOI: 10.18577/2307-6046-2017-0-1-12-12.
  20. Mashinostroitelnyj gidroprivod / pod red. V.N. Prokofeva [Machine-building hydraulic actuator / ed. by V.N. Prokofev]. M.: Mashinostroenie, 1978. 495 s.
  21. Evzovich V.E., Rajbman P.G. Avtomobilnye shiny i kolesa. Naznachenie, ekspluataciya. 2-e izd. [Automobile tires and wheels. Assignment, operation. 2nd ed.]. M.: MIROS, 2012. 160 s.