Directions for the development of manufacturing technologies in the field of rare earth metals

Sevastyanov D.V., Doriomedov M.S., Sutubalov I.V., Kulagina G.S.
Sevastyanov D.V., Doriomedov M.S., Sutubalov I.V., Kulagina G.S. Directions for the development of manufacturing technologies in the field of rare earth metals // Proceedings of VIAM. 2018. No. 1. DOI: 10.18577/2307-6046-2018-0-1-4-4. URL: https://www.viam-works.ru/en/journal/2018/1/4
Keywords
rare earth metals, trends, manufacturing technologies.
Abstract

Based on the analysis of scientific and technical literature, the main trends in the development of manufacturing technologies in the field of rare-earth metals were revealed. These trends include recovery of rare earths from end-of-life products (fluorescent lamps, permanent magnets, Ni-MH batteries) and industrial waste as well as production of high-purity rare earth metals. The special features of the applied technologies and the further development of technological solutions in this area were presented.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  3. Jha M.K., Kumari A., Panda R. et al. Review on hydrometallurgical recovery of rare earth metals // Hydrometallurgy. 2016. Vol. 165. P. 2–26.
  4. Binnemans K., Jones P.T., Blanpain B. et al. Recycling of rare earths: A critical review // Journal of Cleaner Production. 2013. Vol. 51. P. 1–22.
  5. Wu Y., Yin X., Zhang Q. et al. The recycling of rare earths from waste tricolor phosphors in fluorescent lamps: A review of processes and technologies // Resources, Conservation and Recycling. 2014. Vol. 88. P. 21–31.
  6. Binnemans K., Jones P.T. Perspectives for the recovery of rare earths from end-of-life fluorescent lamps // Journal of Rare Earths. 2014. Vol. 32. No. 3. P. 195–200.
  7. Method for recovering rare-earth elements from a solid mixture containing a halophosphate and a compound of one or more rare earth elements: pat. US8501124B2; publ. 06.08.13.
  8. Kablov E.N., Ospennikova O.G., Rezchikova I.I., Valeev R.A. i dr. Sravnenie temperaturnoj stabilnosti magnitov na osnove SmCo i PrDy–FeCo–B [Comparison of the temperature stability of SmCo and PrDy–FeCo–B magnets] // Aviacionnye materialy i tehnologii. 2015. №S2. S. 42–46. DOI: 10.18577/2071-9140-2015-0-S2-42-46.
  9. Kablov E.N., Ospennikova O.G., Piskorskij V.P., Valeev R.A. i dr. Fazovyj sostav spechennyh materialov sistemy Nd–Dy–Fe–Co–B [Phase composition of Nd–Dy–Fe–Co–B sintered materials] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 95–100. DOI: 10.18577/2071-9140-2014-0-s5-95-100.
  10. Tanaka M., Oki T., Koyama K. et al. Recycling of rare earths from scrap // Handbook on the Physics and Chemistry of Rare Earths. 2013. Vol. 43. P. 159–211.
  11. Zhang Z., Jia Q., Liao W. Progress in the separation processes for rare earth resources // Handbook on the Physics and Chemistry of Rare Earths. 2015. Vol. 48. P. 287–376.
  12. Takeda O., Okabe T.H. Current status on resource and recycling technology of rare earths // Metallurgical and Materials Transactions: E. 2014. Vol. 1A. No. 2. P. 160–173.
  13. Ferron C.J., Henry P. A review of the recycling of rare earth metals // Canadian Metallurgical Quarterly. 2015. Vol. 54. No. 4. P. 388–394.
  14. Kolobov G.A., Karpenko A.V. Rafinirovanie legkih redkih, redkozemel'nyh i radioaktivnyh metallov [Refinement of light rare, rare earth and radioactive metals ] // Voprosy atomnoj nauki i tehniki. 2016. №1 (101). S. 3–9.
  15. Zhang Z., Wang Z., Chen D. et al. Purification of praseodymium to 4N5+ purity // Vacuum. 2014. Vol. 102. P. 67–71.
  16. Pang S., Chen D., Li Z. et al. Theory and technology of vacuum distillation method for preparing high-purity metal neodymium // Journal of the Chinese Rare Earth Society. 2013. Vol. 1. P. 14–19.
  17. Cheng W., Li Z., Chen D. et al. Preparation of high purity lanthanum by combined method of
  18. lithium-thermal reduction and vacuum distillation // Chinese Journal of Rare Metals. 2011. Vol. 35. P. 781–785.
  19. Novel method for utilizing hydrogen plasma electric arc melting technology to prepare high-purity rare earth gadolinium elementary substance: pat. CN10340650B; publ. 12.11.14.
  20. Li G., Guo H., Li L. et al. Purification of terbium by means of argon and hydrogen plasma arc melting // Journal of Alloys and Compounds. 2016. Vol. 659. Р. 1–7.
  21. Li G., Li L., Yang C. et al. Removal of gaseous impurities from terbium by hydrogen plasma arc melting // International Journal of Hydrogen Energy. 2015. Vol. 40. No. 25. P. 7943–7948.
  22. Maslov V.P., Polyakov E.G., Polyakova L.P., Stangrit P.T. Elektroliticheskoe nanesenie pokrytij i elektrorafinirovanie redkih metallov v solevyh rasplavah [Electrolytic drawing coverings and electrorefinement of rare metals in salt melt] // Cvetnye metally. 2000. №10. S. 66–70.