Efficiency of improvement of quality of products from polycarbonate heat treatment

Petrova G.N., Starostina I.V., Rumyantseva T.V., Sapego Yu. A.
Petrova G.N., Starostina I.V., Rumyantseva T.V., Sapego Yu. A. Efficiency of improvement of quality of products from polycarbonate heat treatment // Proceedings of VIAM. 2017. No. 9. DOI: 10.18577/2307-6046-2017-0-9-6-6. URL: https://www.viam-works.ru/en/journal/2017/9/6
Keywords
quality, polycarbonate, glycerin, oil, ultrasound, heat treatment, annealing.
Abstract

Results of researches on influence of modes of heat treatment of polycarbonate are given in article on quality of products made of it, Is shown that the choice of thermoplastic is caused by high level of the physicist – mechanical properties, dimensional stability, high accuracy when molding, good decorative look, and also expansion of areas of its application. Conditions of need of carrying out heat treatment for this material are given. It is shown that simple on configuration, thin-walled, irresponsible assignment of detail can be not subjected to heat treatment; at the same time the details working in the field of high temperatures, in surface-active environments, details of difficult configuration and having metal armature, it is reasonable to subject to heat treatment. Results of influence of different modes of heat treatment (tempering, annealing, etc.) on physical, strength and deformation properties of samples of material are given. On the basis of the received test results

Reference list
  1. Sadova A.N., Kuznecova O.N., Arhireev V.P. i dr. Principy upravleniya kachestvom polimernoj produkcii [Principles of quality management of polymeric products]. M.: KolosS, 2009. 319 s.
  2. Starostina I.V., Dodonova R.N., Polepkina N.A. Kontrol i upravlenie kachestvom produkcii [Control and product quality control] // Materialy i tehnologii dlya aviacionno-kosmicheskoj tehniki: sb. tez. dokl. nauch.-tehnich. konf. M.: VIAM, 2005. S. 5–12.
  3. Orehov N.G., Starostina I.V. Analiz kachestva litoj prutkovoj (shihtovoj) zagotovki iz zharoprochnyh splavov proizvodstva FGUP «VIAM» // Aviacionnye materialy i tehnologii. 2014. №S5. S. 23–30. DOI: 10.18577/2071-9140-2014-0-s5-23-30.
  4. Petrova G.N., Starostina I.V., Rumyanceva T.V. Issledovanie vozmozhnosti markirovki detalej iz polikarbonata [Study of the possibility of marking parts of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №10. St. 11. Available at: http://www.viam-works.ru (accessed: February 08, 2017). DOI: 10.18577/2307-6046-2016-0-10-11-11.
  5. Sudarushkin Yu.K., Gudimov M.M., Romanov D.S., Sokolov M.Yu. Primenenie litevyh polikarbonatov v aviapriborostroenii [Application of molding polycarbonates in avionics] // Aviacionnaya promyshlennost. 2003. №2. S. 48–52.
  6. Petrova G.N., Bejder E.Ya., Starostina I.V. Litevye termoplasty dlya izdelij aviacionnoj tehniki [Molding thermoplastics for products of aviation engineering] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №6. S. 10–15.
  7. Kryzhanovskij V.K., Burlov V.V., Panimatchenko A.D., Kryzhanovskaya Yu.V. Tehnicheskie svojstva polimernyh materialov [Engineering properties of polymeric materials]. SPb.: Professiya, 2005. 238 s.
  8. Simonov-Emel'yanov I.D, Yurkin A.A., Surikov P.V. i dr. Ocenka effektivnosti dejstviya reologicheskih dobavok pri pererabotke polikarbonata [Assessment of efficiency of action of rheological additives when processing polycarbonate] // Plasticheskie massy. 2015. №7–8. S. 37–40.
  9. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  10. Petrova G.N., Abakumova N.M., Rumyanceva T.V. i dr. Pozharobezopasnye litevye termoplasty [Fireproof molding thermoplastics] // Plasticheskie massy. 2005. №1. S. 45–46.
  11. Petrova G.N., Rumyanceva T.V., Beyder E.Ya. Vliyanie modificiruyushhih dobavok na pozharobezopasnye svojstva i tehnologichnost polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №6. St. 06. Available at: http://www.viam-works.ru (accessed: July 19, 2017).
  12. Lazareva T.K., Ermakin S.N., Kostyagina V.A. Problemy sozdaniya kompozicionnyh materialov na osnove konstrukcionnyh termoplastov [Problems of creation of composite materials on the basis of constructional thermoplastics] // Uspehi v himii i himicheskoj tehnologii. 2010. T. 24. №4. S. 58–63.
  13. Kerber M.L., Vinogradov V.M., Golovkin G.S. i dr. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologiya [Polymeric composite materials: structure, properties, technology]. SPb.: Professiya, 2011. S. 32–33.
  14. Kablov E.N. Additivnye tehnologii – dominanta nacional'noj tehnologicheskoj iniciativy [The additive technologies – dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
  15. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  16. Petrova G.N., Larionov S.A., Platonov M.M., Perfilova D.N. Termoplastichnye materialy novogo pokoleniya dlya aviacii [Thermoplastic materials of new generation for aviation] // Aviacionnye materialy i tehnologii 2017. №S. S. 420–436. DOI: 10.18577/2071-9140-2017-0-S-420-436.
  17. Petrova G.N., Platonov M.M., Bolshakov V.A., Ponomarenko S.A. Issledovanie kompleksa harakteristik bazovyh materialov dlya FDM tehnologii additivnogo sinteza. Fiziko-mehanicheskie i teplofizicheskie svojstva [Research of complex of characteristics of base materials for FDM technology of the additive synthesis. Physicomechanical and heatphysical properties] // Plasticheskie massy. 2016. №5–6. S. 53–58.
  18. Petrova G.N., Larionov S.A., Sapego Yu.A., Platonov M.M. Reologicheskie svojstva termoplastichnoj kompozicii na osnove polikarbonata: zavisimost ot temperatury pererabotki; vliyanie na mehanicheskie harakteristiki i razmernuyu stabilnost obektov, sozdannyh po FDM-tehnologii [Rheological properties of the thermoplastic composition with a reduced fire hazard polycarbonate-based: depending on the temperature processing; effect on mechanical properties and stability dimension objects created software FDM-technology] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4 (52). St. 09. Available at: http://viam-works.ru (accessed: July 19, 2017). DOI: 10.18577/2307-6046-2017-0-4-9-9.
  19. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Optimizaciya sostava polimernoj kompozicii s ponizhennoj pozharnoj opasnostyu na osnove polikarbonata dlya tehnologii 3D-pechati rasplavlennoj polimernoj nityu [Optimization of structure of polymeric composition with the lowered fire danger on the basis of polycarbonate for technology of the 3D-press the melted polymeric thread] // Izvestiya vuzov. Himiya i himicheskaya tehnologiya. 2017. T. 60. №1. S. 87–94.
  20. Petrova G.N., Beider E.Yа. Construction materials based on reinforced thermoplastics Chemistry and Materials Science // Russian Journal of General Chemistry. 2011. Vol. 81. No. 5. Р. 1001–1007.
  21. Novakova-Marcincinova L., Novak-Marcincin J. Verification of mechanical properties of abs materials used in FDM rapid prototyping technology // Proceedings in Manufacturing Systems. 2016. Vol. 8. Is. 2. P. 87–92.
  22. Smirnov O.I., Skorodumov S.V. Modelirovanie tehnologii poslojnogo sinteza pri razrabotke izdelij slozhnoj formy [Modeling of technology of level-by-level synthesis when developing products of difficult form] // Sovremennye naukoemkie tehnologii. 2010. №4. S. 83–87.
  23. Moskatov K.A. Termicheskaya obrabotka plastmassovyh i rezinovyh detalej mashin [Thermal processing of plastic and rubber details of machines]. M.: Mashinostroenie, 1976. 200 s.
  24. Kestelman N.Ya. Termicheskaya obrabotka polimernyh materialov v mashinostroenii [Thermal processing of polymeric materials in mechanical engineering]. M.: Mashinostroenie, 1968. S. 170–201.
  25. Sposob obrabotki izdelij iz polikarbonata: a. s. 804659 [Way of processing of products from polycarbonate: copyright certificate 804659]; zayavl. 19.04.79; opubl. 15.02.81.
  26. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.