Determination of boron in solders based on nickel VPr24 and VPr27

Titov V.I.
Titov V.I. Determination of boron in solders based on nickel VPr24 and VPr27 // Proceedings of VIAM. 2017. No. 9. DOI: 10.18577/2307-6046-2017-0-9-12-12. URL: https://www.viam-works.ru/en/journal/2017/9/12
Keywords
photometry, H-resorcinol, complexon III, boron, nickel solders.
Abstract

As a result of the research and experimental work on the possible determination of boron content in solders based on nickel VPr24 and VPr27, a photometric analysis method was used. The main reagent was chosen H-resorcinol. Using this reagent, the reaction proceeds in a weakly acidic medium, there is no need to extract the complex formed with organic solvents. During the experiment, it was found that one of the components of the solder – niobium – interacts with the reagent H-resorcinol, thereby negatively affecting the possibility of correct determination of boron content. Masking reagent, allowing to obtain correct results of the analysis, was selected complexon III. To prevent loss of boron during the sample preparation, phosphoric acid must be added. As a result of the conducted studies, a technique for determining the boron content in the concentration range 0,1–3,0% by weight was developed in solders based on nickel VPr24 and VPr27.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [What the future to make of? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  4. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  5. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy VIAM 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
  6. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. 3-e izd. [Tendencies and reference points of innovative development of Russia: collection scientific informatsio ny materials. 3rd ed.]. M.: VIAM, 2015. 720 s.
  7. Lukin V.I., Koval'chuk V.G., Samorukov M.L., Gridnev Yu.M. Issledovanie vliyaniya tehnologii rotacionnoj svarki treniem deformiruemogo zharoprochnogo nikelevogo splava VZh175 na strukturu i prochnostnye harakteristiki svarnyh soedinenij [Research of influence of technology of rotational friction bonding of deformable heat resisting VZh175 nickel alloy on structure and strength characteristics of welded connections] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 114–121.
  8. Sorokin L.I. Svarivaemost zharoprochnyh splavov, primenyaemyh v aviacionnyh gazoturbinnyh dvigatelyah [Bondability of the hot strength alloys applied in aviation gas turbine engines] // Svarochnoe proizvodstvo. 1997. №4. S. 4–11.
  9. Lukin V.I., Sorokin L.I., Bagdasarov Yu.S. Svarivaemost' litejnyh zharoprochnyh nikelevyh splavov tipa ZhS6M [Bondability of cast heat resisting nickel alloys of the ZhS6M type] // Svarochnoe proizvodstvo. 1997. №6. S. 12–17.
  10. Lukin V.I., Semenov V.N., Starova L.L. i dr. Obrazovanie goryachih treshhin pri svarke zharoprochnyh splavov [Formation of hot cracks when welding hot strength alloys] // MiTOM. 2007. №12. S. 7–14.
  11. Horunov V.F., Maksimova S.V. Pajka zharoprochnyh splavov na sovremennom etape [The soldering of hot strength alloys at the present stage] // Svarochnoe proizvodstvo. 2010. №10. S. 24–27.
  12. Rylnikov V.S. Voprosy po pajke, reshennye v processe izgotovleniya izdeliya «Buran» [Some problems of brazing solved in the course of manufacture of «Buran» reusable spaceship] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 33–34.
  13. Lukin V.I., Banas I.P., Kovalchuk V.G., Golev E.V. Argono-dugovaya svarka vysokoprochnoj cementuemoj stali VNS-63 [TIG welding of high-strengthened cemented steel VNS-63] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 01. Available at: http://www.viam-works.ru (accessed: June 01, 2017).
  14. Afanasev-Hodykin A.N., Lukin V.I., Rylnikov V.S. Vysokotehnologichnye polufabrikaty zharoprochnyh pripoev (lenty i pasty na organicheskom svyazuyushhem) [High-tech semi-finished high-temperature solders (tape and paste on an organic binder] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 02. Available at: http://viam-works.ru (accessed: June 01, 2017).
  15. Rylnikov V.S., Afanasev-Hodykin A.N., Galushka I.A. Tehnologiya pajki konstrukcii tipa «blisk» iz raznoimennyh splavov [Technology of the soldering of design of the blisk type from heteronymic alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №10. St. 02. URL: http://www.viam-works.ru (accessed: June 01, 2017).
  16. Ryl'nikov V.S., Afanas'ev-Hodykin A.N., Krasikov M.I. Issledovanie remontnoj tehnologii ispravleniya defektov payanyh soedinenij toplivnyh kollektorov [Research of repair technology of correction of defects of sweated connections of fuel manifolds] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №12. St. 02. URL: http://www.viam-works.ru (accessed: June 01, 2017).
  17. Titov V.I., Gundobin N.V., Pilipenko L.V. Opredelenie niobiya v pripoe VPr17 [Determination of niobium in VPr17 solder] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 10. URL: http://www.viam-works.ru (accessed: June 01, 2017). DOI: 10.18577/2307-6046-2015-0-5-10-10.
  18. Titov V.I., Gundobin N.V., Pilipenko L.V. Razrabotka metoda opredeleniya soderzhaniya fosfora v pripoe VPr18 [Development of a method for determination of phosphorus in the solder VPr18] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 11. URL: http://www.viam-works.ru (accessed: June 01, 2017). DOI: 10.18577/2307-6046-2015-0-11-11-11.