Evaluation of binder VST-1210 with different curing modes by sclerometry methods

Veshkin E.A, Postnov V.I., Semenychev V.V.
Veshkin E.A, Postnov V.I., Semenychev V.V. Evaluation of binder VST-1210 with different curing modes by sclerometry methods // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-9-9. URL: https://www.viam-works.ru/en/journal/2017/8/9
Keywords
binder, cure modes, sclerometry, microscopic studies, microhardness.
Abstract

Cured samples from the binder VST-1210 with the help of a laboratory sclerometer were applied to scratches under various loads on the diamond indenter, after which the character of the formed grooves and their geometry were studied. It has been established that the microhardness of the samples and the nature of the grooves depend on the modes of curing the binder. The applied method of sclerometry made it possible to determine the curing regimes of the samples in which, after the action of the indenter, the plastic is cracked, or the chevron character of the channel of the groove, indicating a low degree curing.

Reference list
  1. Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod obshh. red. E.N. Kablova [Armor for «Buran». Materials and VIAM technologies for ISS of «Energiya–Buran» / gen. ed. by E.N. Kablov]. M.: Nauka i zhizn, 2013. 128 s.
  2. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Kablov E.N. VIAM. Napravlenie glavnogo udara [Direction of main attack] // Nauka i zhizn. 2012. №6. S. 14–18.
  4. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  5. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. 520 s.
  6. Sposob izgotovleniya detalej iz polimernyh kompozicionnyh materialov: pat. 2574269 Ros. Federaciya [Way of manufacturing of details from polymeric composite materials: part. 2574269 Rus. Federation]; opubl. 14.11.14, Byul. №4.
  7. Postnov V.I., Strelnikov S.V., Makrushin K.V., Veshkin E.A. Semipreg dlya polimernyh osnastok [Semipreg for polymeric equipments] // Izvestiya Samarskogo nauchnogo centra Rossijskoj akademii nauk. 2016. T. 18. №4 (3). S. 183–185.
  8. Postnov V.I., Pletin I.I., Veshkin E.A., Starostina I.V. Tehnologicheskie osobennosti proizvodstva tonkolistovyh obshivok lopastej vertoleta iz konstrukcionnogo stekloplastika VPS-53K [Technological features of production it is thin sheet coverings of blades of the helicopter from constructional VPS-53K fibreglass] // Izvestiya Samarskogo nauchnogo centra Rossijskoj akademii nauk. 2016. T. 18. №4 (3). S. 186–188.
  9. Veshkin E.A. Osobennosti bezavtoklavnogo formovaniya nizkoporistykh PKM [Features of out-of-autoclave forming of poor-porous PCM] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2016. №2. St. 07. Available at: http://www.viam-works.ru (accessed: May 11, 2017). DOI 10.1857/2307-6046-2016-0-2-7-7
  10. Semenychev V.V. Nikelirovanie stali metodom elektronatiraniya [Nickel plating became method of electrograting] // Galvanotehnika i obrabotka poverhnosti. 2017. №1. S. 23–27.
  11. Semenychev V.V., Panarin A.V. Primenenie sklerometrii dlya povysheniya informativnosti izmeryaemyh harakteristik hromovyh i nikelevyh pokrytij [Application of sclerometry for more informativeness measured characteristics of chromium and nickel coatings] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2016. №3 (21). St. 05. Available at: http://materialsnews.ru (accessed: May 11, 2017).
  12. Semenychev V.V., Salahova R.K. Ocenka adgezii nikel-kobaltovogo pokrytiya k steklo- i ugleplastiku metodom carapanya [Evaluation of nickel-cobalt coating adhesion to fiberglass and carbon fiber–reinforced plastic by scratching] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7 (43). St. 06. Available at: http://www.viam-works.ru (accessed: May 11, 2017). DOI: 10.18577/2307-6046-2016-0-7-6-6.
  13. Semenychev V.V., Salahova R.K. Sklerometriya kak metod ocenki intensivnosti mezhkristallitnoj korrozii [Sclerometry as method of assessment of intensity between crystallite corrosion] // Korroziya: materialy, zashhita. 2015. №12. S. 37–41.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Semenychev V.V., Salahova R.K. Pribor dlya ocenki svojstv pokrytij [The device for assessment of properties of coverings] // Zavodskaya laboratoriya. Diagnostika materialov. 2017. T. 83. №2. S. 60–65.