To the problem of determining the moisture sorbed in polymeric composite materials

Nikolaev E.V., Pavlov M.R., Laptev A.B., Ponomarenko S.A.
Nikolaev E.V., Pavlov M.R., Laptev A.B., Ponomarenko S.A. To the problem of determining the moisture sorbed in polymeric composite materials // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-7-7. URL: https://www.viam-works.ru/en/journal/2017/8/7
Keywords
polymer composite materials, epoxy binder, cyanide binder, carbon fiber, fiberglass, natural weathering test, chromatography-mass spectrometer, titrimetry, Fourier infrared spectroscopy.
Abstract

The content of moisture sorbed in polymeric composite materials of various nature was estimated by three different methods of physico-chemical analysis. The applicability of all analytical methods is shown. Recommendations on preparation conditions for each type of materials studied are proposed.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials is the security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  3. SNiP 28.13330.2012. Zashhita stroitelnyh konstrukcij ot korrozii [Health Regulations and Norms 28.13330.2012. Protection of construction designs against corrosion]. M.: Min-vo regionrazvitiya RF, FAU «FCS», 2012. 54 s.
  4. FWHA-RD-01-156. Nace Corrosion 2010 Wrap-Up report. 19 р. Available at: http://www.nace.org (accessed: April 05, 2017).
  5. Polyakova A.V., Krivushina A.A., Goryashnik Yu.S., Yakovenko T.V. Ispytaniya na mikrobiologicheskuyu stojkost v usloviyah teplogo i vlazhnogo klimata [Microbiological resistance tests under conditions of warm and damp climate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №7. St. 06. Available at: http://www.viam-works.ru (accessed: April 05, 2017).
  6. Ahiyarov R.Zh., Bugaj D.E., Laptev A.B. Problemy podgotovki oborotnyh i stochnyh vod predpriyatij neftedobychi [Problems of preparation reverse and drain waters of the enterprises of oil production] // Neftepromyslovoe delo. 2008. №9. S. 61–65.
  7. Ahiyarov R.Zh., Laptev A.B., Ibragimov I.G. Povyshenie promyshlennoj bezopasnosti ekspluatacii obektov neftedobychi pri biozarazhenii i vypadenii solej metodom kompleksnoj obrabotki plastovoj vody [Increase of industrial safety of operation of objects of oil production at bioinfection and loss of salts by method of complex processing of formation water] // Neftepromyslovoe delo. 2009. №3. S. 44–46.
  8. Ahiyarov R.Zh., Matveev Yu.G., Laptev A.B., Bugaj D.E. Resursosberegayushhie tehnologii predotvrashheniya biozarazheniya plastovyh vod predpriyatij neftedobychi [Resource-saving technologies of prevention of bioinfection of formation waters of the enterprises of oil production] // Neftegazovoe delo. 2011. №5. S. 232–242.
  9. Laptev A.B., Lucenko A.N., Kurs M.G., Buharev G.M. Opyt issledovanij biokorrozii metallov [Experience of researches of biocorrosion of metals] // Praktika protivokorrozionnoj zashhity. 2016. №2 (80). S. 36–57.
  10. Antyufeeva N.V., Aleksashin V.M., Pavlov M.R., Stolyankov Yu.V. Issledovanie vozmozhnosti ispolzovaniya ugleplastikov v usloviyah arkticheskogo klimata [Research of possibility of use carbon fiber reinforced polymers in the conditions of the Arctic climate] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 86–94. DOI: 10.18577/2071-9140-2016-0-4-86-94.
  11. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy stareniya [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] // Deformaciya i razrushenie materialov. 2010. №11. S. 19–27.
  12. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. II. Relaksaciya ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging of composite materials of aviation assignment. II. Relaxation of initial structural non-equilibrium and gradient of properties on thickness] // Deformaciya i razrushenie materialov. 2010. №12. S. 40–46.
  13. Sugita Y., Winkelmann C., La Saponara V. Environmental and chemical degradation of carbon/epoxy lap joints for aerospace applications, and effects on their mechanical performance // Compos. Sci. and Technol. 2010. Vol. 70. No. 5. P. 829–839.
  14. Kirillov V.N., Efimov V.A. Problemy issledovaniya klimaticheskoj stojkosti aviacionnyh nemetallicheskih materialov [Problems of research of climatic firmness of aviation non-metallic materials] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 379–388.
  15. Mikols W.J., Seferis J.C., Apicella A., Nicolais L. Evaluation of structural changes in epoxy systems by moisture sorption-desorption and dynamic mechanical studies // Polym. Compos. 1982. Vol. 3. No. 3. P. 118–24.
  16. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Issledovanie zakonomernostej vlagoperenosa i razrabotka standarta po opredeleniyu koefficienta diffuzii i predelnogo vlagosoderzhaniya dlya ocenki mehanicheskih svojstv ugleplastikov [Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics] // Aviacionnye materialy i tehnologii. 2013. №3. S. 44–48.
  17. Mishra G., Mohapatra S.R., Behera P.R., Dash B., Mohanty U.K., Ray B.C. Environmental stability of GFRP laminated composites: an emphasis on mechanical behaviour // Aircraft Eng. and Aerosp. technol. 2010. Vol. 82. No. 4. P. 258–266.
  18. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  19. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://viam-works.ru (accessed: April 6, 2017).
  20. Firefighting and emergency responsestudy of advanced composites aircraft. Objective 2: Firefighting Effectiveness of Technologies and Agents on Composite Aircraft Fires. Distribution A: Approved for public release; distribution unlimited. 88ABW-2012-0190. January 10, 2012.
  21. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Kompleksnoe issledovanie vozdeystviya klimaticheskikh i ekspluatatsionnykh faktorov na novoe pokolenie epoksidnogo svyazuyushchego i polimernykh kompozitsionnykh materialov na ego osnove. Chast 1. Issledo-vanie vliyaniya sorbirovannoy vlagi na epoksidnuyu matritsu i ugleplastik na ee osnove [Complex research of influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 1. Research of influence of sorbirovanny moisture on epoxy matrix and carbon plastics on its basis] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2015. №12. St. 11. Available at: http://www.viam-works.ru (accessed: April 6, 2017). DOI: 10.18577/2307-6046-2015-0-12-11-11.
  22. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Kompleksnoe issledovanie vozdejstviya klimaticheskih i ekspluatacionnyh faktorov na novoe pokolenie epoksidnogo svyazuyushhego i polimernyh kompozicionnyh materialov na ego osnove. Chast 2. Obosnovanie vybora rezhimov i provedenie teplovogo stareniya polimernyh kompozicionnyh materialov na osnove epoksidnoj matricy [Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis Part 2. Substantiation of the choice of modes and conducting heat aging of polymeric composite materials based on epoxy matrix] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1. St. 10. Available at: http://www.viam-works.ru (accessed: April 7, 2017). DOI: 10.18577/2307-6046-2016-0-1-10-10.
  23. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Kompleksnoe issledovanie vozdejstviya klimaticheskih i ekspluatacionnyh faktorov na novoe pokolenie epoksidnogo svyazuyushhego i polimernyh kompozicionnyh materialov na ego osnove. Chast 3. Raschet energii aktivacii i teplovogo resursa polimernyh kompozicionnyh materialov na osnove epoksidnoj matricy [Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis Part 3. Calculation of activation energy and thermal resource of polymeric composite materials on the basis of epoxy matrix] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 11. Available at: http://www.viam-works.ru (accessed: April 7, 2017). DOI: 10.18577/2307-6046-2016-0-5-11-11.
  24. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Kompleksnoe issledovanie vozdeystviya klimaticheskikh i ekspluatatsionnykh faktorov na novoe pokolenie epoksidnogo svyazuyushchego i polimernykh kompozitsionnykh materialov na ego osnove. Chast 4. Naturnye klimaticheskie ispytaniya polimernykh kompozitsionnykh materialov na osnove epoksidnoy matritsy [Complex research of influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 4. Natural climatic tests of polymeric composite materials on the basis of epoxy matrix] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2016. №6. St. 11. Available at: http://www.viam-works.ru (accessed: April 7, 2017). DOI: 10.18577/2307-6046-2016-0-6-11-11.
  25. Kirillov V.N., Efimov V.A., Shvedkova A.K., Aleksashin V.N., Zuev A.V., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva ugleplastika KMU-11TR [Research of influence of climatic factors and mechanical loading on structure and mechanical properties carbon plastic KMU-11TP] // Sb. dokl. VIII nauch. konf. po gidroaviacii «Gidroaviasalon–2010». M.: VIAM, 2010. Ch. II. S. 111–115.
  26. Nikolaev E.V., Kirillov V.N., Efimov V.A., Grashhenkov D.V. Moskovskij centr klimaticheskih ispytanij FGUP «VIAM» – regionalnyj centr ispytanij materialov v predstavitelnoj zone umerennogo klimata [The Moscow center of climatic tests of FSUE «VIAM» – the regional center of tests of materials in representative zone of temperate climate] // Ibid. S. 202–208.