The method of impurities concentration by decrement moving rate of directed melt solidification in high gradient conditions

Min P.G., Sidorov V.V., Vadeev V.E., Bondarenko Yu.A.
Min P.G., Sidorov V.V., Vadeev V.E., Bondarenko Yu.A. The method of impurities concentration by decrement moving rate of directed melt solidification in high gradient conditions // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-3-3. URL: https://www.viam-works.ru/en/journal/2017/8/3
Keywords
silicon, phosphorus, sulfur, superalloy, impurities, nonmetallic inclusions, crystallization, method of impurities concentration, metallographic research.
Abstract

The efficiency method for concentration of nonmetallic inclusions with sulfur, phosphorus and silicon from melt of nickel-based superalloys in high gradient conditions and reduced rate of moving the crystallization front (V=6 mm/h). Experimentally established that using of this method allows to concentrate a main part of nonmetallic inclusions with sulfur, phosphorus and silicon in casting top limited volume. It makes enable detection of inclusions, chemical composition research, morphology and location in structure of alloy. In this case occurs reducing of impurities content in bottom part of casting.

Reference list
  1. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya / pod red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technologies, covers / gen. ed. by E.N. Kablov]. M.: Nauka, 2006. 632 s.
  2. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. Metallurgicheskie osnovy obespecheniya vysokogo kachestva monokristallicheskih zharoprochnyh nikelevykh splavov [The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
  3. Kablov D.E., Sidorov V.V., Min P.G., Vadeev V.E. Vliyanie primesej i lantana na ekspluatacionnye svojstva splava ZhS36-VI [Influence of impurity and lanthanum on operational properties of alloy ZhS36-VI] // Metallurgiya mashinostroeniya. 2015. №6. S. 19–23.
  4. Kablov D.E., Sidorov V.V., Min P.G., Gerasimov V.V., Bondarenko Yu. A. Vliyanie primesej sery i fosfora na svojstva monokristallov zharoprochnogo splava ZhS36-VI i razrabotka effektivnyh sposobov ego rafinirovaniya [The sulfur and phosphorus influence on properties of single crystals GHS36-VI supperalloy and design of effective methods their refining] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 3–9. DOI: 10.18577/2071-9140-2015-0-3-3-9.
  5. Kablov D.E., Belyaev M.S., Sidorov V.V., Min P.G. Vliyanie primesej sery i fosfora na malociklovuyu ustalost monokristallov zharoprochnogo splava ZhS36-VI [The influence of sulfur and phosphorus impurities on low cycle fatigue of single crystals of ZhS36-VI alloy] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 25–28. DOI: 10.18577/2071-9140-2015-0-4-25-28.
  6. Sidorov V.V., Rigin V.E., Timofeeva O.B., Min P.G. Vliyanie kremniya i fosfora na zharoprochnye svojstva i strukturno-fazovye prevrashheniya v monokristallah iz vysokozharoprochnogo splava VZhM4-VI [An effect of silicon and phosphorus on high temperature properties and structure-phase transformations of single crystals of VGM4-VI superalloy] // Aviacionnye materialy i tehnologii. 2013. №3. S. 32–38.
  7. Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I. Vliyanie fosfora i kremniya na strukturu i svojstva vysokozharoprochnyh litejnyh splavov i razrabotka effektivnyh metodov ustraneniya ih otricatelnogo vliyaniya [Influence of phosphorus and silicon on structure and properties of high-heat resisting cast alloys and development of effective methods of elimination of their negative influence] // MiTOM. 2015. №6 (720). S. 55–59.
  8. Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I., Timofeeva O.B., Filonova E.V., Ishodzhanova I.V. Vliyanie primesej na strukturu i svojstva vysokozharoprochnyh litejnyh splavov i razrabotka effektivnyh metodov ustraneniya ih otricatelnogo vliyaniya [Influence of impurity on structure and property of high-heat resisting cast alloys and development of effective methods of elimination of their negative influence] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 03. Available at: http://www.materialsnews.ru (accessed: June 19, 2017).
  9. Min P.G., Sidorov V.V., Budinovskij S.A., Vadeev V.E. Vliyanie sery na zharostojkost monokristallov zharoprochnogo nikelevogo splava sistemy Ni–Al–Co–Re–Ta–Mo–W–Ru–Cr [Influence of sulfur on the heat resistance of monocrystals of heat resisting nickel alloy of Ni–Al–Co–Re–Ta–Mo–W–Ru–Cr system] // Materialovedenie. 2016. №7. S. 9–12.
  10. Kablov D.E., Sidorov V.V., Budinovskij S.A., Min P.G. Vliyanie primesi sery na zharostojkost monokristallov zharoprochnogo splava ZhS36-VI s zashhitnym pokrytiem [The influence of sulfur impurity on heat resistance of single crystals of ZhS36-VI alloy with protective coating] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 20–23. DOI: 10.18577/2071-9140-2016-0-1-20-23.
  11. Min P.G., Sidorov V.V., Budinovskiy S.A., Vadeev V.E. Influence of Sulfur on Heat Resistance of Single Crystals of Heat-Resistant Nickel Alloy of Ni–Al–Co–Re–Ta–Mo–W–Ru–Cr System // Inorganic Materials: Applied Research. 2017. Vol. 8. No. 1. P. 90–93.
  12. Min P.G., Vadeev V.E., Kramer V.V. Resursosberegayushhaya tehnologiya polucheniya deformiruemogo nikelevogo zharoprochnogo splava VZh175 s primeneniem nekondicionnyh othodov [Resource-saving technology of receiving deformable nickel VZh175 hot strength alloy using unconditioned waste] // Metallurg. 2016. №9. S. 88–94.
  13. Min P.G., Vadeev V.E., Kalicev V.A., Kramer V.V. Tehnologiya polucheniya deformiruemogo splava VZh175 dlya diskov GTD iz kondicionnyh othodov [Technology of receiving deformable alloy ВЖ175 for disks GTE from conditioned waste] // Metallurg. 2015. №9. S. 76–80.
  14. Min P.G., Vadeev V.E., Kalicev V.A., Kramer V.V. Rafinirovanie nekondicionnyh othodov deformiruemyh nikelevyh splavov v vakuumnoj indukcionnoj pechi [Refinement of unconditioned waste of deformable nickel alloys in the vacuum induction furnace] // Tehnologiya metallov. 2015. №4. S. 8–13.
  15. Min P.G., Goryunov A.V., Vadeev V.E. Sovremennye zharoprochnye nikelevye splavy i effektivnye resursosberegayushhie tehnologii ih izgotovleniya [Modern heat resisting nickel alloys and effective resource-saving technologies of their manufacturing] // Tehnologiya metallov. 2014. №8. S. 12–23.
  16. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resursosberegayushhie tehnologii vyplavki perspektivnyh litejnyh i deformiruemyh superzharoprochnyh splavov s uchetom pererabotki vseh vidov othodov [Resource-saving smelting technologies of perspective cast and deformable superhot strength alloys taking into account processing of all types of waste] // Elektrometallurgiya. 2016. №9. S. 30–41.
  17. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resource-Saving Technologies of Making Advanced Cast and Deformable Superalloys with Allowance for Processing All Types of Wastes // Russian Metallurgy (Metally). 2016. Vol. 2016. No. 12. P. 1187–1195.
  18. Ospennikova O.G., Min P.G., Vadeev V.E., Kalitsev V.A., Kramer V.V. Resursosberegayushhaya tehnologiya pererabotki nekondicionnyh othodov deformiruemogo splava VZh175 dlya diskov GTD [Resource-saving processing technology of off-grade scrap of wrought superalloy VG175 for GTE disks production] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №2. St. 01. Available at: http://www.viam-works.ru (accessed: June 19, 2017). DOI: 10.18577/2307-6046-2016-0-2-1-1.
  19. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniyu lityh prutkovyh (shihtovyh) zagotovok [The experience of GS32-VI alloy scrap recycling at the VIAM scientific and production complex for cast bars production] // Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  20. Min P.G., Sidorov V.V., Kablov D.E., Vadeev V.E. Rafinirovanie monokristallicheskih zharoprochnyh nikelevyh splavov ot primesej sery i kremniya i nejtralizaciya vrednogo vliyaniya fosfora [Refining of single-crystal superalloys to remove a sulfur and silicon impurity and eliminating unfavorable effect of phosphorus] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4. St. 04. Available at: http://www.viam-works.ru (accessed: June 19, 2017). DOI: 10.18577/2307-6046-2017- 0-4-4-4.
  21. Sidorov V.V., Min P.G., Burcev V.T., Kablov D.E., Vadeev V.E. Komp'yuternoe modelirovanie i eksperimental'noe issledovanie reakcij rafinirovaniya v vakuume slozhnolegirovannyh renijsoderzhashhih nikelevyh rasplavov ot primesej sery i kremniya [Computer modeling and pilot study of reactions of refinement in vacuum complex-alloyed rhenium containing nickel melt from sulfur and silicon impurity] // Vestnik RFFI. 2015. №1 (85). S. 32–36.
  22. Min P.G., Sidorov V.V. Rafinirovanie othodov zharoprochnogo nikelevogo splava ZhS32-VI ot primesi kremniya v usloviyah vakuumnoj indukcionnoj plavki [Refining of scraps of Ni-base superalloy ZhS32-VI to eliminate silicon impurity under conditions of vacuum induction melting] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №9. St. 01. Available at: http://viam-works.ru (accessed: June 19, 2017). DOI: 10.18577/2307-6046-2014-0-9-1-1.
  23. Min P.G., Sidorov V.V., Kablov D.E., Vadeev V.E. Issledovanie sery i fosfora v litejnyh zharoprochnyh nikelevyh splavah i razrabotka effektivnyh sposobov ih rafinirovaniya [Sulfur and phosphorus research in cast heat resisting nickel alloys and development of effective ways of their refinement] // Tehnologiya metallov. 2015. №12. S. 2–9.
  24. Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I. Issledovanie processov rafinirovaniya v vakuume slozhnolegirovannyh nikelevyh rasplavov ot primesi sery [Research of refining processes in vacuum complex-alloyed nickel melt from sulfur impurity] // Metally. 2015. №6. S. 37–43.
  25. Sidorov V.V., Min P.G. Rafinirovanie slozhnolegirovannogo nikelevogo rasplava ot primesi sery pri plavke v vakuumnoj indukcionnoj pechi (chast 2) [Refinement complex-alloyed nickel melt from sulfur impurity when melting in the vacuum induction furnace (part 2)] // Elektrometallurgiya. 2014. №5. S. 26–30.
  26. Sidorov V.V., Min P.G., Folomejkin Yu.I., Vadeev V.E. Vliyanie skorosti filtracii slozhnolegirovannogo nikelevogo rasplava cherez penokeramicheskij filtr na soderzhanie primesi sery v metalle [Influence of speed of filtering complex-alloyed nickel rasplava via the foam ceramics filter on the content of impurity of sulfur in metal] // Elektrometallurgiya. 2015. №5. S. 12–15.
  27. Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A. Vliyanie lantana na kachestvo i ekspluatacionnye svojstva monokristallicheskogo zharoprochnogo nikelevogo splava ZhS36-VI [The lanthanum influence on quality and operational properties of single crystal nickel base ZhS36-VI superalloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 02. Available at: http://www.viam-works.ru (accessed: June 19, 2017). DOI: 10.18577/2307-6046-2015-0-12-2-2.
  28. Sidorov V.V., Min P.G., Kablov D.E. Desulfuraciya monokristallicheskih zharoprochnyh nikelevyh splavov pri plavke v vakuume [Desulphuration of single-crystal heat resisting nickel alloys when melting in vacuum] // Metallurg. 2017. №5. S. 57–62.
  29. Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A. Vliyanie poverhnostno-aktivnyh primesej i dobavki lantana na strukturu i svojstva monokristallicheskogo zharoprochnogo nikelevogo splava ZhS36 [Influence of surface-active impurities and lanthanum on structure and properties of singlecrystal nickel superalloy ZhS36] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4. St. 02. Available at: http://www.viam-works.ru (accessed: June 19, 2017). DOI: 10.18577/2307-6046-2017-0-4-2-2.
  30. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  31. Pfann V. Zonnaya plavka. 2-e izd., pererab. i dop. [Zone melting. 2nd ed., rev. and add.]. M.: Mir, 1970. 336 s.
  32. Mehanik E.A., Min P.G., Gundobin N.V., Rastegaeva G.Yu. Opredelenie massovoj doli sery v zharoprochnyh nikelevyh splavah i stalyah v diapazone koncentracij ot 0,0001 do 0,0009% (po masse) [Determination of sulfur mass fraction in heat-resistant nickel alloy and steels within the concentration range from 0,0001 to 0,0009% wt.] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №9. St. 12. Available at: http://viam-works.ru (accessed: June 19, 2017). DOI: 10.18577/2307-6046-2014-0-9-12-12.
  33. Yakimovich P.V., Alekseev A.V., Min P.G. Opredelenie nizkih soderzhanij fosfora v zharoprochnyh nikelevyh splavah metodom ISP-MS [Determination of low phosphorus content in heat-resistant nickel alloys by ICP-MS method] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №10. St. 02. Available at: http://viam-works.ru (accessed: June 19, 2017). DOI: 10.18577/2307-6046-2014-0-10-2-2.
  34. Jakubowski N., Prohaska T., Rottmann L., Vanhaecke F. Inductively coupled plasma- and glow discharge plasma-sector field mass spectrometry // J. Anal. At. Spectrom. 2011. Vol. 26. P. 693–726.