Study of the light transmission of sulfamino acid electrolyte nickel plating with additives of various nanosized particles and evaluation of the properties deposited in them of cluster nickel coatings

Semenychev V.V., Smirnova T.B., Panarin A.V.
Semenychev V.V., Smirnova T.B., Panarin A.V. Study of the light transmission of sulfamino acid electrolyte nickel plating with additives of various nanosized particles and evaluation of the properties deposited in them of cluster nickel coatings // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-11-11. URL: https://www.viam-works.ru/en/journal/2017/8/11
Keywords
nanosize particles, light transmission, galvanic nickel plating, coating properties, sclerometry.
Abstract

Using a photometer KFK-3-01-«ZOMZ», the light transmission of sulfamino acid electrolyte of nickel plating containing nanosized particles of various manufacturers was investigated. In the initial and each electrolyte with nanoparticles, nickel coatings were deposited on samples from steel 30ХГСА. The effect of the presence of nanoparticles in the electrolyte was evaluated by measuring the porosity of the deposited coating, its thickness and microhardness, as well as by studying the geometry of the grooves formed by the diamond indentor under various loads.

Reference list
  1. Istoriya aviacionnogo materialovedeniya. VIAM-80 let: gody i lyudi / pod obsh. red. E.N. Kablova [History of aviation materials science. VIAM-80 years: years and people / gen. ed. by E.N. Kablov]. M. VIAM, 2012. S. 520.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Semenychev V.V. Korrozionnaya stojkost obrazcov splava 1201 v morskih subtropikah [Corrosion resistance of samples of alloy 1201 in sea subtropics] // Korroziya: materialy, zashhita. 2015. №3. S. 1–5.
  4. Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn. 2012. №3. S. 16–21.
  5. Semenychev V.V., Salahova R.K., Tyurikov E.V., Ilin V.A. Zashhitnye i funkcionalnye galvanicheskie pokrytiya, poluchaemye s primeneniem nanorazmernyh chastic [The protective and functional galvanic coverings received using nanodimensional particles] // Aviacionnye materialy i tehnologii. 2012. №S. S. 335–342.
  6. Tyurikov E.V., Ilin V.A. Semenychev V.V. O roli nanorazmernyh chastic oksida alyuminiya v samoreguliruyushhemsya elektrolite hromirovaniya [About role of nanodimensional particles of aluminum oxide in self-regulating electrolit of chromizing] // Izvestiya Samarskogo nauchnogo centra RAN. T. 14. №4 (3). 2012. S. 208–807.
  7. Nagaeva L.V. Primenenie nanoporoshkov v elektrolitah nikelirovaniya kak sposob polucheniya nikelevyh pokrytij, po svojstvam ne ustupayushhim hromovym pokrytiyam [Application of nanopowders in nickel plating electrolits, as way of receiving nickel coverings, on the properties which are not conceding to chrome platings] // Korroziya: materialy, zashhita. 2007. №9. S. 32–36.
  8. Elektrolit nikelirovaniya: pat. 2293803 Ros. Federaciya. №2005124342/02 [Nickel plating electrolit: pat. 2293803 Rus. Federation. No. 2005124342/02]; zayavl. 01.08.05; opubl. 20.02.07, Byul. №5.
  9. Semenychev V.V., Nagaev V.V. Galvanicheskie pokrytiya na osnove cinka, poluchennye iz elektrolitov, soderzhashhih soli nikelya ili kobalta i nanoporoshki oksidov i karbidov [Galvanic coverings on the basis of the zinc, received from the electrolits containing salts of nickel or cobalt and nanopowders of oxides and carbides] // Izvestiya Samarskogo nauchnogo centra RAN. 2008. T. 1. Spec. vyp. S. 29–32.
  10. Elektrolit cinkovaniya: pat.№2301289 Ros. Federaciya. №2005139708/02 [Electrolyte of zinc-plating: pat. 2301289 Rus. Federation. No. 2005139708/02]; zayavl. 20.12.05; opubl. 20.06.07, Byul. №17.
  11. Koshelev V.N., Semenychev V.V., Panarin A.V. Ekologicheski bezopasnyj tehnologicheskij process naneseniya zashhitnyh piroliticheskih alyuminievyh pokrytij bez navodorozhivaniya stalnoj podlozhki [Ecologically safe technological process of drawing protective pyrolitic aluminum coverings without hydrogen saturation of steel substrate] // Izvestiya Samarskogo nauchnogo centra RAN. 2008. T. 1. Spec. vyp. S. 18–23.
  12. Panarin A.V. Piroliticheskie karbidohromovye pokrytiya. Tehnologiya polucheniya i svojstva [Pyrolitic carbide chrome platings. Technology of receiving and property] // Aviacionnye materialy i tehnologii. 2011. №4. S. 14–18.
  13. Panarin A.V., Semenychev V.V., Salahova R.K. Svojstva titanovyh i alyuminievyh splavov s piroliticheskim karbidohromovym pokrytiem [Properties of titanium and aluminum alloys with pyrolitic carbide chrome plating] // Tehnologiya legkih splavov. 2015. №3. S. 131–137.
  14. Semenychev V.V. Korrozionnaya stojkost listov splava D16ch.-T v morskih subtropikah [Corrosion resistance of alloy D16ch.-T sheets in marine subtropics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 11. Available at: http://www.viam-works.ru (accessed: July 18, 2017). DOI: 10.18577/2307-6046-2014-0-7-11-11.
  15. Semenychev V.V. Degradaciya prochnostnyh i ustalostnyh harakteristik splavov sistemy Al–Cu–Mg posle dlitelnyh korrozionnyh ispytanij v morskih subtropikah [Degradation of strength and fatigue characteristics of alloys of Al–Cu–Mg system after long corrosion tests in sea subtropics] // Tehnologiya legkih splavov. 2015. №1. S. 62–69.
  16. Zhirnov A.D., Semenychev V.V., Holshev S.I. Ispytanie aviacionnyh materialov v usloviyah morskogo subtropicheskogo klimata: metodicheskoe rukovodstvo [Testing of aviation materials in the conditions of sea subtropical climate: methodical management]. M.: VIAM, 1987. 48 s.
  17. Salahova R.K., Semenychev V.V., Tyurikov E.V., Tihoobrazov A.B. Issledovanie vnutrennih (ostatochnyh) napryazhenij v kompozicionno-klasternyh hromovyh i nikelevyh pokrytiyah [Investigation of internal (residual) stresses in composite-cluster chrome and nickel coatings] // Aviacionnye materialy i tehnologii. 2014. № S3. S. 42–46. DOI: 10.18577/2071-9140-2014-0-s3-42-46.
  18. Vulf B.K., Romadin K.P. Aviacionnoe materialovedenie [Aviation materials science]. M.: Mashinostroenie, 1967. 392 s.
  19. Kostrzhickij A.I., Karpov V.F., Kabanchenko M.P. i dr. Spravochnik operatora ustanovok po naneseniyu pokrytij v vakuume [The directory of the operator of installations on drawing coverings in vacuum. M.: Mashinostroenie, 1991. 125 s.
  20. Semenychev V.V., Smirnova T.B. O vozmozhnosti ocenki poristosti pokrytij potenciostaticheskimi metodami [About possibility of assessment of porosity of coverings potential static methods] // Aviacionnye materialy i tehnologii. 2009. №2. S. 7–10.
  21. Semenychev V.V., Smirnova T.B. Ocenka poristosti karbidohromovyh pokrytij na razlichnyh klassah konstrukcionnyh materialov putem izmereniya stacionarnyh potencialov sistemy [Evaluation of porosity of chromecarbide coatings on different classes of structural materials using measurement of systems stationary potential] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4. St. 07. Available at: http://www.viam-works.ru (accessed: July 18, 2017). DOI: 10.18577/2307-6046-2016-0-4-7-7.
  22. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  23. Semenychev V.V., Salahova R.K. Sklerometriya kak metod ocenki intensivnosti mezhkristallitnoj korrozii [Sclerometry as method of assessment of intensity of between crystallite corrosion] // Korroziya: materialy, zashhita. 2015. №12. S. 37–41.