Evaluation of effect of duration and storage condition on the properties of prepreg and PCM based on it

Veshkin E.A, Satdinov R.A., Postnov V.I., Strelnikov S.V.
Veshkin E.A, Satdinov R.A., Postnov V.I., Strelnikov S.V. Evaluation of effect of duration and storage condition on the properties of prepreg and PCM based on it // Proceedings of VIAM. 2017. No. 8. DOI: 10.18577/2307-6046-2017-0-8-10-10. URL: https://www.viam-works.ru/en/journal/2017/8/10
Keywords
prepreg, technological properties, fiberglass, binder, storage time, PCM, method.
Abstract

The effect of time and storage conditions of the prepreg, based on the phenol-formaldehyde binder VSF-16M and T-64 glass fiber cloth (VMP), on its technological properties was evaluated. Elastic-strength properties of GRP based on this prepreg are investigated. To assess the prepreg of fiberglass, the differential scanning calorimetry (DSC) method was used and the gel time of the binder in it was analyzed. Based on the results of the study, conclusions were drawn as to the shelf life of the prepreg.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  5. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: April 17, 2017). DOI: 10.18577/2307-6046-2014-0-4-6-6.
  6. Veshkin E.A. Osobennosti bezavtoklavnogo formovaniya nizkoporistykh PKM [Features of out-of-autoclave forming of poor-porous PCM] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2016. №2 (38). St. 07. Available at: http://www.viam-works.ru (accessed: April 20, 2017). DOI 10.1857/2307-6046-2016-0-2-7-7
  7. Veshkin E.A., Postnov V.I., Zastrogina O.B., Satdinov R.A Tehnologiya uskorennogo formovaniya trehslojnyh panelej interera samoleta [Technology of the accelerated formation of three-layered panels of interior of airplane] // Izvestiya Samarskogo nauchnogo centra RAN. 2013. T. 15. №4 (4). S. 799–805.
  8. Minakov V.T., Postnov V.I., Shvec N.I., Zastrogina O.B., Petuhov V.I., Makrushin K.V. Osobennosti izgotovleniya trehslojnyh sotovyh panelej s polimernym zapolnitelem goryachego otverzhdeniya [Features of manufacturing of three-layered cellular panels with polymeric filler of hot curing] // Aviacionnye materialy i tehnologii. 2009. №3. S. 6–19.
  9. Veshkin E.A., Postnov V.I., Strelnikov S.V., Abramov P.A., Satdinov R.A. Opyt primeneniya tehnologicheskogo kontrolya polufabrikatov PKM [Experience of application of technological control of semi-finished products of PCM] // Izvestiya Samarskogo nauchnogo centra RAN. 2014. T. 16. №6 (2). S. 393–398.
  10. Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Fenolformaldegidnye svjazuyushhie novogo pokoleniya dlya materialov interera [Phenolformaldehyde binding new generation for interior materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 265–272.
  11. Satdinov R.A., Istyagin S.E., Veshkin E.A. Analiz temperaturno-vremennyh parametrov rezhimov otverzhdeniya PKM s zadannymi harakteristikami [Analysis of the temperature-time parameters mode curing PCM with specified characteristics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №3. St. 09. Available at: http://www.viam-works.ru (accessed: April 19, 2017). DOI: 10.18577/2307-6046-2017-0-3-9-9.
  12. Bobovich B.B. Polimernye konstrukcionnye materialy (struktura, svojstva, primenenie) [Polymeric constructional materials (structure, properties, application)]. M.: FORUM INFRA-M, 2014. 400 s.
  13. Davydova I.F., Kavun N.S. Stekloplastiki ‒ mnogofunkcionalnye kompozicionnye materialy [Fibreglasses ‒ multipurpose composite materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 253–260.
  14. Satdinov R.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. Vozduhovody nizkogo davleniya iz PKM v letatelnyh apparatah [РСМ low-pressure air ducts in aircraft] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8. St. 08. Available at: http://www.viam-works.ru (accessed: April 22, 2017). DOI: 10.18577/2307-6046-2016-0-8-8-8.
  15. Nikitin K.E., Burhan O.L., Postnov V.I., Petuhov V.I. Laboratornaya ustanovka dlya issledovaniya i otrabotki processov formovaniya IPF-2003 polimernyh kompozicionnyh materialov ultrazvukovym metodom [Laboratory installation for research and working off of processes of formation IPF-2003 of polymeric composite materials by ultrasonic method] // Zavodskaya laboratoriya. Diagnostika materialov. 2008. №4. S. 38–41.
  16. Postnov V.I., Burhan O.L., Rahmatullin A.E., Kachura S.M. Nerazrushayushhie metody kontrolya soderzhaniya svyazuyushhih v prepregah i PKM (obzor) [Nondestructive control methods of the content of binders in prepregs and PCM (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №12. St. 06 Available at: http://www.viam-works.ru (accessed: April 22, 2017).
  17. Veshkin E.A., Abramov P.A., Postnov V.I., Strelnikov S.V. Vliyanie tehnologii podgotovki preprega na svojstva PKM [Influence of technology of preparation of prepreg on PCM properties] // Vse materialy. Enciklopedicheskij spravochnik. 2013. №9. S. 8–14.
  18. Satdinov R.A., Veshkin E.A., Postnov V.I., Abramov P.A. Rol antiadgezionnyh pokrytij v tehnologicheskom processe formovaniya PKM [The role of anti-adhesive coatings in the technological process of PCM molding] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4 (40). St. 10. Available at: http://www.viam-works.ru (accessed: March 20, 2017). DOI: 10.18577/2307-6046-2016-0-4-10-10.