Superalloy VJ175 structural and phase stability assessment after heat treatment and exposure at working temperature

Bakradze M.M., Lomberg B.S., Filonova E.V., Chabina E.B.
Bakradze M.M., Lomberg B.S., Filonova E.V., Chabina E.B. Superalloy VJ175 structural and phase stability assessment after heat treatment and exposure at working temperature // Proceedings of VIAM. 2017. No. 7. DOI: 10.18577/2307-6046-2017-0-7-5-5. URL: https://www.viam-works.ru/en/journal/2017/7/5
Keywords
Ni-base superalloy, anneal, isothermal forging, heat treatment, mechanical properties.
Abstract

The changes of microstructure and phase composition of disks for gas turbine engines made of superalloy VJ175 after heat treatment and imitation of operating at working temperature (long-term exposure at maximal operating temperature 750°С) are investigated. Mechanical properties are defined, fractography investigations are carried out in initial (heat treated) condition and after long-term for 1000 and 2000 hours heating up to operating temperature.

Reference list
  1. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] // Problemy chernoj metallurgii i materialovedeniya. 2013. №3. S. 47–54
  2. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. 2-e izd. [Tendencies and reference points of innovative development of Russia: collection of scientific information materials]. M.: VIAM, 2013. 544 s.
  3. Kablov E.N., Ospennikova O.G., Lomberg B.S. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  4. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 20–26.
  5. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  6. Locq D., Caron (Onera) P. On Some Advanced Nickel-Based Superalloys for Disk Applications // High Temperature Materials AL03-01. 2011. Issue 3. P. 1–9.
  7. Gabb T.P., Gayda J., Telesman J. Thermal and Mechanical Property Characterization of the Advanced Disk Alloy // NASA / TM–2005-213645. June, 2005.
  8. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovaniya i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej no-vogo pokolenija [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] // Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
  9. Filonova E.V., Bakradze M.M., Kochubey A.Ya., Vavilin N.L. Issledovanie izmenenij strukturno-fazovogo sostoyaniya splava VZh175 v processe goryachej deformacii i termicheskoj obrabotki [Structural-phase evolution of VZH175-alloy during hot deformation and heat treatment] // Aviacionnye materialy i tehnologii. 2014. №3. S. 10–13. DOI: 10.18577/2071-9140-2014-0-3-10-13.
  10. Chabina E.B., Lomberg B.S., Filonova E.V., Ovsepyan S.V., Bakradze M.M. [Change of structural and phase condition of heat resisting deformable nickel alloy at alloying tantalum and rhenium] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 03. Available at: http://www.viam-works.ru (accessed: February 01, 2017). DOI: 10.18577/2307-6046-2015-0-9-3-3.
  11. Sharpe H.J., Saxena A. Effect of Microstructure on High-Temperature Mechanical Behavior of Nickel-Base Superalloys for Turbine Disc Applications // EuroSuperalloys 2010: Advanced Materials Research. 2011. Vol. 278. P. 259–264. URL: http://www.scientific.net (дата обращения: 02.02.2017).
  12. Gabb T.P., Gayda J., Kantzos P. The Grain Size-Temperature Response of Advanced Nickel-Base Disk Superalloys During Solution Heat Treatments // NASA / TM–2007-214912. December, 2007.
  13. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Proizvodstvo diskov GTD iz zharoprochnyh splavov na izotermicheskih pressah // Aviacionnye materialy i tehnologii. 2013. №1.
  14. S. 13–16.
  15. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  16. Orlov M.R., Ospennikova O.G., Avtaev V.V., Terehin A.M., Filonova E.V. Fraktograficheskij analiz ekspluatacionnogo razrusheniya diska rotora vysokogo davleniya aviacionnogo gazoturbinnogo dvigatelya iz zharoprochnogo splava EP741-NP [Fractography analysis of operational distructure of the gas-turbine engine high pressure rotor disk made of EP741-NP superalloy] // Aviacionnye materialy i tehnologii. 2015. №S1. S. 5–12. DOI: 10.18577/2071-9140-2015-0-S1-5-12.
  17. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and X-ray of the structural analysis for research of structural and phase condition of materials] // TestMat-2013: sb. dokl. Vseros. konf. po ispytaniyam i issledovaniyam svojstv materialov. M., 2013. S. 32.