Creation of the mathematical model and calculation of sample temperatures at tests on fire resistance

Barbotko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N.
Barbotko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N. Creation of the mathematical model and calculation of sample temperatures at tests on fire resistance // Proceedings of VIAM. 2017. No. 7. DOI: 10.18577/2307-6046-2017-0-7-12-12. URL: https://www.viam-works.ru/en/journal/2017/7/12
Keywords
fire resistance, fireproof, fire safety, mathematical model, fire tests, aviation technique.
Abstract

One of the major characteristics in ensuring fire safety of aviation engineering are fire resistance and fireproof of materials and constructive elements on their basis. Fire resistance characteristics, except the thermal stability of material of fireproof partition are defined also by the size of transmitted heat flux and temperature of not warmed surface. On these characteristics are influence as properties of the tested material, and condition of carrying out testing, therefore development of mathematical model allowing to evaluate influence of different factors on normed characteristics is required. The mathematical model describing heat transfer from flame on monolithic wall and from wall in surrounding space is constructed. Calculation for influence the different factors of material and environmental conditions on specimen fireproof partition temperature are executed.

Reference list
  1. Normy letnoj godnosti samoletov transportnoj kategorii: AP-25 [Standards of the flight validity of airplanes of transport category]; 5-e izd., s popravkami 1–8: utv. Postanovleniem 28-j sessii Soveta po aviacii i ispolzovaniyu vozdushnogo prostranstva 11.12.2008. M.: Aviaizdat, 2015. 290 s.
  2. Normy letnoj godnosti dvigatelej vozdushnyh sudov: AP-33 [Standards of the flight validity of engines of air vehicles]; 3-e izd., s popravkami 33-1 i 33-2: utv. Postanovleniem 32-j sessii Soveta po aviacii i ispolzovaniyu vozdushnogo prostranstva 17.02.2012. M.: Aviaizdat, 2012. 86 s.
  3. Barbotko S.L. Trebovaniya aviacionnyh norm i metody ocenki pozharnoj bezopasnosti aviacionnyh materialov: istoriya, sovremennoe sostoyanie i perspektivy razvitiya [Requirements of aviation norms and methods of assessment of fire safety of aviation materials: history, current state and development perspectives] // Vestnik Voronezhskogo instituta GPS MChS Rossii, 2014. №3. S. 23–33.
  4. Barbotko S.L., Volnyj O.S., Kirienko O.A., Lucenko A.N., Shurkova E.N. 1) Sopostavlenie metodov ocenki pozharnoj opasnosti polimernyh materialov v razlichnyh otraslyah transporta i promyshlennosti [Comparison of methods of assessment of fire danger of polymeric materials in the different industries of transport and the industry] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №1. S. 2–9. 2) Sopostavlenie metodov ocenki pozharnoj opasnosti polimernyh materialov v razlichnyh otraslyah transporta i promyshlennosti [Comparison of methods of assessment of fire danger of polymeric materials in the different industries of transport and the industry] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №2. S. 2–9.
  5. Barbotko S.L. Pozharnaya opasnost, metody ocenki i trebovaniya k materialam dlya izgotovleniya vneshnego kontura aviacionnoj tehniki [Fire danger, assessment and requirement methods to materials for manufacturing of external circuit of aviation engineering] // Vestnik Voronezhskogo instituta GPS MChS Rossii, 2014. №4. S. 6–15.
  6. Barbotko S.L., Kirienko O.A., Volnyj O.S., Lucenko A.N. Analiz pozharnoj opasnosti motogondol aviacionnyh dvigatelej i drugih pozharoopasnyh zon; ispolzuemye metody ognevyh ispytanij materialov i konstruktivnyh elementov na sootvetstvie trebovaniyam aviacionnyh norm [Analysis of fire danger of motor-gondolas of aircraft engines and other fire hazardous zones; used methods of fire tests of materials and constructive elements on compliance to requirements of aviation norms] // Problemy bezopasnosti poletov, 2017. №5. S. 3–24.
  7. Powerplant Installation and Propulsion System Component Fire Protection Test Methods, Standards, and Criteria // Advisory Circular. 1990. No. 20-135. 18 p.
  8. Certification Specifications and Acceptable Means of Compliance for Large Aeroplanes: CS-25, Amendment 15 / EASA. July 21, 2014. 921 p.
  9. Standard Fire Apparatus and Procedure (For Flexible Hose Assemblies) // Powerplant Engineering Report No. 3A (revised) / U.S. Department of Transportation, Federal Aviation Administration, Flight Standard Service. Washington, 1978. 35 p.
  10. Aircraft Materials Fire Test Handbook / U.S. Department of Transportation, Federal Aviation Administration, William J. Hughes Technical Center. New Jersey, 2000. No. DOT/FAA/AR-00/12. URL: http://www.fire.tc.faa.gov/handbook.stm (Available at: June 06, 2017).
  11. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coalplastics and fibreglasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://www.viam-works.ru (accessed: May, 18 2017).
  12. Beider E.Ya., Petrova G.N., Izotova T.F., Barbotko S.L. Stekloplastiki na termoplastichnoj matrice [Glass reinforced plastics on the basis of thermoplastic matrix] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №7. St. 03. Available at: http://www.viam-works.ru (accessed: May, 18 2017).
  13. Veshkin E.A. Osobennosti bezavtoklavnogo formovaniya nizkoporistykh PKM [Features of out-of-autoclave forming of poor-porous PCM] // Trudy VIAM elektron. nauch.-tekhnich. zhurn. 2016. №2. St. 07. Available at: http://www.viam-works.ru (accessed: May, 18 2017). DOI 10.1857/2307-6046-2016-0-2-7-7
  14. Veshkin E.A., Postnov V.I., Abramov P.A. Puti povysheniya kachestva detalej iz PKM pri vakuumnom formovanii [Ways of improvement of quality of details from PCM at vacuum formation] // Izvestiya Samarskogo nauchnogo centra Rossijskoj akademii nauk. T. 14. №4 (3). 2012. S. 834–839.
  15. Lukina N.F., Dementeva L.A., Kutsevich K.E. Kleevye prepregi na osnove tkanej Porcher – perspektivnye materialy dlya detalej i agregatov iz PKM [Adhesive prepregs based on tissue Porsher – perspective materials for parts and units out of polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №6. St. 10. Available at: http://www.viam-works.ru (accessed: May, 18 2017). DOI: 10.18577/2307-6046-2014-0-6-10-10.
  16. Kurnosov A.O., Melnikov D.A., Sokolov I.I. Structural glass-reinforced plastics purposed for aviation industry // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 08. Available at: http://viam-works.ru (accessed: May, 18 2017). DOI: 10.18577/2307-6046-2015-0-8-8-8.
  17. Shurkova E.N., Volnyj O.S., Lucenko A.N., Barbotko S.L. Sravnitelnaya ocenka pozharobezopasnosti PKM dlya izgotovleniya konstruktivnyh elementov letatelnyh apparatov [Comparative assessment of fire safety of PCM for manufacturing of constructive elements of flight vehicles] // Pozharovzryvobezopasnost. 2014. №2. C. 20–27.
  18. Shurkova E.N., Barbotko S.L., Dementeva L.A., Serezhenkov A.A. Sopostavlenie pozharobezopasnosti PKM na osnove kleevyh prepregov, ispolzuemyh dlya izgotovleniya konstrukcij vneshnego kontura aviacionnoj tehniki [Comparison of fire safety of PCM on the basis of the glue prepregs used for manufacturing of designs of external circuit of aviation engineering] // Klei. Germetiki. Tehnologii. 2013. №8. C. 13–17.
  19. Barbotko S.L., Shurkova E.N. O pozharnoj bezopasnosti materialov, ispolzuemyh dlya izgotovleniya vneshnego kontura samoletov [About fire safety of the materials used for manufacturing of external circuit of airplanes] // Pozharovzryvobezopasnost. 2011. T. 20. №10. C. 19–24.
  20. Barbotko S.L., Shurkova E.N., Volny O.S., Skrylyov N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlya vneshnego kontura aviacionnoj tehniki [Evolution of polymer composite fire-safety for the outer contour of aeronautical engineering] // Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
  21. Mishurov K.S., Mishkin S.I. Vliyanie vneshnej sredy na svojstva ugleplastika VKU-39 [Environmental effect on properties of CFRP (Carbon Fiber Reinforced Plastic) VKU-39] // Trudy VIAM: elektron.-nauch. tehnich. zhurn. 2016. №12 (48). St. 08. Available at: http://www.viam-works.ru (accessed: May, 18 2017). DOI: 10.18577/2307-6046-2016-0-12-8-8.
  22. Shurkova E.N., Volny O.S., Izotova T.F., Barbotko S.L. Issledovanie vozmozhnosti snizheniya teplovydeleniya pri gorenii kompozicionnogo materiala putem izmeneniya ego struktury [Research of possibility of decrease in heat release when burning composite material by change of its structure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 27–30.
  23. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  24. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  25. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  26. Pavlov K.F., Romankov P.G., Noskov A.A. Primery i zadachi po kursu processov i apparatov himicheskoj tehnologii: ucheb. posobie dlya vuzov, 9-e izd. / pod red. P.G. Romankova [Examples and tasks of course of processes and devices of chemical technology: the manual for higher education institutions, the 9th ed. / ed. P.G. Romankov]. L.: Himiya, 1981. 560 s.
  27. Krasnoshhekov E.A., Sukomel A.S. Zadachnik po teploperedache. 3-e izd. [The book of problems on heat transfer. 3rd ed.]. M.: Energiya, 1975. 280 s.
  28. Dubrovkin N.F., Malanicheva V.G., Massur Yu.P., Fedorov E.P. Fiziko-himicheskie i ekspluatacionnye svojstva reaktivnyh topliv: spravochnik [Physical and chemical and operational properties of reactive fuels: directory]. M.: Himiya, 1985. S. 145–149.
  29. Balajka B., Sikora K. Processy teploobmena v apparatah himicheskoj promyshlennosti / perevod G.M. Goldenberga; pod red. V.A. Grigoreva [Heat exchanging processes in offices of the chemical industry / trans. by G. M. Goldenberg; ed. V.A. Grigoriev]. M.: Mashgiz, 1962. S. 141–153.
  30. Miheev M.A., Miheeva I.M. Osnovy teploperedachi [Heat transfer bases]. M.: Energiya, 1977. 344 s.