Method of large-sized deformed turbine discs manufacturing from EK151-ID industrial ingots with limited diameter (320 mm)

Bakradze M.M., Lomberg B.S., Sidorov S.A., Bubnov M.V.
Bakradze M.M., Lomberg B.S., Sidorov S.A., Bubnov M.V. Method of large-sized deformed turbine discs manufacturing from EK151-ID industrial ingots with limited diameter (320 mm) // Proceedings of VIAM. 2017. No. 6. DOI: 10.18577/2307-6046-2017-0-6-2-2. URL: https://www.viam-works.ru/en/journal/2017/6/2
Keywords
gas turbine engines discs, technological process, superalloys, forging, deformation, properties, structure.
Abstract

The article presents results of large-sized deformed turbine discs from nickel-based superalloy EK151-ID manufacturing technology development. The developed process provides the manufacturing possibility of large-sized forged discs from nickel-based superalloy with regulated structure and properties using industrial ingots with limited diameter (320 mm). Metal forming simulation engineering software QForm-3D was used in this work.

Reference list
  1. Sklyarov N.M. Put dlinoyu v 70 let – ot drevesiny do supermaterialov / pod obshh. red. E.N. Kablova [Way of 70 years – from wood to supermaterials / gen. ed. by E.N. Kablov]. M.: MISIS–VIAM, 2002. S. 317–319.
  2. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova[History of aviation materials science. VIAM is 80: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. S. 245–248.
  3. Kablov E.N., Golubovskij E.R. Zharoprochnost nikelevyh splavov: ucheb. posobie [Thermal stability of nickel alloys: manual]. M.: Mashinostroenie, 1998. 464 s.
  4. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Shtampovka diskov GTD iz zharoprochnykh splavov na izotermicheskikh pressakh [Punching of disks GTD from hot strength alloys on isothermal presses] // Aviacionnye materialy i tekhnologii. 2013. №1. S. 13–16.
  5. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  6. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvyaz struktury i svojstv vysokozharoprochnykh nikelevykh splavov dlya diskov gazoturbinnykh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] // Aviacionnye materialy i tekhnologii. 2011. №2. S. 25–30.
  7. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  8. Lomberg B.S., Gorin V.A., Gerasimov D.E., Rahmanov N.S., Stepanov V.P. Vysokozharoprochnye deformiruemye nikelevye splavy dlya diskov GTD i tehnologiya ih proizvodstva [High-heat resisting deformable nickel alloys for disks GTE and technology of their production] // Tehnologiya legkih splavov, 1993. №7–8. S. 54–63.
  9. Razuvaev E.I., Bubnov M.V., Bakradze M.M., Sidorov S.A. GIP i deformatsiia granulirovannykh zharoprochnykh nikelevykh splavov [HIP and deformation of the granulated heat resisting nickel alloys] // Aviatsionnye materialy i tekhnologii. 2016. №S1. S. 80–86. DOI: 10.18577/2071-9140-2016-0-S1-80-86
  10. Ponomarenko D.A., Skugorev A.V., Sidorov S.A., Strokov V.V. Tehnologicheskie vozmozhnosti specializirovannyh izotermicheskih pressov siloj 6,3 i 16 MN v proizvodstve detalej aviacionno-kosmicheskogo naznacheniya [Technological capabilities specialized isothermal presses with a force of 6,3 and 16 MN in production of details of aerospace assignment] // Kuznechno-shtampovochnoe proizvodstvo. Obrabotka metallov davleniem. 2015. №9. S. 36–41.
  11. Razuvaev E.I., Bubnov M.V., Grigoreva G.A., Sidorov S.A. Razvitie i prakticheskoe primenenie fiziko-himicheskoj teorii v processah obrabotki davleniem aviacionnyh stalej i splavov [Development and practical application of physico-chemical theory in of processing by pressure applied to aircraft steels and alloys] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 07. URL: http://www.materialsnews.ru (data obrashheniya: 23.02.2017).
  12. Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N. Vliyanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava EK151-ID [The influence of quenching on structure and properties nickel-based superalloy EK151-ID forgings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 01. Available at: http://www.viam-works.ru (accessed: February 13, 2017).
  13. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  14. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Sovremennye tehnologii obrabotki metallov davleniem [Modern technologies of plastic working of metals] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 03. Available at: http://www.viam-works.ru (accessed: February 23, 2017). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  15. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.