Analysis of nickel alloys by ICP-MS with laser ablation

Alekseev A.V., Yakimovitch P.V., Leykin A.Yu.
Alekseev A.V., Yakimovitch P.V., Leykin A.Yu. Analysis of nickel alloys by ICP-MS with laser ablation // Proceedings of VIAM. 2017. No. 5. DOI: 10.18577/2307-6046-2017-0-5-12-12. URL: https://www.viam-works.ru/en/journal/2017/5/12
Abstract

Currently nickel alloys are widely used in modern aviation industry and engine building. They are made of critical parts with thermal and power load. An important task is to control the chemical composition of nickel alloys, especially the content of trace. In this work determination of B, Si, P, Mn, Fe, Cu, As, Se, Sn, Sb, Pb and Bi in the certified standard samples of nickel alloys by a mass spectrometry method with inductively coupled plasma and laser ablation (ICP-MS-LA). The technique of preparation of test for the analysis is given. The results are compared with the results of the analysis of the classical method of ICP-MS. The detection limits are as follows: the range of detectable concentrations 0,00002–2,2% (by weight), relative standard deviation is less than 0,07.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTE from hot strength alloys with single-crystal and composition structure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  3. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlya lit'ya lopatok s napravlennoj i monokristallicheskoj strukturoj (Chast II) [Nickel hot strength alloys for molding of blades with the directed and single-crystal structure (Part II)] // Materialovedenie. 1997. №5. S. 14–16.
  4. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlya perspektivnyh aviacionnyh GTD [Cast heat resisting nickel alloys for perspective aviation GTD] // Tehnologiya legkih splavov. 2007. №2. S. 6–16.
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  6. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: April 03, 2017).
  7. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizatsii v resursosberegayushchej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 01. Available at: http://www.viam-works.ru (accessed: April 03, 2017).
  8. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  9. Pupyshev A.A., Surikov V.T. Mass-spektrometriya s induktivno svyazannoj plazmoj. Obrazovanie ionov [Mass-spectrometry with inductively connected plasma. Formation of ions]. Ekaterinburg: UrO RAN, 2006. 276 s.
  10. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS // Mikrochim. Acta. 2001. Vol. 137. P. 149–155.
  11. Pupyshev A.A., Epova E.N. Spektralnye pomehi poliatomnyh ionov v metode mass-spektrometrii s induktivno svyazannoj plazmoj [Spectral hindrances of polynuclear ions in mass-spectrometry method with inductively connected plasma] // Analitika i kontrol. 2001. T. 5. №4. S. 335–369.
  12. Lejkin A.Yu., Yakimovich P.V. Sistemy podavleniya spektralnyh interferencij v mass-spektrometrii s induktivno svyazannoj plazmoj [Systems of suppression of spectral interferences in mass-spectrometry with inductively connected plasma] // Zhurnal analiticheskoj himii. 2012. T. 67. №8. S. 752–762.
  13. Nie X., Liang Y. Determination of trace elements in high purity nickel by high resolution inductively coupled plasma mass spectrometry // J. Cent. South Univ. 2012. Vol. 19. P. 2416−2420.
  14. MI 1.2.052–2013. Metodika izmerenij massovoj doli primesej R, Mn, Fe, Cu, Zn, Ga, As, Se, Ag, Cd, Sn, Sb, Te, Tl, Pb, Bi v nikelevyh splavah metodom mass-spektrometrii s induktivno svyazannoj plazmoj [Measurement technique of mass fraction of impurity P, Mn, Fe, Cu, Zn, Ga, As, Se, Ag, CDs, Sn, Sb, Te, Tl, Pb, Bi in nickel alloys mass-spectrometry method with inductively connected plasma]. M.: VIAM, 2013.
  15. Chernonozhkin S.M., Saprykin A.I. Osobennosti lazernoj ablyacii stekla i stali i ih vliyanie na rezultaty LA-ISP-MS analiza [Features of laser ablation of glass and steel and their influence on results of LA-ISP-MS of the analysis] // Analitika i kontrol. 2011. T. 15. №4. S. 413–420
  16. Mochizuki T., Shimamura T., Sakashita A., Iwata H., Blair P. Laser ablation for direct elemental analysis of solid samples by inductively coupled plasma mass spectrometry // Analytical Sciences. 1998. Vol. 4. P. 403–409.
  17. Karasev A.V., Inoue R., Suito H. Quantitative analysis of total and insoluble elements and inclusion composition in metal by laser ablation ICP-MS method // ISIJ International. 2001. Vol. 41. P. 757–765.
  18. Latkoczy C., Muller Y., Schmutz P., Gunther D. Quantitative element mapping of Mg alloys by laser ablation ICP-MS and EPMA // Applied Surface Science. 2005. Vol. 252. P. 127–132.
  19. Izmer A.V., Zoriy M.V., Pickhardt C. et al. LA-ICP-MS studies of cross section of NiCrAlY-based coatings on high-temperature alloys // JAAS. 2005. Vol. 20. P. 918–923.