Reduction of non-metallic inclusions in the nitrogen-containing corrosion-resistant steels

Krylov S.А., Shcherbakov A.I., Makarov А.А., Tonysheva О.А.
Krylov S.А., Shcherbakov A.I., Makarov А.А., Tonysheva О.А. Reduction of non-metallic inclusions in the nitrogen-containing corrosion-resistant steels // Proceedings of VIAM. 2017. No. 5. DOI: 10.18577/2307-6046-2017-0-5-1-1. URL: https://www.viam-works.ru/en/journal/2017/5/1
Abstract

An important prerequisite for high-performance stainless steel VNS-65 (18Cr13Ni4Co4Si2NMo3) is a high purity non-metallic inclusions – oxides and sulfides, no more than 1 point in accordance with GOST 1778–70. The existing steel smelting technology VNS-65 outdoor furnace followed by electroslag remelting is not always provides the desired purity of the metal, resulting in a high-level properties of instability. To reduce the amount of nonmetallic inclusions is necessary to reduce to 2–3 times the oxygen content (less than 0,01%) and sulfur (less than 0,005%). The aim of the study is to develop a technology of steel smelting VNS-65, providing the reduction of non-metallic inclusions, improved stability properties through the use of new refining slag mixtures and technology microalloying rare earth metals, administered through the slag. The work within the framework of an integrated research area 8.2. «High-strength and corrosion-resistant welded structural steel with high fracture toug

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Tonysheva O.A., Voznesenskaya I.M., Eliseev E.A., Shalkevich A.B. Novaya vysokoprochnaya ekonomnolegirovannaya azotsoderzhashchaya stal povyshennoj nadezhnosti [The new high-strength containing steel of increased reliability economically alloyed nitrogen] // Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
  4. Tonysheva O.A., Voznesenskaya N.M. Perspektivnye vysokoprochnye korrozionnostojkie stali, legirovannye azotom (sravnitelnyj analiz) [Perspective high-strength corrosion-resistant steels alloyed with nitrogen (comparative analysis] // Aviacionnye materialy i tehnologii. 2014. №3. S. 27–32. DOI: 10.18577/2071-9140-2014-0-3-27-32.
  5. Voznesenskaya N.M., Kablov E.N., Petrakov A.F., Shalkevich A.B. Vysokoprochnye korrozionnostojkie stali austenitno-martensitnogo klassa [High-strength corrosion-resistant steel of the austenit-martensitic class] // Metallovedenie i termicheskaya obrabotka metallov. №7. 2002. S. 34–37.
  6. Tonysheva O.A., Voznesenskaja N.M., Shalkevich A.B., Petrakov A.F. Issledovanie vlijanija vysokotemperaturnoj termomehanicheskoj obrabotki na strukturu, tehnologicheskie, mehanicheskie i korrozionnye svojstva vysokoprochnoj korrozionnostojkoj stali pere-hodnogo klassa s povyshennym soderzhaniem azota [Research of influence of high-temperature thermomechanical processing on structure, technological, mechanical and corrosion properties of high-strength corrosion-resistant steel of transitional class with the raised content of nitrogen] // Aviacionnye materialy i tehnologii. 2012. №3. S. 31–36.
  7. Bratuhin A.G., Demchenko O.F., Dolzhenkov N.N., Krivonogov G.S. Vysokoprochnye korrozionnostojkie stali sovremennoj aviacii [High-strength corrosion-resistant became modern aircraft]. M.: MAI, 2006. S. 112–143.
  8. Krivonogov G.S., Kablov E.N. Granicy zeren i ih rol v ohrupchivanii vysokoprochnyh korrozionnostojkih stalej [Borders of grains and their role in fragility high-strength corrosion-resistant the steels] // Metally. 2002. №1. S. 35–45.
  9. Waudby P.E. Intern. // HetalsRev. Z3. 1976. No. 2. P. 74–98.
  10. Klyuev M.M., Kablukovskij A.F. Metallurgiya elektroshlakovogo pereplava [Metallurgy electroslag melting]. M.: Metallurgiya, 1969. 256 s.
  11. Litye lopatki gazoturbinnyh dvigatelej. Splavy, tehnologiya, pokrytiya / pod obshh. red. E.N. Kablova [Cast blades of gas turbine engines. Alloys, technology, coverings / gen. ed. by E.N. Kablov]. M.: Nauka, 2006. S. 119–135.
  12. Kulikov I.S. Raskislenie metallov [Deoxidation of metals]. M.: Metallurgiya, 1975. 504 s.
  13. Snitko Yu.P., Surovoj Yu.N., Lyakishev N.P. Osobennosti raskisleniya stali [Features of steel deoxidation] // Doklady AN SSSR. 1983. T. 268. №5. S. 115–117.
  14. Dub V.S., Levkov L.Ya., Shurygin D.A. i dr. Opyt proizvodstva polyh trubnyh zagotovok metodom elektroshlakovoj vyplavki [Experience of production of hollow pipe preparations by method of electroslag smelting] // Elektrometallurgiya. 2015. №1. S. 10–19.
  15. Levkov L.Ya. Povyshenie effektivnosti rafinirovaniya stali shlakom na osnove kontrolya ego okislennosti: dis. … kand. tehn. nauk [Increase of efficiency of refinement became slag on the basis of control its oxide: thesis, Cand. Sc. (Tech.)]. M, 1987. 159 s.
  16. Available at: http://www.steelcast.ru/rare_earth_elements_steel_deoxidation (accessed: April 25, 2015).
  17. Shurygin D.A., Levkov L.Ya., Dub V.S. i dr. Razrabotka sposobov kontrolya i upravlenie okislitelno-vosstanovitelnymi processami i kristallizaciej slitkov EShP [Development of ways of control and management of oxidation-reduction processes and crystallization of ingots of EShP] // Sovremennye problemy elektrometallurgii stali: mater. XV Mezhdunar. nauch. konf. Chelyabinsk, 2013. Ch. 2. S. 91–96.
  18. Averin V.V. Rastvorimost kisloroda, azota i aktivnost'elementov-raskislitelej v rasplavah na osnove zheleza, kobalta, nikelya i hroma: avtoref. diss. … dokt. tehn. nauk [Solubility of oxygen, nitrogen and activity of elements deoxidants in rasplavakh on the basis of iron, cobalt, nickel and chrome: thesis, Dr. Sc. (Tech.)]. M.: Imet AN SSSR, 1968. 32 s.