Features of foaming of polyimide pitches with reduced pressure

Sorokin A.E., Platonov M.M., Malyshenok S.V.
Sorokin A.E., Platonov M.M., Malyshenok S.V. Features of foaming of polyimide pitches with reduced pressure // Proceedings of VIAM. 2017. No. 4. DOI: 10.18577/2307-6046-2017-0-4-7-7. URL: https://www.viam-works.ru/en/journal/2017/4/7
Keywords
polymeric material, rigid polyimide foam, vacuum, foaming, compressive strength, heat resistance.
Abstract

The approach of the blowing polyimide resins and thereof compositions under reduced pressure is considered in the article. A comparison of the properties of foams obtained by foaming in air and under reduced pressure has been made. It was shown that the foaming under vacuum allows to obtain material possessing more stable strength properties and high thermal stability. A comparison of the properties of the material obtained from imported developments has been made. The technology of their production, properties and processing of different geometries products have been shown. The work was performed as part of the strategic direction number 16. «Ultra-light foam» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  4. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  5. Kompoziciya dlya polucheniya penoplasta: pat. 2213752. Ros. Federaciya [Composition for receiving polyfoam: pat. 2213752. Rus. Federation]; opubl. 10.10.03.
  6. Parahin I.V., Tumanov A.S. Fenolokauchukovyj penoplast povyshennoj plastichnosti [Phenolic-rubber foamed plastic of higher plasticity] // Aviacionnye materialy i tehnologii. 2014. №4 (33). C. 65–67. DOI: 10.18577/2071-9140-2014-0-4-65-67.
  7. Parahin I.V., Tumanov A.S. Fenolno-kauchukovyj penoplast marki VRP-4 [Phenolic-rubber foam the grade of VPP-4] // Aviacionnye materialy i tehnologii. 2014. №1 (30). C. 42–46. DOI: 10.18577/2071-9140-2014-0-1-42-46.
  8. Samatadze A.I., Parahin I.V., Troshkin I.V., Porosova N.F., Tumanov A.S. Fenolno-kauchukovyj penoplast s ponizhennoj goryuchestyu [Phenolic and rubber polyfoam with the lowered combustibility] // Vse materialy. Enciklopedicheskij spravochnik. 2013. №2. C. 14–17.
  9. Shivakumar K.N., Argade S.D., Sadler R.L., Sharpe M.M., Dunn L., Swaminathan G. Processing and properties of a lightweight fire resistant core material for sandwich structures // Journal of Advanced Materials. 2006. Vol. 38. No. 1. P. 1–17.
  10. Kablov E.N., Bejder E.Ya., Petrova G.N., Stolyankov Yu.V., Rumyanceva T.V. Penopoliimidy [Foamed polyimides] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 09. Available at: http://viam-works.ru (accessed: January 09, 2017). DOI: 10.18577/2307-6046-2015-0-4-9-9.
  11. Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Thermoplastic composite materials and foam polyimides] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 01. Available at: http://www.viam-works.ru (accessed: January 11, 2017).
  12. Poliimidnaya pena i metod ee polucheniya: pat. 101812232 Kitaj [Polyimide foam and method of its receiving: pat. 101812232 China]; zayavl. 9.04.10; opubl. 25.08.10.
  13. Kompoziciya dlya polucheniya penopoliimida: pat. 2024562 Ros. Federaciya [Composition for receiving penopoliimida: pat. 2024562 Rus. Federation]; zayavl. 30.04.92; opubl. 15.12.94.
  14. Zhestkij konstrukcionnyj penopoliimidnyj material i sposob ego polucheniya: pat. 102127225 Kitaj [Rigid constructional foam polyimide material and way of its receiving: pat. 102127225 China]; zayavl. 8.12.10; opubl. 20.07.11.
  15. Forming a foamed polyimide article: pat. 3249561 USA; filed 18.03.63; publ. 3.05.66.
  16. Ambient cure polyimide foam: pat. 4263410 USA; filed 19.02.80; publ. 21.04.81.
  17. Process of preparing polyimides from isocyanates and polycarboxylic acids: pat. 3489696 USA; filed. 6.10.66; publ. 13.06.70.
  18. Sposob i oborudovanie dlya nepreryvnogo vspenivaniya poliimidnogo poroshka: pat. 5338765 SShA [Way and the equipment for continuous foaming of polyimide powder: pat. 5338765 USA]; zayavl. 23.11.93; opubl. 16.08.94.
  19. Vspenennyj poliimidnyj blok i sposob ego polucheniya: zayavka 20040229969 SShA [Frothed polyimide block and way of its receiving: request 20040229969 USA]; zayavl. 21.04.04; opubl. 18.11.04.
  20. Sposob polucheniya teplostojkogo i teploizolyacionnogo baka: zayavka 2004256561 Yaponiya [Way of receiving heatresistant and heatinsulating tank: request 2004256561 Japan]; zayavl. 16.09.04; opubl. 16.03.06.
  21. Ahn M.-K., Moon Y.-W., Koh Y.-H., Kim H.-E. Production of highly porous triphasic calcium phosphates caffolds with excellent in vitro bioactivity using vacuum-assisted foaming of ceramic suspension (VFC) technique // Ceramics International. 2013. No. 39. P. 5879–5885.
  22. Vogt U.F., Gorbar M., Dimopoulos-Eggenschwiler P., Broenstrup A., Wagner G., Colombo P. Improving the properties of ceramic foams by a vacuum infiltration process // Journal of the European Ceramic Society. 2010. No. 30. Р. 3005–3011.
  23. Ahn M.-K., Jo I.-H., Koh Y.-H., Kim H.-E. Production of highly porous titanium (Ti) scaffolds by vacuum-assisted foaming of titanium hydride (TiH2) suspension // Materials Letters. 2014. No. 120. Р. 228–231.
  24. Qu Y.-N., Su Z.-G., Xu J., Huo W.-L., Song K.-C., Wang Y.-L., Yang J.-L. Preparation of ultralight glass foams via vacuum-assisted foaming // Materials Letters. 2016. No. 166. Р. 35–38.
  25. Vacuum refining of glassy materials with controlled foaming: pat. 0257238 France; filed 29.06.87, publ. 04.10.89.
  26. Vacuum refining of glass or the like with enhanced foaming: pat. 0297405 France; filed 22.06.88; publ. 04.01.89.
  27. Method and apparatus for vacuum foaming of panels: pat. 1048429 Spain; filed 27.03.00; publ. 08.10.03.
  28. Method and apparatus for vacuum foaming refrigerator cabinets: pat. 1781457 Spain; filed 27.03.00; publ. 30.07.10.
  29. Apparatus and method for vacuum foaming a refrigerator cabinet: pat. 2012099379 Korea, China; filed 17.01.12; publ. 17.01.11.
  30. Vacuum-assisted foaming method and apparatus for moulding insulation of refregiration containers: pat. 2011260351 USA; filed 17.02.10; publ. 27.10.11.
  31. Method and rotary drum installation for vacuum foaming of refrigerators: pat. 2006013002 Spain; filed 17.02.10; publ. 09.02.06.