Corrosion inhibitors in fiber-metal laminates based on aluminum and carbon fiber reinforced plastics

Voinov S.I., Zhelezina G.F., Volkov I.A., Solovjova N.A.
Voinov S.I., Zhelezina G.F., Volkov I.A., Solovjova N.A. Corrosion inhibitors in fiber-metal laminates based on aluminum and carbon fiber reinforced plastics // Proceedings of VIAM. 2017. No. 4. DOI: 10.18577/2307-6046-2017-0-4-6-6. URL: https://www.viam-works.ru/en/journal/2017/4/6
Keywords
carbon fiber, CFRP, aluminum alloys, fiber-metal laminates.
Abstract

The article discusses opportunity of application corrosion inhibitors in the layered metal-polymer composite material based on aluminum alloy sheets and layers of carbon fiber. The influence of corrosion inhibitors on corrosion processes, that occur when aluminum alloy sheet contacts with layer of carbon fiber, was investigated. Layered composite «aluminum–carbon fiber reinforced plastic» with separation layer, witch is contented corrosion inhibitors, has high corrosion resistance, which allows to consider layered composite «aluminum-carbon fiber reinforced plastic» as perspective material for application in aviation technology. This work was done as part of the complex scientific direction 6.2. «Layered crack resistance, high strength metal-polymer materials» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Gunyaev G.M., Krivonos V.V., Rumyancev A.F., Zhelezina G.F. Polimernye kompozicionnye materialy v konstrukciyah letatelnyh apparatov [Polymeric composite materials in designs of flight vehicles] // Konversiya v mashinostroenii. 2004. №4 (65). S. 65–69.
  5. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  6. Kablov E.N. Materialy i tehnologii VIAM dlya «Aviadvigatelya» [Materials and VIAM technologies for «Aircraft engine»] // Permskie aviacionnye dvigateli: inform. byul. 2014. №31. S. 43–47.
  7. Grabilnikov A.S., Mashinskaya G.P., Zhelezina G.F., Zinevich O.M., Deev I.S. Mezhslojnaya treshhinostojkost' gibridnogo kompozitnogo materiala ALOR [Interlaminar crack resistance of hybrid composite material ALOR] // Mehanika kompozitnyh materialov. 1994. T. 30. №2. S. 136–145.
  8. Mashinskaya G.P., Zhelezina G.F., Senatorova O.G. Laminated Fibrous Metal – Polymer Composites Soviet Advanced Composites Technology Series // Chapman & Hall. 1995. Р. 487–570.
  9. Postnov V.I., Senatorova O.G., Karimova S.A. i dr. Osobennosti formovaniya krupnogabaritnyh listov metallopolimernyh KM, ih struktura i svojstva [Features of formation of large-size sheets of metalpolymeric CM, their structure and properties] // Aviacionnye materialy i tehnologii. 2009. №4. S. 23–32.
  10. Kompozicionnyj sloistyj material i sposob ego polucheniya: pat. 2565186 Ros. Federaciya [Composite layered material and way of its receiving: pat. 2565186 Russ. Federation]; opubl. 15.09.15.
  11. Postnov V.I., Senatorova O.G., Zhelezina G.F. i dr. Opyt primeneniya MPKM ALOR D16/41 v nosovoj chasti kryla samoleta AN-124-100 [Experience of application of MPKM ALOR D16/41 in nasal part of airplane wing AN-124-100] // Aviacionnye materialy i tehnologii. 2009. №4. S. 8–17.
  12. Zhelezina G.F. Konstrukcionnye i funkcionalnye organoplastiki novogo pokoleniya [Constructional and functional organoplastics of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 06. Available at: http://www.viam-works.ru (accessed: November 1, 2016).
  13. Deev I.S., Zhelezina G.F. Fraktograficheskij analiz sloistogo metallopolimernogo kompozita alor posle ispytanij na treshhinostojkost [The fractographic analysis of layered metalpolymeric composite Alor after tests for crack resistance] // Kompozity i nanostruktury. 2015. T. 7. №3. S. 162–176.
  14. Laurens B.V. Development of a new hybrid material (ARALL) for aircraft structures // Industrial & Engineering Chemistry. 1983. Vol. 22 (3). P. 492–496.
  15. Gunnink J.W., Vlot A., De Vries T.J., Van Der Hoeven W. Glare technology development 1997–2000 // Applied Composite Materials. 2002. No. 9. P. 201–219.
  16. Antipov V.V., Senatorova O.G., Lukina N.F. i dr. Sloistye metallopolimernye kompozicionnye materialy [Layered metalpolymeric composite materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
  17. Botelho E.C., Campos A.N., de Barros E. et al. Damping behavior of continuous fiber/metal composite materials by the free vibration method // Composites. Part B. 2006. Vol. 37. P. 255–263.
  18. Freischmidt G., Coults R.S.P., Janardhana M.N. Aluminium/lithium alloy-CFRP hybrid laminate – fabrication and properties // Advanced composites ’93: proceedings of ICACM. 1993. С. 491–494.
  19. Karimova S.A., Pavlovskaya T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v usloviyah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2013. №4. St. 02. Available at: http://www.viam-works.ru (accessed: November 1, 2016).
  20. Pavlovskaya T.G., Kozlov I.A., Volkov I.A., Zakharov К.Е. Formation of hard wear-resistant anodic oxide coatings on parts made of casting aluminium alloys // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 04. Available at: http://viam-works.ru (accessed: November 1, 2016). DOI: 10.18577/2307-6046-2015-0-8-4-4.
  21. Pavlovskaya T.G., Volkov I.A., Kozlov I.A., Naprienko S.A. Ekologicheski uluchshennaya tehnologiya obrabotki poverhnosti alyuminievyh splavov [Ecologically improved technology of aluminum alloys surface treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 02 (accessed: November 1, 2016). DOI: 10.18577/2307-6046-2016-0-7-2-2.
  22. Kablov E.N., Karimova S.A., Semenova L.V. Korrozionnaya aktivnost ugleplastikov i zashhita metallicheskih silovyh konstrukcij v kontakte s ugleplastikom [Corrosion activity carbon plastics and protection of metal load bearing structures in contact with the carbon plastics] // Korroziya: materialy, zashhita. 2011. №12. S. 1–7.
  23. Ostapiuka M., Surowskaa B., Bienias J. Interface analysis of fiber metal laminates //Composite Interfaces. 2014. Vol. 21. No. 4. P. 309–318.
  24. Almeida R.S., Damato C.A., Botelho E.C., Pardini L.C., Rezende M.C. Effect of surface treatment on fatigue behavior of metal/carbon fiber laminates // J. Mater. Sci. 2008. No. 43. Р. 3173–3179.
  25. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  26. Wang W.X., Takao Y., Kashima I., Matsubara T. CFRP/Al-FRML based on nano-composite coating and its mechanical properties // Proceedings of International Conference 48th AIAA/ASME/ASCE/AHS/ASC Structures. 2007. Р. 1–10.
  27. Wang W.X., Takao Y., Matsubara T. Galvanic corrosion-resistant carbon fiber metal laminates // // Proceedings of 16th International Conference on Composite Materials. 2007. Р. 1–10.
  28. Vojnov S.I., Zhelezina G.F., Pavlovskaya T.G., Volkov I.A. Problema kontaktnoj korrozii pri sozdanii sloistyh metallopolimernyh kompozicionnyh materialov na osnove alyuminiya i ugleplastika [Problem of contact corrosion at creation of layered metalpolymeric composite materials on the basis of aluminum and carbon plastics] // Voprosy materialovedeniya. 2016. №1 (85). S. 127–133.
  29. Kozlova L.S., Sibileva S.V., Chesnokov D.V., Kutyrev A.E. Ingibitory korrozii (obzor) [Corrosion inhibitors (review)] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 67–75.