Influence of surface-active impurities and lanthanum on structure and properties of singlecrystal nickel superalloy ZhS36

Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A.
Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A. Influence of surface-active impurities and lanthanum on structure and properties of singlecrystal nickel superalloy ZhS36 // Proceedings of VIAM. 2017. No. 4. DOI: 10.18577/2307-6046-2017-0-4-2-2. URL: https://www.viam-works.ru/en/journal/2017/4/2
Keywords
single crystal superalloys, surface-active impurities, oxygen, sulfur, rare earth metals, lanthanum, structure, segrigation, high temperature strength, fatigue life, fatigue strength
Abstract

It is shown that impurity surface-active elements oxygen and sulfur contribute to the formation of misaligned (stray) grains and accelerate the diffusion at interfaces, growth of pores, cracks and coarsening of the hardening γ'-phase. Lanthanum is superior in refining capacity than the other rare-earth metals and magnesium, and the introduction of lanthanum addition allows to obtain ultrapure in the content of oxygen and sulfur alloy ZhS36, and to decrease misaligned grain defect formation. Segregating at interfaces, lanthanum replaces sulfur and decrease interface diffusion and mobility of interface dislocations. It is shown that lanthanum is a highly effective refining, microalloying and modifying addition that increase high temperature strength, cyclic strain life and heat resistance of ZhS36 single crystals. The work was performed with in the scope of complex scientific direction 10.1. realization: «The resourse saved technology of perspective cast and wrought supper alloy melting

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov D.E., Sidorov V.V., Min P.G. Povyshenie ekspluatacionnyh harakteristik monokristallov splava ZhS36-VI putem ego rafinirovaniya ot primesi sery // Rol' fundamental'nyh issledovanij pri realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda»: sb. dokl. III Vseros. nauch.-tehnich. konf. M.: VIAM, 2016. S. 13.
  3. Sidorov V.V., Min P.G., Burcev V.T., Kablov D.E., Vadeev V.E. Kompyuternoe modelirovanie i eksperimentalnoe issledovanie reakcij rafinirovaniya v vakuume slozhnolegirovannyh renijsoderzhashhih nikelevyh rasplavov ot primesej sery i kremniya [Computer modeling and pilot study of reactions of refinement in vacuum complex-alloyed rhenium contain nickel melt from sulfur and silicon impurity] // Vestnik RFFI. 2015. №1 (85). S. 32–36.
  4. Kablov E.N., Logunov A.V., Sidorov V.V. Obespechenie ultravysokoj chistoty metalla – garantiya kachestva litejnyh zharoprochnyh splavov [Ensuring ultrahigh purity of metal – quality assurance of foundry hot strength alloys] // Metally. 2000. №6. S. 40–46.
  5. Kablov D.E., Sidorov V.V., Min P.G., Gerasimov V.V., Bondarenko Yu. A. Vliyanie primesej sery i fosfora na svojstva monokristallov zharoprochnogo splava ZhS36-VI i razrabotka effektivnyh sposobov ego rafinirovaniya [The sulfur and phosphorus influence on properties of single crystals GHS36-VI supperalloy and design of effective methods their refining] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 3–9. DOI: 10.18577/2071-9140-2015-0-3-3-9.
  6. Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A. Vliyanie lantana na kachestvo i ekspluatacionnye svojstva monokristallicheskogo zharoprochnogo nikelevogo splava ZhS36-VI [The lanthanum influence on quality and operational properties of single crystal nickel base ZhS36-VI superalloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 02. Available at: http://www.viam-works.ru (accessed: February 2, 2016). DOI: 10.18577/2307-6046-2015-0-12-2-2.
  7. Min P.G., Sidorov V.V., Kablov D.E., Vadeev V.E. Issledovanie sery i fosfora v litejnyh zharoprochnyh nikelevyh splavah i razrabotka effektivnyh sposobov ih rafinirovaniya [Sulfur and phosphorus research in cast heat resisting nickel alloys and development of effective ways of their refinement] // Tehnologiya metallov. 2015. №12. S. 2–9.
  8. Burcev V.G., Sidorov V.V., Rigin V.E. Issledovanie poverhnostnogo natyazheniya i plotnosti rasplavov nikelya, soderzhashhego primesi sery, fosfora i azota [Research of surface tension and density rasplavov the nickel containing impurity of sulfur, phosphorus and nitrogen] // Fizika i himiya obrabotki materialov. 2013. №1. S. 52–56.
  9. McLean D. Grain Boundaries in Metals. Oxford University Press, 1957. P. 347.
  10. Kablov D.E., Sidorov V.V., Puchkov Yu.A. Osobennosti diffuzionnogo povedeniya primesej i rafiniruyushhih dobavok v nikele i monokristallicheskih zharoprochnyh splavah [Diffusion behavior features of impurities and microalloying additives in nickel and single crystal superalloys] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 24–31. DOI: 10.18577/2071-9140-2016-0-1-24-31.
  11. Kablov D.E., Sidorov V.V., Budinovskij S.A., Min P.G. Vliyanie primesi sery na zharostojkost monokristallov zharoprochnogo splava ZhS36-VI s zashhitnym pokrytiem [The influence of sulfur impurity on heat resistance of single crystals of ZhS36-VI alloy with protective coating] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 20–23. DOI: 10.18577/2071-9140-2016-0-1-20-23.
  12. Kablov D.E., Belyaev M.S., Sidorov V.V., Min P.G. Vliyanie primesej sery i fosfora na malociklovuyu ustalost monokristallov zharoprochnogo splava ZhS36-VI [The influence of sulfur and phosphorus impurities on low cycle fatigue of single crystals of ZhS36-VI alloy] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 25–28. DOI: 10.18577/2071-9140-2015-0-4-25-28.
  13. Sidorov V.V., Min P.G. Rafinirovanie slozhnolegirovannogo nikelevogo rasplava ot primesi sery pri plavke v vakuumnoj indukcionnoj pechi. Chast 1 [Refinement complex-alloyed nickel melt from sulfur impurity when melting in the vacuum induction furnace. Part 1] // Elektrometallurgiya. 2014. №3. S. 18–23.
  14. Sidorov V.V., Min P.G. Rafinirovanie slozhnolegirovannogo nikelevogo rasplava ot primesi sery pri plavke v vakuumnoj indukcionnoj pechi. Chast 2 [Refinement complex-alloyed nickel melt from sulfur impurity when melting in the vacuum induction furnace. Part 2] // Elektrometallurgiya. 2014. №5. S. 26–30.
  15. Sidorov V.V., Min P.G., Folomejkin Yu.I., Vadeev V.E. Vliyanie skorosti fil'tracii slozhnolegirovannogo nikelevogo rasplava cherez penokeramicheskij filtr na soderzhanie primesi sery v metalle [Influence of speed of filtering complex-alloyed nickel melt via the foamceramics filter on the content of impurity of sulfur in metal] // Elektrometallurgiya. 2015. №5. S. 12–15.
  16. Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I. Issledovanie processov rafinirovaniya v vakuume slozhnolegirovannyh nikelevyh rasplavov ot primesi sery [Research of refining processes in vacuum complex-alloyed nickel melt from sulfur impurity] // Metally. 2015. №6. S. 57–63.
  17. Smirnov L.A., Rovnushkin V.A., Oryshhenko A.S., Kalinin G.Yu., Milyuc V.G. Modificirovanie stali i splavov redkozemelnymi elementami. Soobshhenie 1 [Modifying of steel and alloys rare earth elements. Message 1] // Metallurg. 2015. №11. S. 57–63.
  18. Kablov D.E., Simonov V.N., Alekseeva M.S. Issledovanie stroeniya fil'tra i osobennostej filtracii primesej poristoj keramikoj iz oksida alyuminiya Al2O3 [Research of structure of the filter and features of impurity filtering by porous ceramics from Al2O3 aluminum oxide] // Aviacionnye materialy i tehnologii. 2016. №4 (45). S. 47–53. DOI: 10.18577/2071-9140-2016-0-4-47-53.
  19. Goryunov A.V., Sidorov V.V., Rigin V.E., Zajcev V.E. Formirovanie nanostrukturirovannogo sostoyaniya v litejnom zharoprochnom splave VZhM4-VI pri mikrolegirovanii ego lantanom [Creation of nanostructure state in cast supperalloy due to microalloying with lanthanum] // Aviacionnye materialy i tehnologii. 2013. №3. S. 39–43.
  20. Wang S., Nates R., Pasang T., Ramesany M. Modelling of gas tungsten arc welding under Maragony convection // Universal Journal of Mechanical Engineering. 2015. Vol. 3 (5). P. 185–201.
  21. Kuang-Di Xu, Zhong-Ming Ren, Chuan-Jun Li. Progress in application of rare metals in superalloys // Rare Met. 2014. Vol. 33 (2). P. 111–126.
  22. Seah M.P. Grain boundary segregation // Journal of Physics F: Metal Physics. 1980. Vol. 10. P. 1043–1064. DOI:10.1088/0305-4608/10/6/006.
  23. Kaptay G. Partial Tension of components of a solution // Langmuir. 2015. Vol. 31. P. 5796–5804. DOI: 10.1021/acs.langmuir.5b00217.
  24. Bokshtejn B., Epishin A., Esin V. i dr. Rost i zalechivanie por v monokristallah zharoprochnyh splavov na nikelevoj osnove [Growth and curing of time in monocrystals of hot strength alloys on nickel basis] // Zhurnal funkcional'nyh materialov. 2007. T. 1. №5. S. 162–169.