The research of fretting-wear slip and ion-plasma coatings

Gorlov D.S., Skripak V.I., Muboyadzhyan S.A., Egorova L.P.
Gorlov D.S., Skripak V.I., Muboyadzhyan S.A., Egorova L.P. The research of fretting-wear slip and ion-plasma coatings // Proceedings of VIAM. 2017. No. 3. DOI: 10.18577/2307-6046-2017-0-3-7-7. URL: https://www.viam-works.ru/en/journal/2017/3/7
Keywords
fretting wear, antifretting coating, hard lubricant coating, slip technology, ion-plasma technology, tribological properties
Abstract

This article provides test data on fretting-wear antifretting coatings developed at VIAM for the last time. Experienced hard lubricant coating VFP-5, slip VPMSA and microcline coating system Ti–TiN, obtained by ion-plasma technology. For the research of the tribological properties was chosen as the method of «finger-plate». According to test results was estimated wear curves, graphs of the coefficient of friction and resistance, the appearance of spots of wear. This work was performed within the framework of strategic directions 17. «Comprehensive anticorrosion protection, hardening, wear-resistant protective and heat-resistant coating», сomplex problem 17.3. «Multilayer heat-resistant and heat-resistant coating, nanostructural hardening of erosion and corrosion-resistant, wear-resistant, antifatigue coating to protect parts hot gas path and compressor of GTE and GTU» («The strategic directions of development of materials and technologies of their processing for the period till 2030»

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] // Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  3. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S. Nanoslojnye uprochnyayushchie pokrytiya dlya zashhity stalnyh i titanovyh lopatok kompressora GTD [Nanolayer strengthening coverings for protection of steel and titanic compressor blades of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 3–8.
  4. Kablov E.N. Litye lopatki gazoturbinnyh dvigatelej. Splavy, tehnologii, pokrytiya. 2-e izd. [Cast blades of gas turbine engines. Alloys, technologies, coverings. 2nd ed.]. M.: Nauka, 2006. S. 531–534.
  5. Vinogradov S.S., Terkulova Yu.A., Kurdyukova E.A., Nikiforov A.A. Iznosostojkoe, antifrikcionnoe i frettingostojkoe pokrytie na osnove Ni–B [Wear-proof, antifriction and fretting-resistant coating based on Ni–B] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 02. Available at: http://www.viam-works.ru (accessed: December 01, 2016). DOI: 10.18577/2307-6046-2015-0-1-2-2.
  6. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  7. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Pomelov Ya.A. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Konversiya v mashinostroenii. 1999. №2. S. 42–47.
  8. Fouvry S., Duo P., Perrucchaut Ph. A quantitative approach of Ti–6Al–4V fretting damage: friction, wear and crack nucleation // Wear. 2004. Vol. 257. No. 9–10. P. 916–929.
  9. ASTM Standard G133-05. Standard Test Method for Linearly Reciprocating Ball-on-Flat Sliding Wear. 2010.
  10. Markova E.S., Yakusheva N.A., Pokrovskaja N.G., Shalkevich A.B. Tehnologicheskie osobennosti proizvodstva martensitostareyushhej stali VKS-180 [Technological features of the production of maraging steel VKS-180] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №7. St. 01. Available at: http://www.viam-works.ru (accessed: December 01, 2016).
  11. Muboyadzhyan S.A., Lutsenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povysheniya sluzhebnyh harakteristik lopatok kompressora GTD metodom ionnogo modificirovaniya poverhnosti [Research of possibility of increase of office characteristics of compressor blades of GTE by method of ionic modifying of surface] // Trudy VIAM: elektron. nauch-tehnih. zhurn. 2013. №1. St. 02. Available at: http://viam-works.ru (accessed: December 01, 2016)
  12. Galoyan A.G., Muboyadzhyan S.A., Egorova L.P., Bulavinceva E.E. Korrozionnostojkoe pokrytie dlya zashhity detalej GTD iz vysokoprochnyh konstrukcionnyh martensitostareyushhih stalej na rabochie temperatury do 450°C [Corrosion-resistant coating for protection of GTE details made of high-strength maraging constructional steel with operating temperature up to 450°C] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №6. St. 03. Available at: http://www.viam-works.ru (accessed: December 01, 2016). DOI: 10.18577/2307-6046-2014-0-6-3-3.
  13. Umanskij A.P., Pugachevskaya E.P., Himko A.N. Razrabotka tehnologii naneseniya novyh iznosostojkih kompozicionnyh pokrytij dlya uprochneniya detalej aviacionnyh dvigatelej [Development of technology of drawing new anti wear composition coatings for hardening of details of aircraft engines] // Aviacionno-kosmicheskaya tehnika i tehnologiya. 2009. №9. S. 38–44.
  14. Muboyadzhyan S.A., Gorlov D.S., Shhepilov A.A., Konnova V.I. Issledovanie dempfiruyushhej sposobnosti ionno-plazmennyh pokrytij [Study of damping capacity of ion-plasma coatings] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 67–72. DOI: 10.18577/2071-9140-2014-0-s5-67-72.
  15. Gorlov D.S., Muboyadzhyan S.A., Shhepilov A.A., Aleksandrov D.A. Issledovanie erozionnoj stojkosti i teplostojkosti ionno-plazmennyh dempfiruyushhih pokrytij [The research of erosion resistance and heat resistance of the ion-plasma damping coatings] // Aviacionnye materialy i tehnologii. 2016. №2. S. 11–17. DOI: 10.18577/2071-9140-2016-0-2-11-17.