Installation for measuring the transmission coefficient at ultrahigh frequencies of nonmetallic materials at high temperatures up to 1200°C

Beljaev А.А., Bespalova E.E., Payarel S.M.
Beljaev А.А., Bespalova E.E., Payarel S.M. Installation for measuring the transmission coefficient at ultrahigh frequencies of nonmetallic materials at high temperatures up to 1200°C // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-9-9. URL: https://www.viam-works.ru/en/journal/2017/12/9
Keywords
transmission coefficient of microwave frequency, radio-transparent material, high temperature, installation.
Abstract

In aviation and space engineering are widely used materials allowing the passage of electromagnetic energy – radio transparent materials. In the design of radio-transparent materials, especially multilayer and broadband is a very important point is the determination by experiment of the transmission coefficient (KP) as separate layers of the materials and multilayer material (or parts) in the whole specified frequency range (from decimeter to millimeter wavelengths). One of the most common methods is the measurement of dielectric properties of materials and then calculate KP. However, besides the fact that it is not direct measurement, such measurements are accompanied by errors due to inaccuracy of manufacture of the samples to the dimensions of the waveguide or resonator. In addition, at frequencies above 10 GHz, the dimensions of the waveguide or resonator section become smaller than the inhomogeneities of heterogeneous materials, which makes it impossible to carry out measurements

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
  5. Belyaev A.A., Kondrashov S.V., Lepeshkin V.V., Romanov A.M. Radiopogloshhayushhie materialy [Radio absorbing materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 348–352.
  6. Belyaev A.A., Bespalova E.E., Romanov A.M. Pozharobezopasnye radiopogloshhayushhie materialy dlya bezehovyh kamer [Fireproof radio absorbing materials for anechoic cameras] // Aviacionnye materialy i tehnologii. 2013. №1. S. 53–55.
  7. Agafonova A.S., Belyaev A.A., Kondrashov E.K., Romanov A.M. Osobennosti formirovaniya monolitnyh konstrukcionnyh radiopogloshhayushhih materialov na osnove kompozitov, napolnennyh rezistivnym voloknom [Features of the formation of monolithic structural radio absorbing materials based on composites filled with resistive fibers] // Aviacionnye materialy i tehnologii. 2013. №3. S. 56–59.
  8. Hippel A.R. Dielektriki i ih primenenie [Dielectrics and their application]. M.–L.: Gosenergoizdat, 1959. 336 s.
  9. Brandt L.A. Issledovaniya dielektrikov na sverhvysokih chastotah [Researches of dielectrics at super-high frequencies]. M.: Gos. izd-vo fiz.-mat. lit., 1963. S. 191–201.
  10. Krylov V.P. Izmerenie dielektricheskih svojstv dioksida kremniya na chastote 10 GGc pri nagreve do 1200°С v cilindricheskom volnovodnom rezonatore [Measurement of dielectric properties of silicon dioxide at frequency of 10 GHz when heating to 1200°С in the cylindrical waveguide resonator] // Zavodskaya laboratoriya. Diagnostika materialov. 2007. T. 73. №9. S. 47–49.
  11. Ustrojstvo dlya opredeleniya dielektricheskoj pronicaemosti obrazca materiala pri vozdejstvii vneshnih faktorov: pat. 2453856 Ros. Federaciya [The device for determination of dielectric permittivity of sample of material at influence of external factors: pat. 2453856 Rus. Federation]; opubl. 22.02.11.
  12. Krylov V.P. Opredelenie dielektricheskoj pronicaemosti materialov pri vysokotemperaturnom nagreve v obemnom volnovodnom rezonatore [Determination of dielectric permittivity of materials at high-temperature heating in the cavity waveguide resonator] // Zavodskaya laboratoriya. Diagnostika materialov. 2016. T. 82. №7. S. 36–39.
  13. Krylov V.P., Grachev V.A., Rogov D.A. Izmerenie dielektricheskoj pronicaemosti dioksida kremniya pri nagreve v vysokotemperaturnom obemnom volnovodnom rezonatore [Measurement of dielectric permittivity of silicon dioxide when heating in the high-temperature cavity waveguide resonator] // Zavodskaya laboratoriya. Diagnostika materialov. 2016. T. 82. №10. S. 39–43.
  14. Litovchenko A.V., Ignatenko G.K. Nekotorye aspekty metrologicheskogo obespecheniya izmereniya dielektricheskih svojstv materialov na sverhvysokoj chastote v intervale temperatur 20–1200°S [Some aspects of metrological ensuring measurement of dielectric properties of materials at super-high frequency in the range of temperatures 20-1200°C] // Zavodskaya laboratoriya. Diagnostika materialov. 2010. T. 76. №8. S. 66–69.
  15. Arhangel'skij Yu.S., Kalganov S.G., Trigorlyj S.V. Izmerenie dielektricheskih parametrov dielektrikov v diapazone SVCh pri vysokoj temperature [Measurement of dielectric parameters of dielectrics in the range of the microwave oven at high temperature] // Voprosy elektrotehnologii. 2017. №2 (15). S. 102–108.
  16. Gdaljov A.V., Ogurcov K.N. Izmerenie dielektricheskih svojstv materialov pri vysokih temperaturah [Measurement of dielectric properties of materials at high temperatures] // Voprosy elektrotehnologii. 2013. №1 (1). S. 27–30.
  17. Arzhannikov A.V., Ahmetov T.D., Kalinin P.V. i dr. Stend issledovanij po SVCh nagrevu i prevrashheniyu veshhestv [Stand of researches on the microwave oven to heating and transformation of substances]. Novosibirsk: In-t yader. fiziki im. G.I. Budkera SO RAN, 2004. S. 6–11.
  18. Batura V.G., Moiseev V.K., Rybalka N.V. Pribor dlya izmereniya parametrov dielektrikov na SVCh v intervale temperatur 20–1500°C [The device for measurement of parameters of dielectrics on the microwave oven in the range of temperatures 20-1500°C] // Elektronnaya tehnika. Ser.: Elektronika SVCh. 1974. №1. S. 17–24.
  19. Litovchenko A.V. Vysokotochnyj SVCh-izmeritel ε i tg nagrevaemyh obrazcov [High-precision microwave measuring instrument ε and tgδ of heated-up samples] // Zavodskaya laboratoriya. Diagnostika materialov. 2002. T. 68. №10. S. 35–38.
  20. Brehovskih S.M., Demyanov V.V., Zalcman E.B. i dr. Ustanovka dlya izmereniya dielektrikov v sverhvysokochastotnom diapazone pri temperaturah do 2300 K [Installation for measurement of dielectrics in the superhigh-frequency range at temperatures up to 2300 K] // Pribory i tehnika eksperimenta. 1985. №4. S. 141–143.
  21. Nikolskij V.V., Nikolskaya T.I. Elektrodinamika i rasprostranenie radiovoln [Electrodynamics and radio propagation]. M.: URSS, 2012. S. 44–164.
  22. Krylov V.P. Modelirovanie aktualnyh radiofizicheskih zadach prohozhdeniya volny cherez dielektricheskij sloj [Modeling of actual radio physical problems of passing of wave through dielectric layer] // Zavodskaya laboratoriya. Diagnostika materialov. 2014. T. 80. №9. S. 28–32.