Some features of semi-pregs application for vacuum formation of polymeric composite materials (review)

Donetskiy K.I., Dushin M.I., Mischun M.I., Sevastyanov D.V.
Donetskiy K.I., Dushin M.I., Mischun M.I., Sevastyanov D.V. Some features of semi-pregs application for vacuum formation of polymeric composite materials (review) // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-8-8. URL: https://www.viam-works.ru/en/journal/2017/12/8
Keywords
polymeric composite materials, prepregs, semi-pregs, fiber, impregnation, permeability, porosity.
Abstract

Increase in demand for designs from polymeric composite materials (РСМ) has demanded decrease from cost value and as a result, search of replacement to rather expensive and autoclave formation which is now the main way of manufacturing of the high-loaded products. Use of vacuum formation of prepregs has not shown satisfactory results in view of receiving plastics with the high maintenance of time. As one of solutions of this problem, it was offered to pass to development of other materials – semi-pregs, consisting of the dry (not impregnated) part of fabric and binding. Many manufacturing firms of materials include in the nomenclature of the materials wide ruler semi-pregs. Semi-pregs are considered by large developers and consumers of polymeric composite materials when manufacturing perspective elements of rocket and aviation engineering of military and civil assignment. Pressure and temperature are important parameters of processing of such PСM, to questions on air removal from semi-

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  5. Fahrang L., Fernlund G. Void evolution and gas transport during cure in out-of-autoclave prepreg laminates // Proceedings of the SAMPE 2011 Conference (Long Beach, CA, United States, May 23–26, 2011). 2011. Paper No. 1153.
  6. Kostyukov V.I. Stekloplastiki na osnove kapillyarnyh volokon i mikrosfer // Aviacionnye materialy na rubezhe XX–XXI veka. M.: VIAM, 1994. S. 197–203.
  7. Platonov A.A., Kogan D.I., Dushin M.I. Izgotovlenie trehmernorazmernyh PKM metodom propitki plenochnym svyazuyushhim // Plasticheskie massy. 2013. №6. S. 56–61.
  8. Sloan J. Research sheds light on air and air-bubble behavior in OOA aerospace prepregs. Case Study Post: 06.01.2015.
  9. Thomas S., Nutt S.R. Temperature dependence of resin flow in a resin film infusion (RFI) process by ultrasound imaging // Applied Composition Materials. 2009. Vol. 16. P. 183–196.
  10. Centea T., Hubert P. Measuring the impregnation of an out-of-autoclave prepreg by micro-CT // Composition Science Technologies. 2011. Vol. 71. P. 593–599.
  11. Centea T., Hubert P. Modelling the effect of material properties and process parameters on tow impregnation in out-of-autoclave prepregs // Composition Applied Science Manufacture. 2012. Vol. 43. P. 1505–1513.
  12. Simacek P., Neacsu V., Advani S.G. A phenomenological model for fiber tow saturation of dual scale fabrics in liquid composite molding // Polymer Composites. 2010. Vol. 31. P. 1881–1889.
  13. Hwang W.R., Advani S.G. Numerical simulations of Stokes–Brinkman equations for permeability prediction of dual scale fibrous porous media // Physical Fluids. 2010. Vol. 22. P. 113–115.
  14. Zhou F., Alms J., Advani S. A closed form solution for flow in dual scale fibrous porous media under constant injection pressure conditions // Composition Science Technologies. 2008. Vol. 68. P. 699–708.
  15. Zhou F., Kuentzer N., Simacek P., Advani S., Walsh S. Analytic characterization of the permeability of dual-scale fibrous porous media // Composition Science Technologies. 2006. Vol. 66. P. 2795–2803.
  16. Bickerton S., Advani S.G. Characterization of racetracking in liquid composite molding processes // Composition Science Technologies. 1999. Vol. 59. P. 2215–2229.
  17. Dushin M. I., Hrulkov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovleniya izdelij iz PKM metodom propitki pod davleniem [Features of manufacturing of products from PCM impregnation method under pressure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 18–26.
  18. Dushin M.I., Muhametov R.R., Platonov A.A., Merkulova Yu.I. Issledovanie filtracionnyh harakteristik armiruyushhih napolnitelej i svyazuyushhih pri razrabotke tehnologii bezavtoklavnogo formovaniya polimernyh kompozicionnyh materialov [Study of filtration characteristics of reinforcing fillers and binders in the development of non-out-autoclave technology for polymer composite material] // Aviacionnye materialy i tehnologii. 2013. №2. S. 22–25.
  19. Tavares S.S., Michaud V., Mаnson E. Semipregs: how through-thickness air permeability and resin flow correlate during vacuum-bag only cure // The 9th International Conference on Flow Processes in Composite. 2008. P. 76–81.
  20. Maguire J., Brádaigh C.Ó., Simacek P., Advani S.G. Through thickness resin flow and heat transfer modeling of partially impregnated composite materials for thick-section parts // The 13th International conference on flow processing in composite materials. 2010. P. 132–138.
  21. Van West B.P., Pipes R.B., Advani S.G. The consolidation of commingled thermoplastic fabrics // Polymer Composites. 1991. Vol. 12 (6). P. 417–427.
  22. Chan A.W., Morgan R.J. Tow impregnation during resin transfer molding of bi-directional nonwoven fabrics // Polymer Composites. 1993. Vol. 14 (4). P. 335–340.
  23. Sadiq T.A.K., Advani S.G., Parnas R.S. Experimental investigation of transverse flow through aligned cylinders // International Journal of Multiphase Flow. 1995. Vol. 21 (5). P. 755–774.
  24. Bernet N., Michaud V., Bourban P.E., Manson E. An impregnation model for the consolidation of thermoplastic composites made from commingled yarns // Journal of Composites Materials. 1999. Vol. 33 (8). P. 751–772.
  25. Foley M.E., Gillespie W. Modeling the effect of fiber diameter and fiber bundle count on tow impregnation during liquid molding processes // Journal of Composites Materials. 2005. Vol. 39 (12). P. 1045–1065.
  26. Neacsu V., Abu Obaid A., Advani S.G. Spontaneous radial capillary impregnation across a bank of aligned micro-cylinders – Part I: Theory and model development // International Journal of Multiphase Flow. 2006. Vol. 32 (6). P. 661–676.
  27. Yamaleev N., Mohan R. Effect of the phase transition on intra-tow flow behavior and void formation in liquid composite molding // International Journal of Multiphase Flow. 2006. Vol. 32 (10–11). P. 1219–1233.
  28. Centea T., Hubert P. Modelling the effect of material properties and process parameters on tow impregnation in out-of-autoclave prepregs // Composites: Part A. 2012. Vol. 43. P. 1505–1513.
  29. Gebart B.R. Permeability of unidirectional reinforcements for RTM // Journal of Composites Materials. 1992. Vol. 26 (8). P. 1100–1112.
  30. Simacek P., Neacsu V., Advani S.G. A phenomenological model for fiber tow saturation of dual scale fabrics in liquid composite molding // Polymer Composites. 2010. Vol. 31 (11). P. 1881–1889.
  31. Lundström T.S., Gebart B.R. Effect of perturbation of fibre architecture on permeability inside fibre tows // Journal of Composites Materials. 1995. Vol. 29 (4). P. 424–443.
  32. Bechtold G., Ye L. Influence of fibre distribution on the transverse flow permeability in fibre bundles // Composites Science Technologies. 2003. Vol. 63 (14). P. 2069–2079.
  33. Chen X., Papathanasiou T. The transverse permeability of disordered fiber arrays: a statistical correlation in terms of the mean nearest interfiber spacing // Transparence Porous Media. 2008. Vol. 71 (2). P. 233–251.
  34. Grunenfelder L.K., Nutt S.R. Void formation in composite prepregs – effect of dissolved moisture // Composites Science Technologies. 2010. Vol. 70. P. 2304–2309.
  35. Dushin M.I., Hrulkov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Out-of-autoclave formation carbon plastics on the basis of the prepregs received on solution technology] // Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
  36. Dushin M.I., Doneckij K.I., Karavaev R.Yu. Ustanovlenie prichin obrazovaniya poristosti pri izgotovlenii PKM [Identification of the reasons of porosity formation when manufacturing composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6 (42). St. 08. Available at: http://www.viam-works.ru (accessed: October 30, 2017). DOI: 10.18577/2307-6046-2016-0-6-8-8.
  37. Olivier P., Cottu J.P., Ferret B. Effects of cure cycle pressure and voids on some mechanical properties of carbon/epoxy laminates // Composites. 1995. Vol. 26 (7). P. 509–515.
  38. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  39. Lykov A.V. Teoriya sushki [Drying theory]. M.: Energiya, 1968. 472 s.
  40. Ruiz E., Achim V., Bread J., Chatel S., Trouchu F. A fast numerical approach to reduce voud formation in liquid composite molding // The 8-th International Conference on Flow Processes in Composite Materials. 2006. P. 251–260.
  41. Arafath A.R.A., Fernlund G., Poursartip A. Gas Transport in Prepregs:Model and Permeability Experiments // Proceedings of the 17th International Conference on Composite Materials (Edinburgh, UK, July 27–31, 2009). 2009. P. 220–226.
  42. Arbter R., Beraud J.M., Binetruy C. et al. Experimental Determination of the Permeability of Textiles: A Benchmark Exercise // Composites Part A: Applied Science and Manufacturing. 2011. Vol. 42. No. 9. P. 1157–1168.
  43. Louis B., Hsiao K., Fernlund G. Gas Permeability Measurements of Out of Autoclave Prepreg MTM45-1/CF2426A // International SAMPE Symposium. Seattle, 2010. P. 342–354.
  44. Putnam J.W., Seferis J.C. Prepreg Gas Permeation as a Function of Fiber Orientation and Aging Time // Journal of Advanced Materials. 1995. Vol. 26. No. 3. P. 35–41.
  45. Xin C., Li M., Gu Y., Li Y., Zhang Z. Measurement and Analysis on in-Plane and through-Thickness Air Permeation of Fiber/Resin Prepreg // Journal of Reinforced Plastics and Composites. 2011. Vol. 30. No. 17. P. 1467–1479.
  46. Umemoto Y., Gouke M., Mashima Y. Out of autoclave «semi-preg». Technical development of resin transfer molding // Proceedings of the 18th International Conference on Composite materials (Korea, August 21–26, 2011). 2011. Paper No. TH05-2.