On the effectiveness of curing blanks from polymer concrete with a polyether matrix by an ultraviolet irradiator

Veshkin E.A, Postnov V.I., Semenychev V.V., Krasheninnikova E.V., Ershov V.V.
Veshkin E.A, Postnov V.I., Semenychev V.V., Krasheninnikova E.V., Ershov V.V. On the effectiveness of curing blanks from polymer concrete with a polyether matrix by an ultraviolet irradiator // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-7-7. URL: https://www.viam-works.ru/en/journal/2017/12/7
Keywords
sclerometry, microscopic studies, microhardness, polyester resin, ultraviolet irradiation.
Abstract

Samples from cured polyester resin and polymer concrete, made on its basis, were treated with an ultraviolet irradiator for two minutes to two hours. On the initial samples and samples subjected to ultraviolet irradiation, the microhardness values and the width of the grooves obtained with the help of a laboratory sclerometer with a load on a diamond indentor of 10 N were evaluated. It was shown that with increasing duration of ultraviolet irradiation, the microhardness values increase, and the width sclerometric grooves decreases. The increase in the degree of polymerization of the samples leads to the alignment of the shoreline grooves.

Reference list
  1. Solomatov V.I. Tehnologiya polimerbetonov i armopolimerbetonnyh izdelij [Technology of polymer concrete and the reinforced polymer concrete products]. M.: Strojizdat, 1984. 142 s.
  2. Paturoev V.V. Polimerbetony [Polymer concrete]. M.: Strojizdat, 1987. 286 s.
  3. Figovskij O.L., Bejlin D.A. Nanostrukturirovannyj silikatnyj polimerbeton [Nanostructured silicate polymer concrete] // Vestnik MGSU. 2014. №3. S. 197–204.
  4. Satdinov R.A., Veshkin E.A., Postnov V.I., Abramov P.A. Rol antiadgezionnyh pokrytij v tehnologicheskom processe formovaniya PKM [The role of anti-adhesive coatings in the technological process of PCM molding] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №4 (40). St. 10. Available at: http://www.viam-works.ru (accessed: October 04, 2017). DOI: 10.18577/2307-6046-2016-0-4-10-10.
  5. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  6. Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Fenolformaldegidnye svjazuyushhie novogo pokoleniya dlya materialov interera [Phenolformaldehyde binding new generation for interior materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 265–272.
  7. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  8. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  9. Dospehi dlya «Burana». Materialy i tehnologii VIAM dlya MKS «Energiya–Buran» / pod obshh. red. E.N. Kablova. M.: Nauka i zhizn, 2013. 128 s.
  10. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada // Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  11. Postnov V.I., Veshkin E.A., Abramov P.A. Osobennosti podgotovki polimernogo svyazuyushhego dlya snizheniya poristosti stekloplastikov, poluchaemyh metodom vakuumnogo formovaniya [Features of preparation polymeric binding for decrease in porosity of the fibreglasses received by method of vacuum formation] // Izvestiya Samarskogo nauchnogo centra RAN. 2011. T. 13. №4 (2). S. 462–468.
  12. Veshkin E.A., Postnov V.I., Abramov P.A. Puti povysheniya kachestva detalej iz PKM pri vakuumnom formovanii [Ways of improvement of quality of details from PCM at vacuum formation] // Izvestiya Samarskogo nauchnogo centra RAN. 2012. T. 14. №4 (3). S. 834–839.
  13. Veshkin E.A. Osobennosti bezavtoklavnogo formovaniya nizkoporistykh PKM [Features of out-of-autoclave forming of poor-porous PCM] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2016. №2. St. 07. Available at: http://www.viam-works.ru (accessed: October 04, 2017). DOI 10.1857/2307-6046-2016-0-2-7-7
  14. Tager A.A. Fiziko-himiya polimerov [Physics and chemistry of polymers]. M.: Nauchnyj mir, 2007. 128 s.
  15. Postnova M.V., Postnov V.I. Opyt razvitiya bezavtoklavnyh metodov formovaniya PKM [Development experience out-of-autoclave methods of formation PCM] // Trudy VIAM: ehlektron. nauch.-tekhnich. zhurn. 2014. №4. St. 06. Available at: http://www.viam-works.ru (accessed: October 04, 2017). DOI 10.18577/2307-6046-2014-0-4-6-6.
  16. Ilin V.A., Postnov V.I., Semenychev V.V., Petuhov V.I., Nikitin K.E. Effektivnost sovremennyh naukoemkih tehnologij [Efficiency of modern high technologies] // 75 let. Aviacionnye materialy. M.: VIAM, 2007. S. 413–416.
  17. Semenychev V.V., Panarin A.V. Primenenie sklerometrii dlya povysheniya informativnosti izmeryaemyh harakteristik hromovyh i nikelevyh pokrytij [Application of sclerometry for more informativeness measured characteristics of chromium and nickel coatings] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2016. №3. St. 05. Available at: http://www. materialsnews.ru (accessed: October 04, 2017).
  18. Semenychev V.V. Nikelirovanie stali metodom elektronatiraniya [Nickel plating became method of electro polish] // Galvanotehnika i obrabotka poverhnosti. 2017. №1. S. 23–27.
  19. Semenychev V.V., Salahova R.K. Ocenka adgezii nikel-kobaltovogo pokrytiya k steklo- i ugleplastiku metodom carapanya [Evaluation of nickel-cobalt coating adhesion to fiberglass and carbon fiber-reinforced plastic by scratching] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7 (43). St. 06. Available at: http://www.viam-works.ru (accessed: October 04, 2017). DOI: 10.18577/2307-6046-2016-0-7-6-6.
  20. Panarin A.V., Semenychev V.V. Ocenka tribotehnicheskih harakteristik karbidohromovogo pokrytiya [Assessment of tribe of technical characteristics of carbide chrome plating] // Fizika i himiya obrabotki materialov. 2016. №5. S. 65–70.
  21. Panarin A.V., Semenychev V.V. Iznos karbidohromovogo pokrytiya pri razlichnyh urovnyah udel'noj nagruzki [Wear of carbide chrome covering at different levels of unit load] // Materialovedenie. 2017. №6. S. 39–42.
  22. Semenychev V.V., Salahova R.K. Pribor dlya ocenki svojstv pokrytij [The device for assessment of properties of coverings] // Zavodskaya laboratoriya. Diagnostika materialov. 2017. T. 83. №2. S. 60–65.
  23. Veshkin E.A., Postnov V.I., Semenychev V.V. Ocenka svyazuyushhego VST-1210 s razlichnymi rezhimami otverzhdeniya metodami sklerometrii // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №8. St. 09. Available at: http://www.viam-works.ru (accessed: October 04, 2017). DOI: 10.18577/2307-6046-2017-0-8-9-9.
  24. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.