Prospects for the use of organosilicon elastomers in the development of modern polymer materials and coatings for various purposes

Kraev I.D., Popkov O.V., Shuldeshov Е.М., Sorokin A.E., Yurkov G.Yu.
Kraev I.D., Popkov O.V., Shuldeshov Е.М., Sorokin A.E., Yurkov G.Yu. Prospects for the use of organosilicon elastomers in the development of modern polymer materials and coatings for various purposes // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-5-5. URL: https://www.viam-works.ru/en/journal/2017/12/5
Keywords
silicone, sealant, rubber heat-insulating material, sound-absorbing materials, moisture-proof coatings, biocompatible materials, electrical insulating materials, dielectric permittivity.
Abstract

In this paper, organosilicon polymers, as well as composite materials of various purposes on their basis, were considered. The most important properties of organosilicon compounds were identified, which caused their wide application in various spheres: aircraft and rocket engineering, electronics and radio engineering, construction, and medicine. A brief review was carried out in the field of modern silicone sealants, rubbers, paint and varnish materials, materials for electrical and thermal insulation, medical supplies, as well as modern composite materials. Various applications and methods for the modification of silicone rubbers, in particular polydimethylsiloxane rubber, and others have been considered. Special attention was paid in the article to organosilicon stair block copolymers. A number of polymer and composite materials obtained on its basis, include sound-absorbing material, as well as biocompatible coatings, are described.

Reference list
  1. Endovin Yu.P., Pererva O.V., Polivanov A.N., Chekrij E.N., Levchenko A.A. Pryamoj sintez organohlorsilanov: 70 let v GNIIHTEOS [Direct synthesis organic chlorine silanes: 70 years in GNIIKHTEOS] // Himicheskaya promyshlennost'. 2015. №11. S. 6–20.
  2. Venediktova M.A., Naumov I.S., Chajkun A.M., Eliseev O.A. Sovremennye tendencii v oblasti ftorsiloksanovyh i siloksanovyh kauchukov i rezin na ih osnove (obzor) [Investigation of properties changing of serial rubber compounds on the base of different rubbers in standardized working fluids] // Aviacionnye materialy i tehnologii. 2014. №S3. S. 17–24. DOI: 10.18577/2071-9140-2014-0-S3-17-24.
  3. Kahramanov N.T., Gurbanova R.V., Kahramanly Yu.N. Sostoyanie problemy polucheniya, issledovaniya i primeneniya kremnijorganicheskih polimerov [Condition of problem of receiving, research and application of organic silicone polymers] // Evrazijskij soyuz uchenyh. 2016. №2 (27). S. 112–118.
  4. Nanushyan S.R. Kremnijorganicheskie materialy uskorennoj vulkanizacii: istoriya sozdaniya i razvitiya napravleniya [Organic silicon materials of the accelerated curing: history of creation and direction development] // Himicheskaya promyshlennost segodnya. 2015. №11. S. 21–26.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N., Startsev V.O., Inozemtsev A.A. Vlagonasyshhenie konstruktivno-podobnyh elementov iz polimernyh kompozicionnyh materialov v otkrytyh klimaticheskih usloviyah s nalozheniem termociklov [The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  7. Kablov E.N., Semenova L.V., Es'kov A.A., Lebedeva T.A. Kompleksnye sistemy lakokrasochnyh pokrytij dlya zashhity metallicheskih polimernyh kompozicionnyh materialov, a takzhe ih kontaktnyh soedinenij ot vozdejstviya agressivnyh faktorov [Complex systems of paint coatings for protection of metal polymeric composite materials, and also their contact joints against influence of aggressive factors] // Lakokrasochnye materialy i ih primenenie. 2016. №6. S. 32–35.
  8. Eskov A.A., Lebedeva T.A., Belova M.V. Lakokrasochnye materialy s ponizhennym soderzhaniem letuchih veshhestv (obzor) [Paint-and-lacquer materials with lowered content of volatile organic compounds (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 08. Available at: http://www.viam-works.ru (accessed: June 04, 2017). DOI: 10.18577/2307-6046-2015-0-6-8-8.
  9. Suhareva K.V., Andriasyan Yu.O., Mihajlov I.A., Popov A.A. Zashhitnye pokrytiya na osnove sinteticheskih kauchukov [Protecting covers on the basis of synthetic rubbers] // Plasticheskie massy. 2015. №11–12. S. 57–63.
  10. Savenkova A.V., Chursova L.V., Eliseev O.A., Glazov P.A. Germetiki aviacionnogo naznacheniya [Hermetics of aviation assignment] // Aviacionnye materialy i tehnologii. 2012. №3. S. 40–43.
  11. Minasyan R.M., Polivanov A.N., Minasyan O.I. Osnovnye napravleniya rabot GNIIHTEOS v oblasti kremnijorganicheskih kleev-germetikov [The main directions of works GNIIKHTEOS in the field of organic silicon glues-hermetics] // Himicheskaya promyshlennost segodnya. 2015. №11. S. 28–32.
  12. Krasnov L.L., Eliseev O.A., Kirina Z.V., Venediktova M.A., Rogovickij V.A. Issledovanie i modifikaciya termostojkogo germetiziruyushhego sostava i razrabotka tehnologii izgotovleniya lentochnogo germetika na ego osnove [Research and modification of the heat-resistant sealing composition and the development of manufacturing technology of the tape sealant based on it] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4 (52). St. 08. Available at: http://www.viam-works.ru (accessed: June 04, 2017). DOI: 1018577/2307-6046-2017-0-4-8-8.
  13. Chigorina T.M. Novye sshivayushhie agenty dlya kremnijorganicheskih kompozicij [New sewing agents for organic silicon compositions] // Aktualnye problemy himii, biologii i biotehnologii: mater. H Vseros. nauch. konf. Vladikavkaz, 2016. S. 247–249.
  14. Nejolova O.V. Kremnijorganicheskaya kompoziciya dlya zashhity izdelij elektronnoj tehniki s povyshennymi adgezionnymi svojstvami i termo- i morozostojkostyu pokrytij [Organic silicon composition for protection of products of electronic equipment with the increased adhesive properties both thermo- and frost resistance of coverings] // Izvestiya vysshih uchebnyh zavedenij. Ser.: Himiya i himicheskaya tehnologiya. 2014. T. 57. №9. S. 86–92.
  15. Nejolova O.V., Gazzaeva R.A., Koblova L.B. Zashhitnye pokrytiya na osnove kremnijorganicheskih lestnichnyh blok-sopolimerov, primenyaemye v mikroelektronike [Protecting covers on the basis of the organic silicon ladder block copolymers, applied in microelectronics] // Fundamentalnye issledovaniya. 2016. №2–1. S. 76–80.
  16. Horoshavina Yu.V., Francuzova Yu.V., Nikolaev G.A. Svojstva vulkanizatov na osnove polifenilsilseskvioksanpolidimetilsiloksanovogo blok-sopolimera [Properties of cured stocks on basis polyphenylsilsexvyoxanpolydimetilsiloxane block copolymer] // Kauchuk i rezina. 2015. №1. S. 10–11.
  17. Alifanov E.V., Chajkun A.M., Naumov I.S., Eliseev O.A. Elastomernye materialy povyshennoj teplostojkosti (obzor) [Elastomeric materials with high heat resistance (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №2 (50). St. 06. Available at: http://www.viam-works.ru (accessed: June 04, 2017). DOI: 10.18577/2307-6046-2017-0-2-6-6.
  18. Kopylov V.M., Kovyazin V.A., Kostyleva E.I., Fedorov A.Yu., Kovyazin A.V. Termostabilizaciya i keramoobrazovanie silikonovyh rezin [Thermostabilization and ceramic formation of silicone rubbers] // Kauchuk i rezina. 2015. №5. S. 52–59.
  19. Minasyan R.M., Polivanov A.N., Minasyan O.I. Puti povysheniya termostojkosti kremnijorganicheskih elastomernyh materialov [Ways of increase of thermal stability of organic silicon elastomeric materials] // Klei. Germetiki, tehnologii. 2015. №7. S. 24–26.
  20. Krasnov L.L., Kirina Z.V., Eliseev O.A., Menshutina N.V. Bezusadochnyj penoteplozashhitnyj material FKM-S-1B [Non-shrinkable foam protection material FKM-S-1B] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №6. S. 19–24.
  21. Shajdurova G.I., Vasilev I.L., Karmanova L.I. Razrabotka i podtverzhdenie rabotosposobnosti remontnogo sostava dlya naruzhnogo teplozashhitnogo pokrytiya [Development and confirmation of operability of repair structure for outer heat-protective coating] // Vestnik PNIPU. Aerokosmicheskaya tehnika. 2014. №36. S. 49–63.
  22. Volkov D.P., Egorov A.G., Mironenko M.E. Teplofizicheskie svojstva polimernyh kompozicionnyh materialov [Heatphysical properties of polymeric composite materials] // Nauchno-tehnicheskij vestnik informacionnyh tehnologij, mehaniki i optiki. 2017. T. 17. №2. S. 287–293.
  23. Lyubchenko O.D. Razrabotka sovremennyh materialov dlya endoprotezirovaniya [Development of modern materials for endo prosthetics] // Actualscience. 2016. T. 2. №7. S. 5–6.
  24. Shirokova E.S., Vesnin R.L., Husainov A.D. Materialy na osnove termoelastoplastov dlya primeneniya v medicine i farmacevticheskoj promyshlennosti [Materials on the basis of thermoelastoplastics for application in medicine and pharmaceutical industry] // Vestnik tehnologicheskogo universiteta. 2016. T. 19. №11. S. 106–110.
  25. Dudarikov S.A., Emec A.N., Sharofeev A.N. I dr. Endoprotezirovanie melkih sustavov kisti i stopy [Endo prosthetics of small joints of brush and foot] // Amurskij medicinskij zhurnal. 2015. №4 (12). S. 196–198.
  26. Sevostyanov M.A., Baikin A.S., Nasakina E.O., Leonov A.V., Kaplan M.A., Kraev I.D., Kolmakov A.G. Issledovanie mehanicheskih svojstv polimernyh plenok dlya medicinskih izdelij [Research of mechanical properties of polymer films for medical products] // XX Mendeleevskij sezd po obshhej i prikladnoj himii. M., 2016. S. 366. 27. Sevostyanov M.A., Sergienko K.V., Konushkin S.V., Kraev I.D., Kolmakov A.G. Nanesenie biostabilnogo polimernogo pokrytiya na nikelid titana dlya medicinskih izdelij [Drawing biostable polymer coating on nikelid titanium for medical products] // XX Mendeleevskij sezd po obshhej i prikladnoj himii. M., 2016. S. 85.
  27. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  28. Chuhlanov V.Yu., Kriushenko S.S. Tonkoslojnye pokrytiya na osnove vysokonapolnennyh sintaktnyh penoplastatov s siloksanovym svyazuyushhim [Thin layer coverings on the basis of high-filled syntactic foam with the siloxane binding // Himicheskaya promyshlennost' segodnya. 2014. №7. S. 44–51.
  29. Klyushnikov S.A., Kochetkov A.I., Morozova M.R. Optimizaciya sostava dispersnoj fazy dlya sozdaniya termostojkih i vysokoprochnyh kompozitov na osnove polimetilsiloksanovoj smoly [Optimization of structure of disperse phase for creation of heat-resistant and high-strength composites on the basis of polymethylsiloxane pitch] // Uspehi v himii i himicheskoj tehnologii. 2016. T. HHH. №10. S. 34–36.
  30. Davydova I.F., Kavun N.S. Plenochnye kremnijorganicheskie svyazuyushhie dlya stekloplastikov [Film silicon organosilicon resins for glassfibers] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 15–18. DOI: 10.18577/2071-9140-2014-0-s2-15-18.
  31. Chuhlanov V.Yu., Selivanov O.G. Issledovanie dielektricheskih svojstv sintakticheskih pen na osnove kremnijorganicheskogo svyazuyushhego [Research of dielectric properties of syntactic foams on the basis of the organic silicon binding] // Mezhdunarodnyj zhurnal prikladnyh i fundamental'nyh issledovanij. 2014. №8–1. S. 26–29.
  32. Mihajlov V.A. Sintaktnye materialy s vysokimi dielektricheskimi svojstvami na osnove kremnijorganicheskogo polimera [Syntactic materials with high dielectric properties on the basis of organosilicon polymer] // Himicheskie nauki. 2015. №12. S. 47–50.
  33. Kraev I.D., Govorov V.A., Popkov O.V., Filonova E.V., Shuldeshov E.M., Yurkov G.Yu. Poluchenie tonkodispersnyh poroshkov ferrita nikelya NiFe2O4 metodom vysokoenergeticheskogo pomola na bisernoj melnice zamknutogo kontura [Production of nickel ferrite (NiFe2O4) superfine powders by high energy milling in a closed loop bead mill] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 24–30. DOI: 10.18577/2071-9140-2017-0-2-24-30.
  34. Shuldeshov E.M., Platonov M.M. Zvukopogloshhayushhij material s rasshirennym chastotnym diapazonom effektivnogo pogloshheniya dlya perspektivnyh dvigatelnyh ustanovok [Sound-proof material with expanded frequency range of effective absorption for perspective propulsion units] // Sb. dokl. konf. «Funkcional'nye materialy dlya snizheniya aviacionnogo shuma v salone i na mestnosti». M.: VIAM, 2015. St. 12.
  35. Polimernyj zvukopogloshhayushhij material i sposob ego izgotovleniya: pat. 2612674 Ros. Federaciya [Polymeric sound-proof material and way of its manufacturing: pat. 2612674 Rus. Federation]; opubl. 13.03.17.