Calculation of benchmark X-ray diffraction intensities for α- and β-phases in titanium alloys

Panin P.V., Dzunovich D.А., Lukinа E.A.
Panin P.V., Dzunovich D.А., Lukinа E.A. Calculation of benchmark X-ray diffraction intensities for α- and β-phases in titanium alloys // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-4-4. URL: https://www.viam-works.ru/en/journal/2017/12/4
Keywords
titanium alloys, X-ray diffraction analysis, crystallographic texture, benchmark integral intensity.
Abstract

Benchmark X-ray diffraction intensities for α- and β-phases in titanium alloys have been improved with the help of polycrystalline samples of α-alloy VT1-0 and β-alloy Ti–3Al–7Mo–5,5Cr (% wt.). In order to achieve statistically significant data for each sample the corresponding X-ray diffraction patterns have been obtained in four different non-orthogonal macroplanes. Theoretical calculation of specific integral diffraction intensities for h.c.p. and f.c.c. lattices of α- and β-phases has been accomplished in accordance with kinematic theory. As a result a number of averaged normalized diffraction intensities for α- and β-phases have been obtained, the intensities being suitable for direct use in quantitative phase and texture analysis of various titanium alloys.

Reference list
  1. Kablov E.N. Iz chego sdelat' budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  2. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauchno-informacionnyh materialov. 3-e izd., pererab. i dop. [Tendencies and reference points of innovative development of Russia: collection fo scientific information materials. 3rd ed., rev. and add.]. M.: VIAM, 2015. 720 s.
  3. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  4. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  5. Kablov E.N. Materialy dlya aviakosmicheskoj tehniki [Materials for aerospace equipment] // Vse materialy. Enciklopedicheskij spravochnik. 2007. №5. S. 7–27.
  6. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  7. Nochovnaya N.A. Perspektivy i problemy primeneniya titanovyh splavov [Perspectives and problems of application of titanium alloys] // Aviacionnye materialy i tehnologii. 2007. №1. S. 4–8.
  8. Petuhov A.N. Aktualnye voprosy konstrukcionnoj prochnosti titanovyh splavov i detalej iz nih [Topical issues of constructional durability of titanium alloys and details from them] // Aviacionnye materialy i tehnologii.2007. №1. S. 8–13.
  9. Vasserman G., Greven I. Tekstury metallicheskih materialov [Structures of metal materials]. M.: Metallurgiya, 1969. 654 s.
  10. Vishnyakov Ya.D., Babareko A.A., Vladimirov S.A., Egiz I.V. Teoriya obrazovaniya tekstur v metallah i splavah [The theory of formation of structures in metals and alloys]. M.: Nauka, 1979. 343 s.
  11. Borodkina M.M., Spektor E.N. Rentgenograficheskij analiz tekstury metallov i splavov [Radiographic analysis of structure of metals and alloys]. M.: Metallurgiya, 1981. 272 s.
  12. Gorelik S.S., Skakov Yu.A., Rastorguev L.N. Rentgenograficheskij i elektronno-opticheskij analiz: ucheb. posobie dlya vuzov. 3-e izd., pererab. i dop. [Radiographic and electron-optical analysis: the manual for higher education institutions. 3rd ed., rev. and add.]. M.: MISiS, 1994. 328 s.
  13. Smirnov V.S., Durnev V.D. Teksturoobrazovanie metallov pri prokatke [Structure formation of metals when rolling]. M.: Metallurgiya, 1971. 254 s.
  14. Skvorcova S.V., Ilin A.A., Becofen S.Ya., Filatov A.A., Dzunovich D.A., Panin P.V. Anizotropiya mehanicheskih svojstv i tekstura listovyh polufabrikatov iz titanovyh splavov [Anisotropy of mechanical properties and structure of sheet semi-finished products from titanium alloys] // Tehnologiya legkih splavov. 2006. №1–2. S. 81–87.
  15. Murty K.L., Charit I. Texture development and anisotropic deformation of zircaloys // Progress in nuclear energy. 2006. Vol. 48. P. 325–359.
  16. Zaharchenko I.G., Volchok N.A., Bryuhanov P.A., Sovkova T.S. Vliyanie kombinacii pryamoj i poperechnoj prokatok na teksturu i anizotropiyu svojstv listov α-titanovogo splava
  17. Ti–3Al–1,5V [Influence of combination of direct and cross rollings on structure and anisotropy of properties of sheets α-титанового alloy Ti–3Al–1,5V] // Novi materiali i tehnologii v metalurgii ta mashinobuduvanni. 2010. №1. S. 93–98.
  18. Panin P.V. Kristallograficheskaya tekstura i anizotropiya uprugih svojstv splavov na osnove alyuminidov titana [Crystallographic structure and anisotropy of elastic properties of alloys on the basis of titanium aluminides] // Sb. materialov V Mezhdunarodnoj konferencii «Deformaciya i razrushenie materialov i nanomaterialov» (26–29 noyab. 2013 g.). M.: IMET RAN. 2013. S. 341–342.
  19. Skvorcova S.V. Zakonomernosti formirovaniya tekstury v titanovyh splavah raznyh klassov [Patterns of forming of structure in titanium alloys of different classes] // Aviacionnye materialy i tehnologii., 2007. №1. S. 40–42.
  20. Skvorcova S.V., Dzunovich D.A., Panin P.V., Snegireva L.A. Teksturoobrazovanie v listovyh polufabrikatah titanovogo splava VT16 pri plasticheskoj deformacii i termicheskoj obrabotke [Structure forming in sheet semi-finished products of BT16 titanium alloy at plastic strain and thermal processing] // Aviacionnaya promyshlennost. 2007. №4. S. 25–29.
  21. Ilin A.A., Skvorcova S.V., Dzunovich D.A., Panin P.V., Shalin A.V. Vliyanie parametrov termicheskoj i termomehanicheskoj obrabotki na teksturoobrazovanie v listovyh polufabrikatah iz titanovyh splavov [Influence of parameters of thermal and thermomechanical processing on structure forming in sheet semi-finished products from titanium alloys] // Tehnologiya mashinostroeniya. 2012. №8. S. 8–12.
  22. Dzunovich D.A., Shalin A.V., Panin P.V. Struktura, tekstura i mehanicheskie svojstva deformirovannyh polufabrikatov iz splava VT6, poluchennyh po promyshlennym i opytnym tehnologiyam [Structure, structure and mechanical properties of the deformed semi-finished products from alloy of BT6 received on industrial and pilot technologies] // Deformaciya i razrushenie materialov. 2017. №6. S. 19–27.
  23. Kolachev B.A., Becofen S.Ya., Bunin S.Ya., Volodin V.A. Fiziko-mehanicheskie svojstva legkih konstrukcionnyh materialov [Physicomechanical properties of light constructional materials]. M.: Metallurgiya, 1995. 442 s.
  24. Vozdvizhenskij V.M., Zhukov A.A., Postnova A.D., Vozdvizhenskaya M.V. Splavy cvetnyh metallov dlya aviacionnoj tehniki [Non-ferrous alloys for aviation engineering]. Rybinsk: RGATA, 2002. 219 s.
  25. Grytsyna V., Stukalov A., Chernyaeva T. et al. Destruction of crystallographic texture in zirconium alloy tubes // Proceedings of 14th International Symposium «Zirconium in the Nuclear Industry». ASTM, 2005. Vol. 2. No. 8. Р. 305–329.
  26. Vanitha C., Kiran Kumar M., Dey G.K. et al. Recrystallization texture development in single-phase Zircaloy-2 // Materials Science and Engineering: A. 2009. Vol. 519. P. 51–60.
  27. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  28. Ageev N.V., Babareko A.A., Becofen S.Ya. Opisanie tekstury metodom obratnyh polyusnyh figure [Structure description method of return polar figures] // Izvestiya AN SSSR. Ser.: Metally. 1974. №1. S. 94–103.
  29. Rusakov A.A. Rentgenografiya metallov [X-ray graphic of metals]. M.: Atomizdat, 1977. 479 s.
  30. Van Houtte P.A. New Method for the determination of texture functions from incomplete pole figures – comparison with older methods // Gordon and British Science Publishers Inc. «Textures and Microstructures». 1984. Vol. 6. P. 137–162.
  31. Dahms M., Bunge H.J. ODF calculation by series expansion from incompletely measured pole figures using positivity condition // Gordon and British Science Publishers Inc. «Textures and Microstructures». 1987. Vol. 7. P. 171–185.
  32. Kearns J.J. On the relationship among «f» texture factors for the principal planes of zirconium, hafnium and titanium alloys // Journal of Nuclear Materials. 2001. No. 299. Р. 171–174.
  33. Becofen S.Ya., Smirnov V.G., Ashmarin A.A., Shaforostov A.A. Kolichestvennye metody opisaniya tekstury i anizotropii svojstv splavov na osnove titana i magniya [Quantitative methods of the description of structure and anisotropy of properties of titanium-based alloys and magnesium ] // Titan. 2010. №2. S. 16–22.
  34. Mani Krishna K.V., Srivastava D., Dey G.K. et al. Comparative study of methods of the determination of Kearns parameter in zirconium // Journal of Nuclear Materials. 2011. No. 414. Р. 492–497.
  35. Dzunovich D.A., Becofen S.Ya., Panin P.V. Metodicheskie aspekty kolichestvennogo teksturnogo analiza listovyh polufabrikatov iz GPU-splavov (Ti, Zr) [Methodical aspects of the quantitative textural analysis of sheet semi-finished products from GPU-splavov (Ti, Zr)] // Deformaciya i razrushenie materialov. 2016. №11. S. 8–16.
  36. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  37. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  38. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation are the base of innovations, technological leadership and national security of Russia] // Intellekt i tehnologii. 2016. №2 (14). S. 16–21.
  39. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] // Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.