Features of thermal processing of composite materials with the aluminium matrix (review)

Kurbatkina E.I., Shavnev A.A., Kosolapov D.V., Gololobov A.V.
Kurbatkina E.I., Shavnev A.A., Kosolapov D.V., Gololobov A.V. Features of thermal processing of composite materials with the aluminium matrix (review) // Proceedings of VIAM. 2017. No. 11. DOI: 10.18577/2307-6046-2017-0-11-9-9. URL: https://www.viam-works.ru/en/journal/2017/11/9
Keywords
mechanical alloying, composite materials, solid-phase interaction.
Abstract

In this article, main features of the dispersion hardening of metal composite materials (MМС) based on an aluminum matrix were considered using the example of the Al–Cu–Mg–SiC, Al–Mg–Si–Cu–SiC, Al–Mg–Si–Cu–B4C and Al–Zn–Mg–Cu–SiC systems. It was shown that the aging kinetics of MMC differs from the aging kinetics of aluminum alloys: hardness and strength of MMC reach their maximum values in a shorter time. The effect of the volume fraction of the reinforcing component on the dispersion hardening of composite materials was analyzed. Рhase composition and features of the interaction at the matrix/reinforcement interface were studied.

Reference list
  1. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizatsii v resursosberegayushchej tehnologii proizvodstva detalej GTD [Role of the directed crystallization in the resource-saving production technology of details of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 01. Available at: http://www.viam-works.ru (accessed: September 17, 2017).
  2. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Vliyanie termicheskoj obrabotki na harakteristiki svarnyh soedinenij vysokoprochnyh alyuminijlitievyh splavov [Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 06. Available at: http://www.viam-works.ru (accessed: September 18, 2017). DOI: 10.18577/2307-6046-2015-0-4-6-6.
  3. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
  4. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 20–26.
  5. Aviacionnye materialy i tehnologii [Aviation materials and technologies] / pod obshh. red. E.N. Kablova. 2017. №S. S. 11–16.
  6. Chawla N., Shen Y.-L. Mechanical Behavior of Particle Reinforced Metal Matrix Composites // Advanced Engineering Materials. 2001. Vol. 3. No. 6. Р. 357–429.
  7. Davis L.C., Allison J.E. Residual stresses and their effects on deformation // Metallurgical Transactions: A. 1993. Vol. 24. No. 11. Р. 2487–2496.
  8. Vogelsang M., Arsenault R.J., Fisher R.M. An in situ HVEM study of dislocation generation at Al/SiC interfaces in metal matrix composites // Metallurgical Transactions: A. 1986. Vol. 17. No. 3. Р. 379–389.
  9. Arsenault R.J., Wu S.B. A comparison of PM vs. melted SiC/Al composites // Scripta Metallurgica. 1988. Vol. 22. No. 6. P. 767–772.
  10. Ganesh V.V., Chawla N. Effect of particle orientation anisotropy on the tensile behavior of metal matrix composites: experiments and microstructure-based simulation // Materials Science and Engineering: A. 2005. Vol. 391. No. 1–2. P. 342–353.
  11. Serpova V.M., Shavnev A.A., Grishina O.I., Krasnov E.I., Solyaev Yu.O. Smachivaemost' i mezhfaznoe vzaimodejstvie v metallicheskom kompozicionnom materiale na alyuminievoj matrice, armirovannoj oksidom alyuminiya [Wettability and interphase interaction in metal composite material on the aluminum matrix reinforced by aluminum oxide] // Materialovedenie. 2014. №12. S. 29–35.
  12. Sidorov D.V., Shherbakova G.I. Vysokotehnologichnye komponenty kompozicionnyh materialov i specialnye volokna dlya shirokogo spektra primeneniya [Hi-tech components of composite materials and special fibers for application broad spectrum] // Himicheskaya tehnologiya. 2016. T. 17. №4. S. 183–192.
  13. Polmear I.J. Light Alloys: Metallurgy of the Light Metals, John Wiley & Sons, Australia, 1995. 496 p.
  14. Papazian J.M. Effects of SiC whiskers and particles on precipitation in aluminum matrix composites // Metallurgical Transactions: A. 1988. Vol. 19. No. 12. P. 2945–2953.
  15. Oguocha I.N.A., Yannacopoulos S. Precipitation and dissolution kinetics in Al–Cu–Mg–Fe–Ni alloy 2618 and Al–alumina particle metal matrix composite // Materials Science and Engineering: A. 1997. Vol. 231. No 1–2. P. 25–33.
  16. Badini C., Marino F., Verné E. Calorimetric study on precipitation path in 2024 alloy and its SiC composite // Materials Science and Engineering: A. 1995. Vol. 191. No. 1–2. P. 185–191.
  17. Cottu J.-P., Couderc J.-J., Viguier B., Bernard L. Influence of SiC reinforcement on precipitation and hardening of a metal matrix composite // Journal of Materials Science. 1992. Vol. 27. No. 11. P. 3068–3074.
  18. Hunt E., Pitcher P.D., Gregson P.J. Precipitation reactions in 8090 SiC particulate reinforced MMC // Scripta Metallurgica et Materialia. 1990. Vol. 24l. No. 5. P. 937–941.
  19. Hadianfard M.J., Mai Y.-W., Healy J.C. Effect of ceramic reinforcement on the ageing behaviour of an aluminium alloy // Journal of Materials Science. 1993. Vol. 28. No. 13. P. 3665–3669.
  20. Oguocha I.N.A. Characterization of Aluminum Alloy 2618 and its Composites Containing Alumina Particles: thesis, PhD. Ottawa: Department of Mechanical Engineering University of Saskatchewan, 1998. 200 p.
  21. Choi H.J., Min B.H., Shin J.H., Bae D.H. Strengthening in nanostructured 2024 aluminum alloy and its composites containing carbon nanotubes // Composites Part A: Applied Science and Manufacturing. 2011. Vol. 42. No. 10. P. 1438–1444.
  22. Lin G., Zhen-zhu Z., Gui-song W., Bin X.U. Effect of aging treatment on mechanical properties of (SiCw & SiCp)/2024Al hybrid nanocomposites // Transactions of Nonferrous Metals Society of China. 2005. Vol. 16. P. 387–391.
  23. Saheb N., Khalil A., Hakeem A.S., Laoui T. Age Hardening Behavior of Carbon Nanotube Reinforced Aluminum Nanocomposites // Journal of Nano Research. 2013. Vol. 21. P. 29–35.
  24. Oguocha I.N.A., Yannacopoulos S. Natural ageing behaviour of cast alumina particle-reinforced 2618 aluminium alloy // Journal of Materials Science. 1996. Vol. 31. No. 12. P. 3145–3151.
  25. Gribkov A.N., Aksenov A.A., Zhezher M.V., Zolotorevskij V.S. Struktura i svojstva dispersnouprochnennogo kompozicionnogo materiala Al–3%Cu–1%Mg–20%SiC, poluchaemogo metodom mehanicheskogo legirovaniya [Structure and properties of the dispersnouprochnenny Al-3%Cu–1%Mg–20%SiC composite material received by method of mechanical alloying] // Tehnologiya legkih splavov. 1994. №3–4. S. 36–42.
  26. Lee H.-L., Lu W.-H., Chan L.-I. Aging behavior of powder metallurgy composite // Scripta Metallurgica et Materialla. 1992. Vol. 26. P. 1723–1726.
  27. Pal S., Mitra R., Bhanuprasad V.V. Aging behavior of Al–Cu–Mg alloy–SiC composites // Materials Science and Engineering A. 2008. Vol. 480. P. 496–505.
  28. Wang Z., Li C., Wang H., Zhu X., Wu M. Aging Behavior of Nano-SiC/2014Al Composite Fabricated by Powder Metallurgy and Hot Extrusion Techniques // Journal of Materials Science & Technology. 2016. Vol. 32. No. 10. P. 1008–1012.
  29. Hayoune A., Hamana D. Structural evolution during non-isothermal ageing of a dilute Al–Cu alloy by dilatometric analysis // Journal of Alloys and Compounds. 2009. Vol. 474. No. 1–2. P. 118–123.
  30. Wang L.M., Flower H.M., Lindley T.C. Precipitation of the ω phase in 2024 and 2124 aluminum alloys // Scripta Materialia. 1999. Vol. 41. No. 4. P. 391–396.
  31. Gouma P.I., Lloyd D.J., Mills M.J. Precipitation processes in Al–M–Cu alloys // Materials Science and Engineering: A. 2001. Vol. 319–321. P. 439–442.
  32. Guo J., Yuan X. The aging behavior of SiC/Gr/6013Al composite in T4 and T6 treatments // Materials Science and Engineering: A. 2009. Vol. 499. No. 1–2. P. 212–214.
  33. Liu P., Wang A., Xie J., Hao S. Characterization and evaluation of interface in SiCp/2024 Al composite // Transactions of Nonferrous Metals Society of China. 2015. Vol. 25. P. 1410–1418.
  34. He Y., Wang N., Qiao B., Feng L., Chen Z. SiC/Al interface feature of Al–Fe–V–Si alloy reinforced with SiC particles // The Chinese Journal of Nonferrous Metals. 2010. Vol. 20. No. 7. Р. 1302–1308.
  35. Zhang S., Cui Y., Song Y. Microstructural study of SiCp/Al composite prepared by pressureless infiltration // Journal of Materials Engineering. 2000. Vol. 10. P. 3−7.
  36. Cheng N., Zeng S., Liu Z. Рreparation, microstructures and deformation behavior of SiCp/6066 Al composites produced by PM route // Journal of Materials Processing Technology. 2008. Vol. 202. No. 1–3. P. 27–40.
  37. Li B., Luo B., He K., Zeng L., Fan W., Bai Z. Effect of aging on interface characteristics of
  38. Al–Mg–Si/SiC composites // Journal of Alloys and Compounds. 2015. Vol. 649. P. 495–499.
  39. Li Y.Z., Wang Q.Z., Wang W.G., Xiao B.L., Ma Z.Y. Effect of interfacial reaction on age-hardening ability of B4C/6061Al composites // Materials Science & Engineering: A. 2015. Vol. 620. P. 445–53.
  40. Bhaduri A., Gopinathan V., Ramakrishnan P., Miodownik A.P. Processing and properties of SiC particulate reinforced Al–6,2Zn–2,5Mg–1,7Cu alloy (7010) matrix composites prepared by mechanical alloying // Materials Science and Engineering A. 1996. Vol. 221. P. 94–101.
  41. Yuan W., An B. Effect of heat treatment on microstructure and mechanical property of extruded 7090/SiCp composite // Transactions of Nonferrous Metals Society of China. 2012. Vol. 22. P. 2080–2086.
  42. Chen K.H., Liu H.W., Liu Y.Z. The effect of promotively-solutionizing treatment on the mechanical properties and fracture of ultra high strength 7055 aluminum alloys // Journal of Central South University of Technology. 2002. Vol. 31. P. 528–531.
  43. Wang F., Xiong B.Q., Zhang Y.G. Age-hardening characteristic of an Al–Zn–Mg–Cu alloy produced by spray deposition // Rare Metals. 2007. Vol. 26. P. 163–168.
  44. Ludtka G.M., Laughlin D.E. The influence of microstructure and strength on the fracture mode and toughness of 7xxx series aluminum alloys // Metallurgical Transactions 1982. Vol. 13A. P. 411–418.
  45. Bruce M., Claire M., Ravi S. The influence of Al3Zr dispersoids on the recrystallization of hot-deformed AA7010 alloys // Metallurgical and Materials Transactions A. 2001. Vol. 32.P. 625–632.
  46. Sahin A., Sarioglu F. Effect of reinforcement on precipitation behavior in Al 7075/TiCp composite // Scripta Materialia. 1997. Vol. 37. P. 1117–1121.