Production of metal-powder high-purity titanium alloy compositions by induction gas atomization for application in additive manufacturing

Alishin M.I., Knyazev A. E.
Alishin M.I., Knyazev A. E. Production of metal-powder high-purity titanium alloy compositions by induction gas atomization for application in additive manufacturing // Proceedings of VIAM. 2017. No. 11. DOI: 10.18577/2307-6046-2017-0-11-5-5. URL: https://www.viam-works.ru/en/journal/2017/11/5
Keywords
additive manufacturing, metal-powder compositions, titanium alloy powder, Ti-4-6 and VT20 alloy, induction gas atomization, centrifugal disintegration, EIGA-method, crucibleless melting.
Abstract

The issue of production of high-purity metal-powder compositions (powder) of titanium alloys by the method of induction gas atomization is reviewed in the article. With this method of production of titanium powders required technological properties and granulometric composition are improved with low content of gas impurities, which meets the requirements for raw materials for additive technologies. In FSUE «VIAM» the VIPiGR 50/500 unit operated with the method of induction gas atomization and allowing to obtain titanium powders with a low content of oxygen impurities (not more than 0,15% by weight) and hydrogen (not more than 0,01% by weight) was installed and commissioned in operation. The main characteristics of metal powder complexes from alloys of high-purity Ti-4-6 and VT20 obtained on the unit are presented.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  3. Kablov E.N. Materialy i tehnologii VIAM v konstrukciyah perspektivnyh dvigatelej razrabotki OAO «Aviadvigatel» [Materials and VIAM technologies in designs of perspective engines of development of JSC Aviadvigatel] // Permskie aviacionnye dvigateli: inform. byul. 2014. №31. S. 43–47.
  4. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  5. Kablov E.N., Petrushin N.V., Svetlov I.L. Sovremennye litye nikelevye zharoprochnye splavy [Modern cast nickel hot strength alloys] // Tr. Mezhdunar. nauch.-tehnich. konf. «Nauchnye idei S.T. Kishkina i sovremennoe materialovedenie». M.: VIAM, 2006. S. 39–55.
  6. Inozemcev A.A., Bashkatov I.G., Koryavcev A.S. Titanovye splavy v izdeliyah razrabotki OAO «Aviadvigatel» [Titanium alloys in products of development of JSC «Aviadvigatel»] // Sovremennye titanovye splavy i problemy ih razvitiya. M.: VIAM, 2010. S. 43–46.
  7. Sirotkin O.S. Sovremennoe sostoyanie i perspektivy razvitiya additivnyh tehnologij [Current state and perspectives of development of the additive technologies] // Aviacionnaya promyshlennost. 2015. №2. S. 22–25.
  8. Gasser А., Backes G., Kelbassa I., Weisheit A., Wissenbach K. Laser Additive Manufacturing. Laser Metal Deposition (LMD) and Selective Laser Melting (SLM) in Turbo-Engine Application // Laser Technik Journal. 2010. Vol. 7. P. 58–63. DOI: 10.1002/latj.201090029.
  9. Kablov E.N. Poroshki izbavlyayut ot lishnego: intervyu [Powders relieve of the superfluous: interview] // Ekspert. 2014. №9. S 46–51.
  10. Belov S.V., Volkov S.A., Magerramova L.A. Perspektivy primeneniya additivnyh tehnologij v proizvodstve slozhnyh detalej gazoturbinnyh dvigatelej iz metallicheskih materialov [Perspectives of application of the additive technologies in production of difficult details of gas turbine engines from metal materials] // Sb. dokl. konf. «Additivnye tehnologii v rossijskoj promyshlennosti». M.: VIAM, 2015. S. 21–28.
  11. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 20–26.
  12. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  13. Kablov E.N., Evgenov A.G., Rylnikov V.S., Afanasev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev dlya diffuzionnoj vakuumnoj pajki, poluchennyh metodom atomizacii rasplava [Research of finely divided powders of solders for the diffusion vacuum soldering, received by atomization method melt] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 79–87.
  14. Logacheva A.I. Kompleksnaya tehnologiya izgotovleniya tonkostennyh elementov metodom poroshkovoj metallurgii dlya proizvodstva detalej iz konstrukcionnyh i funkcionalnyh splavov na osnove titana i nikelya dlya izdelij raketno-kosmicheskoj tehniki: dis. … dokt. tehn. nauk [Complex manufacturing techniques of thin-walled elements method of powder metallurgy for production of details from constructional and functional titanium-based alloys and nickel for products of space-rocket equipment: thesis, Dr. Sc. (Tech.)]. Korolev, 2017. S. 33–36.
  15. Vostrikov A.V., Garibov G.S., Ber L.B., Shlyapin S.D. Issledovanie fiziko-mehanicheskih svojstv granul iz novogo vysokoprochnogo nikelevogo splava, izgotovlennyh metodom PREP [Research of physicomechanical properties of granules from the new high-strength nickel alloy, made by the PREP method] // Tehnologiya legkih splavov. 2013. №2. S. 69–75.