Research of mechanical properties and microstructure of samples obtained by SLS from metal powder composition of VZh159 alloy
UDC
620.1:669.018.44
DOI
10.18577/2307-6046-2017-0-11-1-1
Article PDF (Russian)
(968.27 KB)
How to cite
Prager S.M., Solodova T.V., Tatarenko O.Yu. Research of mechanical properties and microstructure of samples obtained by SLS from metal powder composition of VZh159 alloy // Proceedings of VIAM. 2017. No. 11. DOI: 10.18577/2307-6046-2017-0-11-1-1. URL: https://www.viam-works.ru/en/journal/2017/11/1
Keywords
metal powder composition, selective laser sintering, heat resistance, porosity, mechanical properties.
Abstract
The article shows the research of mechanical properties of specimens obtained by SLS frommetal powder composition of VGH159 alloy after long-term exposure at working temperatures. It has been shown that strength properties don’t decrease essentially after 500-hour exposure at 900С and plasticity reduction of the material have induced by the additional precipitation of phases with Cr and Mo and y'-phase from the solid solution. The comparison of the mechanical properties with passport characteristics of EP648-PS alloy have carried out. It was shown that VZh159 alloy surpasses that alloy in tensile strength at investigated temperature diapason.
Reference list
- Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy VIAM 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
- Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii [Tendencies and reference points of innovative development of Russia]. M.: VIAM, 2015. 557 s.
- Kablov E.N., Buntushkin V.P., Morozova G.I., Bazyleva O.A. Osnovnye principy legirovaniya intermetallida Ni3Al pri sozdanii vysokotemperaturnyh splavov [The basic principles of alloying of Ni3Al intermetallic compound at creation of high-temperature alloys] // Materialovedenie. 1998. №7. S. 13–15.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] // Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Matilainen V.-P., Pekkarinen J., Salminen F. Weldability of additive manufactured stainless steel // Physics Prosedia. 2016. Vol. 83. P. 808–817.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Sufiyarov V.Sh., Popovich A.A., Borisov E.V., Polozov I.A. Selektivnoe lazernoe plavlenie zharoprochnogo nikelevogo splava [The selection laser melting of heat resisting nickel alloy] // Tsvetnye metally. 2015. №1 (865). S. 79–84.
- Gryaznov M.Yu., Shotin S.V., Chuvildeev V.N. Effekt mezostrukturnogo uprochneniya stali 316L pri poslojnom lazernom splavlenii [Effect of mesostructural hardening of steel 316L at level-by-level laser fusing] // Vestnik Nizhegorodskogo universiteta im. N.I. Lobachevskogo. 2012. №5 (1). S. 43–50.
- Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. Issledovanie svojstv splava EP648, poluchennogo metodom selektivnogo lazernogo splavleniya metallicheskih poroshkov [A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 02. Available at: http://www.viam-works.ru (accessed: October 23, 2017). DOI: 10.18577/2307-6046-2015-0-2-2-2.
- Evgenov A.G., Rogalev A.M., Karachevcev F.N., Mazalov I.S. Vliyanie goryachego izostaticheskogo pressovaniya i termicheskoj obrabotki na svojstva splava EP648, sintezirovannogo metodom selektivnogo lazernogo splavleniya [Influence of hot isostatic pressing and thermal processing on properties of alloy ЭП648 synthesized by method of the selection laser fusing] // Tehnologiya mashinostroeniya. 2015. №9. S. 11–16.
- Mostafa A., Rubio I.P., Brailovski V. et al. Structure, texture and phases in 3D printed In718 alloy subjected to homogenization and HIP treatments // Metals. 2017. Vol. 7. No. 196. P. 2–23.
- Mazalov I.S., Evgenov A.G., Prager S.M. Perspektivy primeneniya zharoprochnogo strukturnostabil'nogo splava VZh159 dlya additivnogo proizvodstva vysokotemperaturnyh detalej GTD [Perspectives of heat resistant structurally stable alloy VZh159 application for additive production of high-temperature parts of GTE] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 3–7. DOI: 10.18577/2071-9140-2016-0-S1-3-7.
- Murayama M., Katayama Y., Hono K. Microstructural Evolution in a 17-4 PH Stainless Steel after Aging at 400°C // Metallurgical and Materials Transactions A. 1999. Vol. 30A. P. 345–353.
- Nilsson J.-O., Kangas P., Karlsson T., Wilson A. Mechanical Properties, Microstructural Stability and Kinetics of σ-Phase Formation in 29Cr–6Ni–2Mo–0,38N Superduplex Stainless Steel // Metallurgical and Materials Transactions A. 2000. Vol. 31A. P. 35–45.