Physical and physico-mechanical properties of antifriction organoplastics based on combined fabric filler and epoxy binder

Kulagina G.S., Korobova A.V., Ilichev A.V., Zhelezina G.F.
Kulagina G.S., Korobova A.V., Ilichev A.V., Zhelezina G.F. Physical and physico-mechanical properties of antifriction organoplastics based on combined fabric filler and epoxy binder // Proceedings of VIAM. 2017. No. 10. DOI: 10.18577/2307-6046-2017-0-10-8-8. URL: https://www.viam-works.ru/en/journal/2017/10/8
Keywords
antifriction organoplastic, polytetrafluoroethylene fibers, polyimide fibers, epoxy binder, combined woven filler, physical and mechanical properties, strain-strain curves, modulus of elasticity, tensile strength, elongation
Abstract

An antifriction organoplastic based on epoxy binder and combined fabric filler including polytetrafluoroethylene and polyimide fibers was investigated. Data on its basic physical properties, physico-mechanical properties under uniaxial tension were obtained. The stress-strain curves were analyzed, the temperature dependences of the modulus of elasticity, strength and elongation at tension were established. Antifrictional organoplastic was a polymer composite material with 0,25–0,30 mm thickness and 1,55 g/cm3 density, has resistance to water and aviation petroleum products. It was shown that in the investigated temperature range from -40 to +60°С the organoplastic was characterized by strength of 30–110 MPa, elastic modulus of 0,7–4,5 GPa and deformations of 3–22%. According to the results of the research, antifriction organoplastics can be successfully used as a coating of a given size and shape for the modification of friction surfaces without significant weight gain and changes in t

Reference list
  1. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
  2. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. 3-e izd. [Tendencies and reference points of innovative development of Russia: collection of scientific information materials. 3rd ed.]. M.: VIAM, 2015. 720 s.
  3. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  4. Kablov E.N. Materialy dlya aviakosmicheskoj tehniki [Materials for aerospace equipment] // Vse materialy. Enciklopedicheskij spravochnik. 2007. №5. S. 7–27.
  5. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  6. Bejder E.Ya., Donskoj A.A., Zhelezina G.F., Kondrashov E.K. i dr. Opyt primeneniya ftorpolimernyh materialov v aviacionnoj tehnike [Experience of application of ftorpolimerny materials in aviation engineering] // Rossijskij himicheskij zhurnal. 2008. T. LII. №3. S. 30–44.
  7. Zhelezina G.F. Konstrukcionnye i funkcionalnye organoplastiki novogo pokoleniya [Constructional and functional organoplastics of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 06. Available at: http://www.viam-works.ru (accessed: July 03, 2017).
  8. Kulagina G.S., Korobova A.V., Zuev S.V., Zhelezina G.F. Issledovanie tribologicheskih svojstv organoplastikov na osnove tkanogo armiruyushhego napolnitelya [Study of tribological properties of organoplastics on the basis of reinforcing fabric filler] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №11. St. 06. Available at: http://www.viam-works.ru (accessed: June 02, 2017). DOI: 10.18577/2307-6046-2016-0-11-6-6.
  9. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  10. Timoshkov P.N., Hrulkov A.V. Sovremennye tehnologii pererabotki polimernyh kompozitsionnyh materialov, poluchaemyh metodom propitki rasplavnym svyazuyushchim [Modern technologies of hotmelt polymer composite materials processing] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 04. Available at: http://www.viam-works.ru (accessed: May 16, 2017). DOI: 10.18577/2307-6046-2014-0-8-4-4.
  11. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  12. Mihajlov M.M. Vlagopronicaemost organicheskih dielektrikov [Humidity permeability of organic dielectrics]. M.: Gosenergizdat, 1961. 163 s.
  13. Perepelkin K.E. Himicheskie volokna: razvitie proizvodstva, metody polucheniya, svojstva, perspektivy [Chemical fibers: production development, methods of receiving, property, perspective]. SPb.: SPGUTD, 2008. 354 s.
  14. Sovremennye mashinostroitelnye materialy. Nemetallicheskie materialy: spravochnik / pod obshh. red. I.V. Gorynina, A.S. Oryshhenko [Modern machine-building materials. Non-metallic materials: directory / gen ed. by I.V. Gorynin, A.S. Oryshhenko]. SPb.: Professional, 2012. 916 s.
  15. Available at: http://www.lirsot.ru (accessed: March 01, 2017).
  16. Eshbi M., Dzhons D. Konstrukcionnye materialy. Polnyj kurs [Constructional materials. Full course]. Dolgoprudnyj: Intellekt, 2010. 672 s.
  17. Mihajlin Yu.A. Konstrukcionnye polimernye kompozicionnye materialy. 2-e izd. [Constructional polymeric composite materials. 2nd ed.]. SPb.: Nauchnye osnovy i tehnologii, 2013. 822 s.
  18. Lipatov Yu.S. Mezhfaznye yavleniya v polimerah [The interphase phenomena in polymers]. Kiev: Nauk. Dumka, 1980. 260 s.
  19. Panshin Yu.A., Malkevich S.G., Dunaevskaya C.S. Ftoroplasty [Fluoropolymers]. L.: Himiya, 1978. 232 s.