Abstract

For the 2012–2015 period at FSUE «VIAM» carried out important experimental work, aimed at obtaining the strength characteristics of the single crystals with the orientation , and of the most promising Nickel-based superalloys. This work is devoted to study the anisotropic characteristics of elasticity in tension (рoisson's ratio and static modulus of elasticity) single crystal Nickel-based superalloys VZHM7 and VZHM8 with crystallographic orientations (CGO) , , in the temperature range 20–1000°C.

Reference list
  1. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Monokristallicheskie zharoprochnye nikelevye splavy dlya turbinnyh lopatok perspektivnyh GTD [Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  2. Toloraiya V.N., Kablov E.N., Demonis I.M. Tehnologiya polucheniya monokristallicheskih otlivok turbinnyh lopatok GTD zadannoj kristallograficheskoj orientacii iz renijsoderzhashhih zharoprochnyh splavov [Technology of receiving single-crystal molding of turbine blades of GTE of the set crystallographic orientation from rhenium containing hot strength alloys] // Aviacionnye materialy i tehnologii. 2004. №1. S. 107–117.
  3. Shalin R.E., Svetlov I.L., Kachanov E.B., Toloraiya V.N., Gavrilin O.S. Monokristally nikelevyh zharoprochnyh splavov [Monocrystals of nickel hot strength alloys]. M.: Mashinostroenie, 1997. 336 s.
  4. Nozhnickij Yu.A., Golubovskij E.R. Obespechenie prochnostnoj nadezhnosti monokristallicheskih rabochih lopatok vysokotemperaturnyh turbin perspektivnyh GTD [Ensuring strength reliability of single-crystal working blades of high-temperature turbines of perspective GTE] // Nauchnye idei S.T. Kishkina i sovremennoe materialovedenie: tr. mezhdunar. nauch.-tehnich. konf. M.: VIAM, 2006. S. 65–71.
  5. Miner R.V., Voigt R.S., Gayda J., Gabb T.P. Orientation and temperature dependence of some mechanical properties of the single-crystal nickel-base superalloy René N4: Part I. Tensile behavior // Metallurgical Transactions A. 1986. Vol. 17. Issue. 3. P. 491–496.
  6. Sass V., Glatzel U., Feller-Kniepmeier M. Creep anisotropy in monocrystalline nickel-base superalloy CMSX-4 // Superalloys-1996. Champion (Pennsylvania): Minerals, Metals & Materials Society. 1996. P. 283–290.
  7. Golubovskij E.R., Svetlov I.L. Temperaturno-vremennaya zavisimost' anizotropii dlitelnoj prochnosti monokristallov ZhNS [Temperature and time dependence of anisotropy of long durability of monocrystals of heat resisting nickel alloys] // Problemy prochnosti. 2002. №2. S. 5–19.
  8. Svetlov I.L., Petrushin N.V., Golubovskij E.R. i dr. Mehanicheskie svojstva monokristallov nikelevogo zharoprochnogo splava, soderzhashhego renij i rutenij [Mechanical properties of monocrystals of the nickel hot strength alloy, containing reniye and ruthenium] // Deformaciya i razrushenie materialov. 2008. №11. S. 26–35.
  9. Golubovskij E.R., Svetlov I.L., Petrushin N.V. i dr. Malociklovaya ustalost' monokristallov zharoprochnyh nikelevyh splavov pri povyshennyh temperaturah [Low-cyclic fatigue of monocrystals of heat resisting nickel alloys at elevated temperatures] // Deformaciya i razrushenie materialov. 2009. №8. S. 41–48.
  10. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  11. Petrushin N.V., Svetlov I.L., Ospennikova O.G. 1) Litejnye zharoprochnye nikelevye splavy [Cast heat resisting nickel alloys] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №5. S. 15–19; 2) Litejnye zharoprochnye nikelevye splavy [Cast heat resisting nickel alloys] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №6. S. 16–21.
  12. Petrushin N.V., Visik E.M., Gorbovec M.A., Nazarkin R.M. Strukturno-fazovye harakteristiki i mehanicheskie svojstva monokristallov zharoprochnyh nikelevyh renijsoderzhashhih splavov s intermetallidno-karbidnym uprochneniem [Structural phase characteristics and mechanical properties of monocrystals of heat resisting nickel rhenium containing alloys with intermetallic-carbide hardening] // Metally. 2016. №4. S. 57–70.
  13. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Solovyev A.E., Golynets S.A., Khvatsky K.K., Aslanyan I.R. Provedenie staticheskih ispytanij pri rastyazhenii na mashinah firmy Zwick/Roell [Performing of static tensile tests on Zwick/Roell machines] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 12. Available at: http://viam-works.ru (accessed: August 28, 2017). DOI: 10.18577/2307-6046-2015-0-8-12-12.
  15. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy, legirovannye ruteniem [The nickel hot strength alloys alloyed by ruthenium] // Aviacionnye materialy i tehnologii. 2004. №1. S. 80–90.
  16. Tolorajya V.N., Kablov E.N., Svetlov I.L., Orehov N.G., Golubovskij E.R. Anizotropiya prochnostnyh harakteristik v monokristallah nikelevyh zharoprochnyh splavov [Anisotropy of strength characteristics in monocrystals of nickel hot strength alloys] // Gornyj informacionno-analiticheskij byulleten. Tematich. prilozhenie: Funkcionalnye materialy. 2005. S. 225–236.