Role of MPСM structures and their effect on vibration fatigue characteristics of GTE constructive components

Postnova M.V., Postnov V.I.
Postnova M.V., Postnov V.I. Role of MPСM structures and their effect on vibration fatigue characteristics of GTE constructive components // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-7-7. URL: https://www.viam-works.ru/en/journal/2017/1/7
Keywords
reverser, fatigue failure, Alor D16/41, skin of engine nacelle.
Abstract

During operation of a reverser of D18T engine 32 cases of damaged skin from D16 alloy of RU-18T reverser mobile case are revealed. In order to increase in service life of this unit it has been decided to use metal-polymeric material Alor D16/41 as a skin material of internal path (crown type). For commercial introduction of metal-polymeric material Alor D16/41 into a structure of airplane manufacturing research of its properties has been conducted. The researches have shown that forming ability of layered MPCM depends on the fiber reinforcement lay-out relative to the direction of deformation Besides all known technological processes of parts forming have been developed. Since units of the reverser are subjected to vibroacoustic impact in the process of operation researches on their sound insulation have been conducted. Application of Alor D16/41 as a skin material in engine nacelle allowed reducing in weight of the structure by 10% and considerable improving of its vibration fatigue p

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aviacionnoe materialovedenie v HHI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubilejnyj nauch.-tehnich. sb. M.: MISIS–VIAM, 2002. S. 23–47.
  3. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] // Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  4. Postnova M.V., Kazakov I.A. Metallopolimernye kompozicionnye materialy – svojstva, tehnologiya formovaniya, oblasti primeneniya [Metalpolymeric composite materials – properties, technology of formation, scope] // Sloistye kompozicionnye materialy. 2001. S. 187–188.
  5. Antipov V.V. Metallicheskie materialy novogo pokoleniya dlya planera perspektivnyh izdelij aviacionno-kosmicheskoj tehniki [Metal materials of new generation for glider of perspective products of aerospace equipment] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 02. Available at: http://www.materialsnews.ru (accessed: June 08, 2016).
  6. Antipov V.V., Senatorova O.G., Sidelnikov V.V., Shestov V.V. Konstrukcionnye sloistye materialy SIAL [SIAL constructional layered materials] // Klei. Garmetiki.Tehnologii. 2012. №6. S. 41–49.
  7. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: June 08, 2016). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  8. Umanskij Ya.S. Kristallografiya, rentgenografiya i elektronnaya mikroskopiya [Crystallography, roentgenography and electron microscopy]. M.: Metallurgiya, 1982. 289 s.
  9. Myasnikov Yu.G. Rentgenovskie difraktometry dlya issledovaniya i kontrolya napryazhenno-deformirovannyh materialov [X-ray diffractometrs for research and control intense the deformed materials] // Zavodskaya laboratoriya. 1985. №7. S. 21–26.
  10. Postnov V.I., Postnova M.V., Arlashkina O.Yu. Issledovanie vliyaniya napryazhenno-deformirovannogo sostoyaniya na ustalostnye harakteristiki MPKM [Research of influence intense the deformed condition on fatigue characteristics of MPCM] // Sb. mater. Mezhdunar. nauch. konf. «Novye perspektivnye materialy i tehnologii ih polucheniya–2010». Volgograd: VolGTU, 2010. S. 183–185.
  11. Postnov V.I., Postnova M.V., Arlashkina O.Yu. Issledovanie vliyaniya tehnologicheskih faktorov na uroven ostatochnyh napryazhenij v MPKM obshivok reversa D18T [Research of influence of technology factors on level of residual stresses in MPKM of coverings of reverse D18T] // Vestnik SGAU im. S.P. Koroleva. 2011. T. 3. Ch. 3. S. 65–73.
  12. Postnov V.I., Senatorova O.G., Karimova S.A. i dr. Osobennosti formovaniya krupnogabaritnyh listov metallopolimernyh KM, ih struktura i svojstva [Features of formation of large-size sheets of metalpolymeric CM, their structure and properties] // Aviacionnye materialy i tehnologii. 2009. №4. S. 23–32.
  13. Lavro N.A., Barabash V.N., Efimov V.A. Prognozirovanie sroka sluzhby i resursa samoletnyh krupnogabaritnyh obtekatelej RLS iz polimernyh kompozicionnyh materialov [Forecasting of service life and resource of aircraft large-size fairing of RLS from polymeric composite materials] // Sb. dokl. 7-j nauch. konf. po gidroaviacii «Gidrosalon–2008». 2008. Ch. 1. S. 353–360.
  14. Postnov A.V., Postnov V.I., Vyakin V.N. Uprugodempfiruyushhie svojstva metallopolimernyh kompozitov pri vysokochastotnom nagruzhenii [Elastic-demping of property of metalpolymeric composites at high-frequency loading] // Vestnik SGAU im. S.P. Koroleva. 2011. №3. Ch. 3. S. 80–87.
  15. Postnov V.I., Postnova M.V., Mantusova O.Yu. Issledovanie vibroustalostnyh svojstv otseka nosovoj chasti kryla iz MPKM [Research vibro fatigue properties of compartment of nasal part of wing from MPKM] // Vestnik SGAU im. S.P. Koroleva. 2012. №3. Ch. 1. S. 281–290.