X-ray diffraction studies of electron beam ceramic thermal barrier coating layer based on ZrO2•Y2O3
UDC
620.179:620.197
DOI
10.18577/2307-6046-2017-0-1-3-3
Article PDF (Russian)
(768.57 KB)
How to cite
Medvedev P.N., Muboyadzhyan S.A. X-ray diffraction studies of electron beam ceramic thermal barrier coating layer based on ZrO2•Y2O3 // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-3-3. URL: https://www.viam-works.ru/en/journal/2017/1/3
Keywords
crystallographic texture, XRD, thermal barrier coating, inverse pole figures.
Abstract
The structure of the ceramic thermal barrier coating layer deposited on the blade of nickel alloy has been evaluated in the paper. The structural aspect is a crystallographic texture and the estimation parameters are an axis and scattering texture. Methodological questions of obtaining this information from the x-ray diffraction spectrum have been observed. These characteristics allow determining the crystallographic growth direction of the coating columnar grains. The average deviation of the grain growth from normal to the surface is 10 degrees. The inverse pole figure analysis method for texture parameters quantifying has been developed in the work.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Muboyadzhyan S.A. Teplozashhitnye pokrytiya s keramicheskim sloem ponizhennoj teploprovodnosti na osnove oksida cirkoniya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat-protective coverings with ceramic layer of the lowered heat conductivity on the basis of zirconium oxide for turbine blades of high pressure of perspective GTE] // Sovremennye dostizheniya v oblasti sozdaniya perspektivnyh nemetallicheskih kompozicionnyh materialov i pokrytij dlya aviacionnoj i kosmicheskoj tehniki: sb. dokl. konf. M.: VIAM, 2015. S. 3.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
- Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
- Matveev P.V., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Zashhitnye zharostojkie pokrytiya dlya splavov na osnove intermetallidov nikelya [High-temperature coatings for intermetallic nickel-based alloys] // Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
- Kablov E.N., Muboyadzhyan S.A. Teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat-protective coverings for turbine blades of high pressure of perspective GTE] // Metally. 2012. №1. S. 5–13.
- Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
- Muboyadzhyan S.A., Egorova L.P., Gorlov D.S., Kosmin A.A. Teplozashhitnye pokrytiya dlya krupnogabaritnyh detalej goryachego trakta perspektivnyh gazoturbinnyh dvigatelej [Heat-protective coverings for large-size details of hot path of perspective gas turbine engines] // Aviacionnye materialy i tehnologii. 2005. №1. S. 23–30.
- Rashkova B. Microstructural characterization of yttria-stabilized zirconia thermal barrier coatings grown on sapphire substrates. Stuttgart. Max-Planck-Institut für metallforschung, 2003. 126 р.
- Zhe Chen. Relation microstructure et propriete mecanique des films de ZrO2 obtenus par MOCVD. Paris. Universite Paris Sud, 2011. 172 p.
- Vasserman G., Greven I. Tekstury metallicheskih materialov [Structures of metal materials]. M.: Metallurgiya, 1969. 655 s.
- Ivanov A.N. Kristallografiya, rentgenografiya i elektronnaya mikroskopiya [Crystallography, roentgenography and electron microscopy]. M.: MISiS, 2009. Ch. 3. 22 s.
- Umanskij Ya.S., Skakov Yu.A., Ivanov A.N., Rastorguev L.N. Kristallografiya, rentgenografiya i elektronnaya mikroskopiya [Crystallography, roentgenography and electron microscopy]. M.: Metallurgiya, 1982. Ch. 3. 632 s.
- Vishnyakov Ya.D., Babareko A.A., Vladimirov S.A., Egiz I.V. Teoriya obrazovaniya tekstur v metallah i splavah [The theory of formation of structures in metals and alloys]. M.: Nauka, 1979. 344 s.