Rubber sealing materials (review)

Chaykun A.М., Naumov I.S., Alifanov E.V.
Chaykun A.М., Naumov I.S., Alifanov E.V. Rubber sealing materials (review) // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-12-12. URL: https://www.viam-works.ru/en/journal/2017/1/12
Keywords
sealant, sealing rubber.
Abstract

Creation and application of rubber sealing materials are described. The main types of sealants are shown as well as features of their design and operation. Both sealants of mass use and special functions are described. Their main utilization properties and features of application are given. The main properties of rubbers applied to manufacture of sealants are shown.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  4. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red.
  5. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. S. 346–348.
  6. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  7. Uplotneniya i uplotnitelnaya tehnika: spravochnik / pod obshh. red. A.I. Golubeva, L.A. Kondakova [Consolidations and sealing equipment: directory / gen. ed. by A.I. Golubev, L.A. Kondakov]. M.: Mashinostroenie, 1986. 464 s.
  8. Bolshoj spravochnik rezinshhika v 2 ch. [Big directory for specialist in rubber in 2 parts]. M.: Tehinform, 2012. 1385 s.
  9. Maskalyunajte O.E., Morozov Yu.L., Suhinin N.S. i dr. Vliyanie sposoba vvedeniya plastifikatorov na svojstva parafinatnyh kauchukov BNKS i standartnyh rezin na ih osnove [Influence of way of introduction of plasticizers on properties of the BNKS parafinatny rubbers and standard rubbers on their basis] // Kauchuk i rezina. 2006. №3. S. 14–17.
  10. Nikolaeva Yu.K., Zaharenko N.V., Doncov A.A. Osobennosti optimal'noj koncentracii dibutilsebacinata pri sozdanii morozostojkih rezin [Features of optimum concentration of dibutyl sebacate at creation of cold-resistant rubbers] // Kauchuk i rezina. 1984. №10. S. 4–7.
  11. Nikolaeva Yu.K., Kucherskij A.M., Zaharenko N.K., Doncov A.A. Vliyanie vvedeniya plastifikatorov nabuhaniem na morozostojkost rezin [Influence of introduction of plasticizers by swelling on frost resistance of rubbers] // Proizvodstvo shin, RTI i ATI. 1983. №11. S. 4–7.
  12. Petrova V.P., Pashina N.R. Ocenka morozostojkih svojstv rezin, kontaktiruyushhih so sredami neftyanogo proishozhdeniya [Assessment of cold-resistant properties of the rubbers contacting to environments of oil origin] // Proizvodstvo shin, RTI i ATI. 1983. №12. S. 27–29.
  13. Hemmer K. Polimernye plastifikatory // Polimernye smesi / pod red. D. Pola, S. Nyumena [Polymeric plasticizers]. M.: Mir, 1981. S. 237–260.
  14. Reznichenko S.V., Lysova G.A., Morozov Yu.L. Syrevye problemy materialovedeniya maslobenzostojkih rezinovyh izdelij [Raw problems of materials science oil and petrol resistant rubber products] // Kauchuk i rezina. 1997. №6. S. 28–32.
  15. Nesterova S.L. Svojstva novyh tipov butadien-nitrilnyh kauchukov, poluchennyh s razlichnymi emulgatorami i osobennosti ih pererabotki: avtoref. dis. … kand. tehn. nauk [Properties of new types of the butadiene nitrile rubbers received with different emulsifiers and feature of their processing: : thesis, Cand.. Sc. (Tech.)]. M.: MITHT im. M.V. Lomonosova, 2004. 15 s.
  16. Nudelman Z.N. Ftorkauchuki: osnovy, pererabotka, primenenie [Fluoroelastomers: bases, processing, application]. M.: RIAS, 2007. 383 s.
  17. Nudelman Z.N. K voprosu o morozostojkih ftorelastomerah [To question of cold-resistant fluoroelastomers ] // Kauchuk i rezina. 2005. №1. S. 8–10.
  18. Nudelman Z.N. Sovmeshhenie ftorkauchukov s drugimi polimerami [Combination of fluoroelastomers with other polymers] // Kauchuk i rezina. 2006. №4. S. 27–37.
  19. Chaikun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti morozostojkih rezin na osnove razlichnyh kauchukov [Features of old-resistant rubbers on the basis on different unvulcanized rubbers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №12. St. 04. Available at: http://www.viam-works.ru (accessed: August 10, 2016).
  20. Kuznecova O.V., Donskoj A.A., Markin E.A. Reziny na osnove ftorsiloksanovyh elastomerov: sostoyanie i perspektivy razvitiya [Rubbers on basis fluorine siloxane elastomer: condition and development perspectives] // Kauchuk i rezina. 2007. №3. S. 37–43.
  21. Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Osobennosti receptur rezin na osnove etilenpropilenovyh kauchukov i ih primenenie v izdeliyah specialnogo naznacheniya (obzor) [Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review)] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 51–55. DOI: 10.18577/2071-9140-2015-0-2-51-55.
  22. Govorova O.A. Recepturostroenie i svojstva rezin na osnove etilenpropilenovyh kauchukov [Compounding structure and properties of rubbers on the basis of ethylene-propylene rubbers]. M.: CNIITEneftehim, 1989. Vyp. 4. 60 s.
  23. Govorova O.A., Frolov A.E., Sorokin G.A. Svojstva rezin na osnove etilenpropilenovyh kauchukov [Properties of rubbers on the basis of ethylene-propylene rubbers]. M.: CNIITEneftehim, 1986. Ser.: Proizvodstvo shin, RTI i ATI. 64 s.
  24. Handbook of Rubber Bonding / ed. by B. Crowther. Rapra Technology, 2001. 400 p.
  25. Jerschow P. Silicone elastomers (Rapra Review Reports). Smithers Rapra Technology, 2001. 172 p.
  26. Marciniec B. Hydrosilylation: a comprehensive review on recent advances. Berlin: Springer. 2009. 408 p.
  27. Wilks E.S. Industrial polymers: handbook // Syntetic polymers (continued), biopolymers and their derivates. Weinheim: Wiley–VHS, 2001. Vol. 3. 1364 p.
  28. Naumov I.S., Petrova A.P., Barbotko S.L., Eliseev O.A. Reziny s ponizhennoj goryuchestyu [Rubbers with the lowered combustibility] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №4. S. 27–33.
  29. Naumov I.S., Petrova A.P., Barbotko S.L. Povyshenie pozharnoj bezopasnosti reziny na osnove siloksanovogo kauchuka [Increase of fire safety of rubber on the basis of siloxane rubber] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №3. S. 30–35.