Research of influence of alloying elements content on properties of high strength near alpha heat resistance titanium alloy VT46
Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Kondrateva A.R. Research of influence of alloying elements content on properties of high strength near alpha heat resistance titanium alloy VT46 // Proceedings of VIAM. 2016. No. 9. DOI: 10.18577/2307-6046-2016-0-9-6-6. URL: https://www.viam-works.ru/en/journal/2016/9/6
Keywords
heat-resistance titanium alloys, mechanical properties, structure, chemical composition.
Abstract
The study of influence of alloying elements content (aluminum, tin, silicon and iron) in the near alpha titanium alloy VТ46 in room and elevated temperatures (500 and 550°С) is performed. It is found that reducing the content of elements such as aluminum, tin, silicon comparing with a nominal composition leads to decrease in creep strength characteristics of the material. Content of iron has a significant effect only on the level of strength in relatively low test temperatures.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Razrabotki VIAM dlya gazoturbinnyh dvigatelej i ustanovok [Development of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
- Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
- Orlov M.R. Strategicheskie napravleniya razvitiya Ispytatelnogo centra FGUP «VIAM» [Strategic directions of development of the Test center FSUE «VIAM»] // Aviacionnye materialy i tehnologii. 2012. №S. S. 387–393.
- Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Metallurgical science of titanium and its alloys]. M.: Metallurgiya, 1992. 352 s.
- Pavlova T.V., Kashapov O.S., Kondrateva A.R., Kalashnikov V.S.Vozmozhnosti po rasshireniyu oblasti primeneniya splava VT8-1 dlya diskov i rabochih koles kompressora [Opportunities to expand the VT8-1 alloy application for disks and compressor rotor wheels] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №3 (39). St. 05. Available at: http://www.viam-works.ru (accessed: July 21, 2016). DOI: 10.18577/2307-6046-2016-0-3-5-5.
- Kashapov O.S., Pavlova T.V. Issledovanie vliyaniya parametrov ctruktury polufabrikatov iz splava VT41 na mehanicheskie svojstva [Research of influence of parameters of structure of semi-finished products from alloy ВТ41 on mechanical properties] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie, 2015. №2 (101). S. 138–145.
- Savushkin A.N., Kashapov O.S., Golynec S.A. Vliyanie skorosti nagruzheniya na mehanicheskie svojstva zharoprochnyh titanovyh splavov [An influence of loading rate on mechanical properties of heat-resistant titanium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 04. Available at: http://www.viam-works.ru (accessed: July 21, 2016). DOI: 10.18577/2307-6046-2015-0-3-4-4.
- Kalashnikov V.S., Kashapov O.S., Pavlova T.V., Istrakova A.R. Issledovanie svarnyh soedinenij splava VT41, poluchennyh metodom ELS [Investigation of VT41 alloy welded joints produced by EBW] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 81–88. DOI: 10.18577/2071-9140-2014-0-S5-81-88.
- Pavlova T.V., Kashapov O.S., Nochovnaya N.A. Titanovye splavy dlya gazoturbinnyh dvigatelej [Titanium alloys for gas turbine engines] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №5. S. 8–14.
- Pavlova T.V., Kashapov O.S., Nochovnaya N.A., Belyaev M.S. Sovremennye titanovye splavy i tehnologii, primenyaemye dlya detalej i uzlov GTD [Modern titanium alloys and the technologies applied to details and GTD nodes] // Sb. tez. dokl. nauch.-tehnich. kongressa po dvigatelestroeniyu «Dvigateli–2012». M.: ASSAD, 2012. S. 347–349.
- Ilyin A., Kolachev B., Volodin V., Ryndenkov D. About the purposefulness of comprasion of titanium alloys in terms of aluminium and Molybdenium equivalents // Titanium 99. Science and technology. 1999. P. 53–60.
- Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. Povyshenie prochnostnyh harakteristik zharoprochnyh psevdo-α-titanovyh splavov [Strengthening of high-temperature near-α-titanium alloys] // Aviacionnye materialy i tehnologii. 2014. №S5. C. 73–80. DOI: 10.18577/2071-9140-2014-0-S5-73-80.
- Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. Vliyanie soderzhaniya zheleza na mehanicheskie svojstva pokovok iz zharoprochnogo titanovogo splava VT41 [Effect of iron content on mechanical properties of forgings from heat-resistance titanium alloy VТ41] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 01. Available at: http://www.viam-works.ru (accessed: July 21, 2016). DOI: 10.18577/2307-6046-2015-0-10-1-1.
- Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. Vliyanie soderzhaniya zheleza na mehanicheskie svojstva prutkov iz zharoprochnogo titanovogo splava VT41 [An effect of iron content on mechanical properties of bars made of heat-resistant titanium alloy VТ41] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 02. Available at: http://www.viam-works.ru (accessed: July 21, 2016). DOI: 10.18577/2307-6046-2015-0-3-2-2.