Development in the field of elastomeric adhesives for aviation

Tyumeneva T.Y., Lukina N.F.
Tyumeneva T.Y., Lukina N.F. Development in the field of elastomeric adhesives for aviation // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-9-9. URL: https://www.viam-works.ru/en/journal/2016/8/9
Keywords
adhesive of cold curing, compound of rubbers with metals, the curing process, the increased durability of glued joints.
Abstract

The description of new developments of Federal State Unitary Enterprise VIAM in the field of elastomeric adhesives and technologies of their application in aviation engineering is provided. The main properties of rubber adhesives of cold curing and the adhesives intended for coupling rubbers with metals during vulcanization are represented. The way of increase of durability of adhesive connections based on rubbers is shown. The work is executed within implementation of the complex scientific direction 15.1. «Multifunction adhesive systems» («The strategic directions of development of materials and technologies of their processing for the period till 2030») [1].

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kardashov D.A., Petrova A.P. Polimernye klei [Polymer adhesives]. M.: Khimiya, 1983. 256 s.
  4. Petrova A.P., Donskoj A.A., Chalykh A.E., Shherbina A.A. Kleyashhie materialy. Germetiki: spravochnik / pod red. A.P. Petrovoj [Adhesive materials. Sealants: reference book / ed. by A.P. Petrova]. SPb.: Professional, 2008. 589 s.
  5. Petrova A.P., Lukina N.F., Dementeva L.A., Tyumeneva T.Yu., Avdonina I.A., Zhadova N.S. Klei dlya aviacionnykh materialov [Adhesives for aviation materials] // RZhKH. 2010. T. LIV. №1. S. 46–52.
  6. Kablov E.N., Minakov V.T., Anikhovskaya L.I. Klei i materialy na ikh osnove dlya remonta konstrukcij aviacionnoj tekhniki [Adhesives and materials on their basis for repair of designs of aviation engineering] // Aviacionnye materialy i tehnologii. 2002. №1. S. 61–65.
  7. Pestov S.S. Kak povysit prochnost' i termostojkost kleevogo krepleniya prorezinennykh tkanej [How increase durability and thermal resistance of adhesive binding of rubber-coated fabrics] // Tez. dokl. II Vseross. nauch.-tekhnich. konf. «Kauchuk i rezina–2010». M., 2010. 426 s.
  8. Voyuckij S.S. Autogeziya i adgeziya vysokopolimerov [Self-adhesion and adhesion of high-molecular polymer]. M.: Rostekhizdat,1960. 244 s.
  9. Tyumeneva T.Yu., Kogtyonkov A.S., Lukina N.F., Chursova L.V. Vliyanie napolnitelej na svojstva kleev rezinotekhnicheskogo naznacheniya [Influence of fillers on properties of adhesives of industrial rubber assignment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 05. Available at: http://www.viam-works.ru (accessed: February 17, 2016). DOI: 10.18577/2307-6046-2014-0-4-5-5.
  10. Lukina N.F., Dement'eva L.A., Petrova A.P., Tyumeneva T.Yu. Svojstva kleev i kleyashhikh materialov dlya izdelij aviacionnoj tekhniki [Properties of adhesions and glue materials for articles of aviation engineering] // Klei. Germetiki. Tehnologii. 2009. №1. S. 14–24.
  11. Sytyj Yu.V., Sagomonova V.A., Kislyakova V.I., Bolshakov V.A. Novye vibropogloshhayushhie materialy [New vibro absorbing materials] // Aviacionnye materialy i tehnologii. 2012. №2. S. 51–54.
  12. Tyumeneva T.Yu., Kogtyonkov A.S., Lukina N.F., Grashhenkov D.V. Vysokoprochnyj klej rezinotekhnicheskogo naznacheniya [High-strength adhesive of industrial rubber application] // Klei. Germetiki. Tehnologii. 2013. №5. S. 10–14.
  13. Tyumeneva T.Yu., Kogtyonkov A.S., Lukina N.F., Chursova L.V. Uspekhi v oblasti razrabotki kleev i tekhnologij dlya izgotovleniya rezinotekhnicheskikh izdelij aviacionnoj tekhniki [Achievements in the field of development of adhesives and technologies for production of industrial rubber articles of aviation engineering] // Klei. Germetiki. Tehnologii. 2013. №10. S. 7–10.
  14. Bajersdorf D. Kreplenie reziny k metallu s pomoshhyu svyazuyushhikh sistem «Khemosil®» [Bonding of rubber to metal by means of binder systems “Chemosil”] // Kauchuk i rezina. 1996. №6. S. 3–7.
  15. Logacheva E.P., Bokov S.V., Polsman G.S. Klei dlya krepleniya rezin mezhdu soboj i s drugimi substratami [Adhesives for binding rubbers among themselves and with other substrates] // Klei. Germetiki. Tehnologii. 2007. №9. S. 26–30.
  16. Tyumeneva T.Yu., Lukina N.F., Petrova A.P. Povyshenie adgezii e'lastomernykh kleev k rezinam pri ispol'zovanii adgezionnogo podsloya [Increase of adhesion of elastomer glues to rubbers when using adhesive interlayer] // Klei. Germetiki. Tehnologii. 2015. №11. S. 7–10.
  17. Kleevaya kompoziciya: pat. 2471842 Ros. Federaciya [Adhesion composition: pat. 2471842 Russian Federation]; opubl. 11.05.11.
  18. Tyumeneva T.Yu., Lukina N.F., Zhuravleva P.L., Gulyaev A.I. Vliyanie nanomodifikatorov na svojstva e'lastomernykh kleevykh sistem [Impact of nanomodifiers on properties of elastomer adhesive systems] // Klei. Germetiki. Tehnologii. 2015. №3. S. 11–16.