Development principles and alloying features of p/m NI base superalloys for jet-engine disks application

Volkov A.M., Vostrikov A.V., Bakradze M.M.
Volkov A.M., Vostrikov A.V., Bakradze M.M. Development principles and alloying features of p/m NI base superalloys for jet-engine disks application // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-2-2. URL: https://www.viam-works.ru/en/journal/2016/8/2
Keywords
disk billet, jet-engine, powder, Ni-base superalloys, alloying elements, microstructure, mechanical properties.
Abstract

The development of new aviation products requires the improvement of applicable alloys. Alloying complication of disk Ni-base superalloys leads to technical difficulties in their production and particularly during forging. Powder metallurgy allows successfully solving this problem and achieving mechanical characteristic that are very difficult to provide with traditional production methods. This article presents the basic principles of Russian P/M disk alloys development and also points the perspective directions of research in FSUE «VIAM». The work is executed within implementation of the complex scientific direction 10.2. «Isothermal deformation on air of new generation heterophase difficult-to-form superalloys» («The strategic directions of development of materials and technologies of their processing for the period till 2030») [1].

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Osnovatel otechestvennoj shkoly vysokotemperaturnykh aviacionnykh konstrukcionnykh materialov. K 100-letiyu so dnya rozhdeniya akademika S.T. Kishkina [Founder of domestic school of high-temperature aviation constructional materials. To the centenary of the birth of Academician S.T. Kishkin] // Krylya Rodiny. 2006. №5. S. 6.
  3. Kablov E.N., Bronfin M.B. Effekt S.T. Kishkina, ili pochemu struktura zharoprochnykh nikelevykh splavov dolzhna byt geterofaznoj [S.T. Kishkin`s effect or why the structure of heat-resistant nickel alloys should be heterogeneous] // Litejnye zharoprochnye splavy. Effekt S.T. Kishkina. M.: Nauka, 2006. S. 7–14.
  4. Letnikov M.N., Lomberg B.S., Ovsepyan S.V. Issledovanie kompozicij sistemy Ni–Al–Co pri razrabotke novogo zharoprochnogo deformiruemogo intermetallidnogo splava [Investigation ekhperimental alloys based on Ni–Al–Co ternary system for development a new high-temperature intermetallic alloy for disk application] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. № 10. St. 01. Available at: http://www.viam-works.ru (accessed: August 08, 2016).
  5. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Sovremennye tehnologii obrabotki metallov davleniem [Modern technologies of plastic working of metals] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 03. Available at: http://www.viam-works.ru (accessed: August 08, 2016). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  6. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvyaz struktury i svojstv vysokozharoprochnykh nikelevykh splavov dlya diskov gazoturbinnykh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] // Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
  7. Belov A.F., Anoshkin N.F., Fatkullin O.Kh. Struktura i svojstva granuliruemykh nikelevykh splavov [Structure and properties of granulated nickel alloys]. M.: Metallurgiya. 1984. 128 s.
  8. Zaderej A.G. Fenomen akademika A.F. Belova [Phenomenon of academician A.F. Belov] // Tekhnologiya legkikh splavov. 2006. №3. S. 37–40.
  9. Iz nauchnogo naslediya akademika A.F. Belova (K 105-letiyu so dnya rozhdeniya) [From scientific heritage of academician A.F. Belov (To the 105th anniversary)] // Tekhnologiya legkikh splavov. 2011. №1. S. 5–7.
  10. Inozemcev A.A., Anoshkin N.F., Bashkatov I.G., Garibov G.S., Koryakovcev A.S. Primenenie diskov iz granul zharoprochnykh nikelevykh splavov v serijnykh GTD aviacionnoj i nazemnoj tekhniki [Application of disks from grains of heat-resistant nickel alloys in serial GTE of aviation and ground engineering] // Perspektivnye tehnologii legkikh i specialnykh splavov. M.: FIZMATLIT, 2006. S. 371–376.
  11. Garibov G.S. Sovremennyj uroven razvitiya poroshkovoj metallurgii zharoprochnykh nikelevykh splavov [Modern level of development of powder metallurgy of heat-resistant nickel alloys] // Tekhnologiya legkikh splavov. 2000. №6. S. 58–68.
  12. Garibov G.S., Gric N.M., Vostrikov A.V., Fedorenko E.A. Krupnogabaritnye diski iz granul novogo vysokozharoprochnogo splava VV750P dlya perspektivnykh GTD [Large-sized disks from grains of new heat-resistant alloy VV750P for advanced GTE] // Tekhnologiya legkikh splavov. 2008. №1. S. 31–36.
  13. Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N. Vliyanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava EK151-ID [The influence of quenching on structure and properties nickel-based superalloy EK151-ID forgings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 01. Available at: http://www.viam-works.ru (accessed: August 08, 2016).
  14. Chabina E.B., Lomberg B.S., Filonova E.V., Ovsepyan S.V., Bakradze M.M. [Change of structural and phase condition of heat resisting deformable nickel alloy at alloying tantalum and rhenium] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 03. Available at: http://www.viam-works.ru (accessed: August 08, 2016). DOI: 10.18577/2307-6046-2015-0-9-3-3.
  15. Garibov G.S., Gric N.M., Vostrikov A.V., Fedorenko E.A. Sozdanie novogo vysokoprochnogo splava VV751P dlya perspektivnykh gazoturbinnykh dvigatelej [Development of new heat-resistant alloy VV750P for advanced gas turbine engines] //Tekhnologiya legkikh splavov. 2009. №1. S. 34–39.
  16. Garibov G.S., Gric N.M., Volkov A.M., Vostrikov A.V., Fedorenko E.A. Metallovedcheskie aspekty proizvodstva zagotovok diskov iz granuliruemykh zharoprochnykh nikelevykh splavov metodom GIP [Metallic aspects of stocks production of disks from granulated heat-resistant nickel alloys by HIP method] // Tekhnologiya legkikh splavov. 2014. №3. S. 54–59.
  17. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  18. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Shtampovka diskov GTD iz zharoprochnykh splavov na izotermicheskikh pressakh [Punching of disks GTD from hot strength alloys on isothermal presses] // Aviacionnye materialy i tehnologii. 2013. №1. S. 13–16.