Engineering method for predicting the value of the elastic modulus of single-layer ion-plasma fused coatings obtained by plasma chemical synthesis

Artemenko N.I., Simonov V.N.
Artemenko N.I., Simonov V.N. Engineering method for predicting the value of the elastic modulus of single-layer ion-plasma fused coatings obtained by plasma chemical synthesis // Proceedings of VIAM. 2016. No. 7. DOI: 10.18577/2307-6046-2016-0-7-5-5. URL: https://www.viam-works.ru/en/journal/2016/7/5
Abstract

The paper presents an engineering method for predicting the value of the modulus of elasticity in the condensed ion-plasma coatings obtained by plasma-chemical synthesis. The process of plasma-chemical synthesis of titanium nitride is considered, the basic characteristics of the process at a degree of binary compound conversion less than 1 is designated. It is found that the degree of conversion is equal to 1 in the excess of reaction gas in vacuum chamber of the ion-plasma unit. The method of measuring the elastic modulus of the material coating by bending the free end of the cantilever beam is developed and described. The elastic modulus of the coating material obtained by plasma synthesis with a deficiency of the reaction gas in chamber of the ion plasma unit is measured. It is found that the elastic modulus of the coating material is proportional to the degree of conversion. A formula is suggested for calculating the modulus of elasticity of the coating obtained by plasma synthesis

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  3. Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Zharoprochnye litejnye intermetallidnye splavy [Heat resisting cast intermetallic alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  4. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  5. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  6. Muboyadzhyan S.A. Osobennosti osazhdeniya potoka mnogokomponentnoj plazmy vakuumno-dugovogo razryada, soderzhashhego mikrokapli isparyaemogo materiala [Features of sedimentation of flow of multicomponent plasma of the vacuum arc discharge containing microdrops of evaporated material] // Metally. 2008. №2. S. 20–34.
  7. Matveev P.V., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Zashhitnye zharostojkie pokrytiya dlya splavov na osnove intermetallidov nikelya [High-temperature coatings for intermetallic nickel-based alloys] // Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
  8. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S. Nanoslojnye uprochnyayushchie pokrytiya dlya zashhity stalnyh i titanovyh lopatok kompressora GTD [Nanolayer strengthening coverings for protection of steel and titanic compressor blades of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 3–8.
  9. Budinovskij S.A., Muboyadzhyan S.A., Gayamov A.M., Stepanova S.V. Ionno-plazmennye zharostojkie pokrytiya s kompozicionnym bar'ernym sloem dlya zashhity ot okisleniya splava ZhS36-VI [Ion-plasma heat resisting coverings with composition barrier layer for protection against oxidation of alloy ZhS36-VI] // MiTOM. 2011. №1. S. 34–40.
  10. Gayamov A.M. Zharostojkoe pokrytie s kompozicionnym bar'ernym sloem dlya zashhity vneshnej poverhnosti rabochih lopatok GTD iz renijsoderzhashhih zharoprochnyh nikelevyh splavov [Heat resisting covering with composition barrier layer for protection of exterior surface of working blades of GTD from reniysoderzhashchy heat resisting nickel alloys] // Fiziko-himiya i tehnologiya neorganicheskih materialov: sb. mater. XI Ros. ezhegod. konf. molodyh nauchnyh sotrudnikov i aspirantov. M.: IMET RAN, 2012. C. 473–475.
  11. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] //Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  12. Sposob obrabotki poverhnosti metallicheskogo izdeliya: pat. 2368701 Ros. Federaciya [Way of surface treatment of metal product: pat. 2368701 Rus. Federation]; opubl. 27.09.09.
  13. Kablov E.N., Muboyadzhyan S.A. Teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat-protective coverings for turbine blades of high pressure of perspective GTD] // Metally. 2012. №1. S. 5–13.
  14. Sposob naneseniya kombinirovannogo zharostojkogo pokrytiya: pat. 2402633 Ros. Federaciya [Way of drawing the combined heat resisting covering: pat. 2402633 Rus. Federation]; 31.03.09.
  15. Budinovskij S.A., Muboyadzhyan S.A., Gayamov A.M., Kos'min A.A. Zharostojkie ionno-plazmennye pokrytiya dlya lopatok turbin iz nikelevyh splavov, legirovannyh reniem [Heat resisting ion-plasma coverings for blades of turbines from the nickel alloys alloyed by reniye] // MiTOM. 2008. №6. S. 31–36.
  16. Budinovskij S.A., Kablov E.N., Muboyadzhyan S.A. Primenenie analiticheskoj modeli opredeleniya uprugih napryazhenij v mnogoslojnoj sisteme pri reshenii zadach po sozdaniyu vysokotemperaturnyh zharostojkih pokrytij dlya rabochih lopatok aviacionnyh turbin [Application of analytical model of determination of elastic stresses in multi-layer system at the solution of tasks on creation of high-temperature heat resisting coverings for working blades of aviation turbines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №2. S. 26–37.
  17. Budinovskij S.A. Primenenie analiticheskoj modeli opredeleniya uprugih mehanicheskih i termicheskih napryazhenij v mnogoslojnoj sisteme v reshenii zadach po sozdaniyu zharostojkih alyuminidnyh pokrytij [Application of analytical model of determination of elastic mechanical and thermal stresses in multi-layer system in the solution of tasks on creation of heat resisting alyuminidny coverings] // Uprochnyayushhie tehnologii i pokrytiya. 2013. №3. S. 3–11.
  18. Feodosev V.I. Soprotivlenie materialov. 10-e izd., pererab. i dop. [Resistance of materials. 10th ed., processed and added]. M.: MGTU im. N.E. Baumana, 1999. 592 s.
  19. Samsonov G.V. Svojstva elementov: spravochnik. 2-e izd. [Properties of elements: directory. 2nd ed.] M.: Metallurgiya, 1976. Ch. 1. Fizicheskie svojstva. 600 s.
  20. Samsonov G.V., Vinickij I.M. Tugoplavkie soedineniya: spravochnik. 2-e izd. [High-melting connections: directory. 2nd ed.] M.: Metallurgiya, 1976. 560 s.
  21. Bielawski M. Residual stress control in TiN/Si coatings deposited by unbalanced magnetron sputtering // Surf. Coat. Technol. 2006. V. 200. P. 3987–3995.
  22. Artemenko N.I., Muboyadzhyan S.A. Inzhenernaya metodika ocenki velichiny i haraktera vnutrennih napryazhenij v odnoslojnyh uprochnyayushhih kondensirovannyh pokrytiyah [Engineering method of estimating the magnitude and nature of the internal stresses in the condensed monolayer reinforcing coatings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1. St. 04. Available at: http://www.viam-works.ru (accessed: February 12, 2016). DOI: 10.18577/2307-6046-2016-0-1-25-35.